Opaque polymers

A method for forming an opaque electron-rich polymer comprising the steps: 1) Coating a substrate with an adhesive either having the structure (i) as above ,where F1 is independently selected from, sulphur, silicon, nitrogen, oxygen, phosphorous or boron containing groups and L is selected from link...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: Mark Beckwith, Adnan Abdul Khader Syed, Jesse Opoku, Francois Morini, Atif Syed
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator Mark Beckwith
Adnan Abdul Khader Syed
Jesse Opoku
Francois Morini
Atif Syed
description A method for forming an opaque electron-rich polymer comprising the steps: 1) Coating a substrate with an adhesive either having the structure (i) as above ,where F1 is independently selected from, sulphur, silicon, nitrogen, oxygen, phosphorous or boron containing groups and L is selected from linking groups; or is an oxysilane. 2) Applying an electron-rich polymer to the adhesive coated substrate to form an opaque electron-rich layer, the polymer having the structure (ii) wherein E is electron-rich groups and R4 is C1-4 alkanediyl, optionally substituted with one or more halides; or is absent. Step 2 is started within 30 minutes of the end of step 1) The adhesive may be (3-mercaptopropyl)triethoxysilane or preferably (3-mercaptopropyl)trimethoxysilane. The electron rich group is preferably a conjugated group, ideally an aromatic group, more preferably a benzene group and may be selected from the poly(xylylenes). The substrate may be an elastomeric polymer material which may comprise a polysiloxane. Step 1) may be carried out under vacuum at a temperature from 5-100 oC and/or for a period of at least 1.5 hours most preferably at least 2.5 hours. Step 2) may be achieved using chemical vapour deposition. Also included are claims to the product of the method and use of an adhesive for obtaining an opaque electron rich polymer layer.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_GB2625503A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>GB2625503A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_GB2625503A3</originalsourceid><addsrcrecordid>eNrjZOD3L0gsLE1VKMjPqcxNLSrmYWBNS8wpTuWF0twM8m6uIc4euqkF-fGpxQWJyal5qSXx7k5GZkampgbGjsaEVQAAFz0eFg</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Opaque polymers</title><source>esp@cenet</source><creator>Mark Beckwith ; Adnan Abdul Khader Syed ; Jesse Opoku ; Francois Morini ; Atif Syed</creator><creatorcontrib>Mark Beckwith ; Adnan Abdul Khader Syed ; Jesse Opoku ; Francois Morini ; Atif Syed</creatorcontrib><description>A method for forming an opaque electron-rich polymer comprising the steps: 1) Coating a substrate with an adhesive either having the structure (i) as above ,where F1 is independently selected from, sulphur, silicon, nitrogen, oxygen, phosphorous or boron containing groups and L is selected from linking groups; or is an oxysilane. 2) Applying an electron-rich polymer to the adhesive coated substrate to form an opaque electron-rich layer, the polymer having the structure (ii) wherein E is electron-rich groups and R4 is C1-4 alkanediyl, optionally substituted with one or more halides; or is absent. Step 2 is started within 30 minutes of the end of step 1) The adhesive may be (3-mercaptopropyl)triethoxysilane or preferably (3-mercaptopropyl)trimethoxysilane. The electron rich group is preferably a conjugated group, ideally an aromatic group, more preferably a benzene group and may be selected from the poly(xylylenes). The substrate may be an elastomeric polymer material which may comprise a polysiloxane. Step 1) may be carried out under vacuum at a temperature from 5-100 oC and/or for a period of at least 1.5 hours most preferably at least 2.5 hours. Step 2) may be achieved using chemical vapour deposition. Also included are claims to the product of the method and use of an adhesive for obtaining an opaque electron rich polymer layer.</description><language>eng</language><subject>LAYERED PRODUCTS ; LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT ORNON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM ; PERFORMING OPERATIONS ; TRANSPORTING</subject><creationdate>2024</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20240626&amp;DB=EPODOC&amp;CC=GB&amp;NR=2625503A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20240626&amp;DB=EPODOC&amp;CC=GB&amp;NR=2625503A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>Mark Beckwith</creatorcontrib><creatorcontrib>Adnan Abdul Khader Syed</creatorcontrib><creatorcontrib>Jesse Opoku</creatorcontrib><creatorcontrib>Francois Morini</creatorcontrib><creatorcontrib>Atif Syed</creatorcontrib><title>Opaque polymers</title><description>A method for forming an opaque electron-rich polymer comprising the steps: 1) Coating a substrate with an adhesive either having the structure (i) as above ,where F1 is independently selected from, sulphur, silicon, nitrogen, oxygen, phosphorous or boron containing groups and L is selected from linking groups; or is an oxysilane. 2) Applying an electron-rich polymer to the adhesive coated substrate to form an opaque electron-rich layer, the polymer having the structure (ii) wherein E is electron-rich groups and R4 is C1-4 alkanediyl, optionally substituted with one or more halides; or is absent. Step 2 is started within 30 minutes of the end of step 1) The adhesive may be (3-mercaptopropyl)triethoxysilane or preferably (3-mercaptopropyl)trimethoxysilane. The electron rich group is preferably a conjugated group, ideally an aromatic group, more preferably a benzene group and may be selected from the poly(xylylenes). The substrate may be an elastomeric polymer material which may comprise a polysiloxane. Step 1) may be carried out under vacuum at a temperature from 5-100 oC and/or for a period of at least 1.5 hours most preferably at least 2.5 hours. Step 2) may be achieved using chemical vapour deposition. Also included are claims to the product of the method and use of an adhesive for obtaining an opaque electron rich polymer layer.</description><subject>LAYERED PRODUCTS</subject><subject>LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT ORNON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM</subject><subject>PERFORMING OPERATIONS</subject><subject>TRANSPORTING</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2024</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZOD3L0gsLE1VKMjPqcxNLSrmYWBNS8wpTuWF0twM8m6uIc4euqkF-fGpxQWJyal5qSXx7k5GZkampgbGjsaEVQAAFz0eFg</recordid><startdate>20240626</startdate><enddate>20240626</enddate><creator>Mark Beckwith</creator><creator>Adnan Abdul Khader Syed</creator><creator>Jesse Opoku</creator><creator>Francois Morini</creator><creator>Atif Syed</creator><scope>EVB</scope></search><sort><creationdate>20240626</creationdate><title>Opaque polymers</title><author>Mark Beckwith ; Adnan Abdul Khader Syed ; Jesse Opoku ; Francois Morini ; Atif Syed</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_GB2625503A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2024</creationdate><topic>LAYERED PRODUCTS</topic><topic>LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT ORNON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM</topic><topic>PERFORMING OPERATIONS</topic><topic>TRANSPORTING</topic><toplevel>online_resources</toplevel><creatorcontrib>Mark Beckwith</creatorcontrib><creatorcontrib>Adnan Abdul Khader Syed</creatorcontrib><creatorcontrib>Jesse Opoku</creatorcontrib><creatorcontrib>Francois Morini</creatorcontrib><creatorcontrib>Atif Syed</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>Mark Beckwith</au><au>Adnan Abdul Khader Syed</au><au>Jesse Opoku</au><au>Francois Morini</au><au>Atif Syed</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Opaque polymers</title><date>2024-06-26</date><risdate>2024</risdate><abstract>A method for forming an opaque electron-rich polymer comprising the steps: 1) Coating a substrate with an adhesive either having the structure (i) as above ,where F1 is independently selected from, sulphur, silicon, nitrogen, oxygen, phosphorous or boron containing groups and L is selected from linking groups; or is an oxysilane. 2) Applying an electron-rich polymer to the adhesive coated substrate to form an opaque electron-rich layer, the polymer having the structure (ii) wherein E is electron-rich groups and R4 is C1-4 alkanediyl, optionally substituted with one or more halides; or is absent. Step 2 is started within 30 minutes of the end of step 1) The adhesive may be (3-mercaptopropyl)triethoxysilane or preferably (3-mercaptopropyl)trimethoxysilane. The electron rich group is preferably a conjugated group, ideally an aromatic group, more preferably a benzene group and may be selected from the poly(xylylenes). The substrate may be an elastomeric polymer material which may comprise a polysiloxane. Step 1) may be carried out under vacuum at a temperature from 5-100 oC and/or for a period of at least 1.5 hours most preferably at least 2.5 hours. Step 2) may be achieved using chemical vapour deposition. Also included are claims to the product of the method and use of an adhesive for obtaining an opaque electron rich polymer layer.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_GB2625503A
source esp@cenet
subjects LAYERED PRODUCTS
LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT ORNON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
PERFORMING OPERATIONS
TRANSPORTING
title Opaque polymers
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-27T11%3A29%3A28IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=Mark%20Beckwith&rft.date=2024-06-26&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EGB2625503A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true