Improvements to the continuous spray forming of metal strip
Continuous lengths of metallic strip are produced by a method in which a free falling stream of molten metallic material is atomised by a plurality of gaseous jets pre-heated to a temperature within the range 400 DEG C to 1200 DEG C to form a spray 6 of molten metal particles which collect on the su...
Gespeichert in:
1. Verfasser: | |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | Continuous lengths of metallic strip are produced by a method in which a free falling stream of molten metallic material is atomised by a plurality of gaseous jets pre-heated to a temperature within the range 400 DEG C to 1200 DEG C to form a spray 6 of molten metal particles which collect on the surface of an internally heated hollow receptor roll 10 and are peeled from the receptor roll in the form of a continuous strip. The receptor roll may be coated with a dried layer of colloidal silica after shot blasting. |
---|