MOULDING COMPOSITION SUITABLE FOR THE PRODUCTION OF MICROPOROUS BATTERY SEPARATORS
The composition comprises polyolefins, fillers and a plasticizer. It contains 0.2 to 20 wt. % etoxysiloxane, 5 to 60 wt. % polyolefin, 10 to 60 wt. % white black filler, and 10 to 75 wt. % polyethyleneglycol, petroleum oil or dioctylphtalate. The polyolefin can be high-density polyethylene with a me...
Gespeichert in:
Hauptverfasser: | , , , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | STEFKA KIRILOVA FILIPOVA EVGENI BOGDANOV BUDEVSKI LYUBE KRESTANOV YANKOV IVO YORDANOV ZLATANOV |
description | The composition comprises polyolefins, fillers and a plasticizer. It contains 0.2 to 20 wt. % etoxysiloxane, 5 to 60 wt. % polyolefin, 10 to 60 wt. % white black filler, and 10 to 75 wt. % polyethyleneglycol, petroleum oil or dioctylphtalate. The polyolefin can be high-density polyethylene with a melt index at a standard charging up to 6, superhigh-molecular polyethylene, polypropylene, or a mixture of polypropylene and polyethylene, or of high-density polyethylene and super-high-molecular polyethylene at as ratio of 0 to 100 wt. parts high-density polyethylene for every 100 wt. parts super-high-molecular polyethylene. The composition is prepared by treating the filler with etoxysiloxane at room temperature, then adding the polyolefin and the plasticizer to form a mixture, and then homogenizing the mixture in a cold state or with heating. With this composition are prepared microporous separators having an average pore size of below 0.05 mu , and having high physicomechanical properties. |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_GB2212509B</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>GB2212509B</sourcerecordid><originalsourceid>FETCH-epo_espacenet_GB2212509B3</originalsourceid><addsrcrecordid>eNqFyrEKwjAQgOEsDlJ9Bu8FChpxcEzSpA00vXC5DJ1KkTiJFur7I4i70z98_1ZQwNw3fmjBYIiYPHscIGXPSvcWHBJwZyESNtl8DR0EbwgjEuYEWjFbGiHZqEgxUtqJzX1-rGX_ayUOzrLp6rK8prIu8608y3tqtZQneTle9fn_8QFrJi9i</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>MOULDING COMPOSITION SUITABLE FOR THE PRODUCTION OF MICROPOROUS BATTERY SEPARATORS</title><source>esp@cenet</source><creator>STEFKA KIRILOVA FILIPOVA ; EVGENI BOGDANOV BUDEVSKI ; LYUBE KRESTANOV YANKOV ; IVO YORDANOV ZLATANOV</creator><creatorcontrib>STEFKA KIRILOVA FILIPOVA ; EVGENI BOGDANOV BUDEVSKI ; LYUBE KRESTANOV YANKOV ; IVO YORDANOV ZLATANOV</creatorcontrib><description>The composition comprises polyolefins, fillers and a plasticizer. It contains 0.2 to 20 wt. % etoxysiloxane, 5 to 60 wt. % polyolefin, 10 to 60 wt. % white black filler, and 10 to 75 wt. % polyethyleneglycol, petroleum oil or dioctylphtalate. The polyolefin can be high-density polyethylene with a melt index at a standard charging up to 6, superhigh-molecular polyethylene, polypropylene, or a mixture of polypropylene and polyethylene, or of high-density polyethylene and super-high-molecular polyethylene at as ratio of 0 to 100 wt. parts high-density polyethylene for every 100 wt. parts super-high-molecular polyethylene. The composition is prepared by treating the filler with etoxysiloxane at room temperature, then adding the polyolefin and the plasticizer to form a mixture, and then homogenizing the mixture in a cold state or with heating. With this composition are prepared microporous separators having an average pore size of below 0.05 mu , and having high physicomechanical properties.</description><edition>5</edition><language>eng</language><subject>BASIC ELECTRIC ELEMENTS ; CHEMISTRY ; COMPOSITIONS BASED THEREON ; COMPOSITIONS OF MACROMOLECULAR COMPOUNDS ; ELECTRICITY ; METALLURGY ; ORGANIC MACROMOLECULAR COMPOUNDS ; PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY ; THEIR PREPARATION OR CHEMICAL WORKING-UP ; USE OF INORGANIC OR NON-MACROMOLECULAR ORGANIC SUBSTANCES ASCOMPOUNDING INGREDIENTS</subject><creationdate>1991</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=19910710&DB=EPODOC&CC=GB&NR=2212509B$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25563,76318</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=19910710&DB=EPODOC&CC=GB&NR=2212509B$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>STEFKA KIRILOVA FILIPOVA</creatorcontrib><creatorcontrib>EVGENI BOGDANOV BUDEVSKI</creatorcontrib><creatorcontrib>LYUBE KRESTANOV YANKOV</creatorcontrib><creatorcontrib>IVO YORDANOV ZLATANOV</creatorcontrib><title>MOULDING COMPOSITION SUITABLE FOR THE PRODUCTION OF MICROPOROUS BATTERY SEPARATORS</title><description>The composition comprises polyolefins, fillers and a plasticizer. It contains 0.2 to 20 wt. % etoxysiloxane, 5 to 60 wt. % polyolefin, 10 to 60 wt. % white black filler, and 10 to 75 wt. % polyethyleneglycol, petroleum oil or dioctylphtalate. The polyolefin can be high-density polyethylene with a melt index at a standard charging up to 6, superhigh-molecular polyethylene, polypropylene, or a mixture of polypropylene and polyethylene, or of high-density polyethylene and super-high-molecular polyethylene at as ratio of 0 to 100 wt. parts high-density polyethylene for every 100 wt. parts super-high-molecular polyethylene. The composition is prepared by treating the filler with etoxysiloxane at room temperature, then adding the polyolefin and the plasticizer to form a mixture, and then homogenizing the mixture in a cold state or with heating. With this composition are prepared microporous separators having an average pore size of below 0.05 mu , and having high physicomechanical properties.</description><subject>BASIC ELECTRIC ELEMENTS</subject><subject>CHEMISTRY</subject><subject>COMPOSITIONS BASED THEREON</subject><subject>COMPOSITIONS OF MACROMOLECULAR COMPOUNDS</subject><subject>ELECTRICITY</subject><subject>METALLURGY</subject><subject>ORGANIC MACROMOLECULAR COMPOUNDS</subject><subject>PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY</subject><subject>THEIR PREPARATION OR CHEMICAL WORKING-UP</subject><subject>USE OF INORGANIC OR NON-MACROMOLECULAR ORGANIC SUBSTANCES ASCOMPOUNDING INGREDIENTS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>1991</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqFyrEKwjAQgOEsDlJ9Bu8FChpxcEzSpA00vXC5DJ1KkTiJFur7I4i70z98_1ZQwNw3fmjBYIiYPHscIGXPSvcWHBJwZyESNtl8DR0EbwgjEuYEWjFbGiHZqEgxUtqJzX1-rGX_ayUOzrLp6rK8prIu8608y3tqtZQneTle9fn_8QFrJi9i</recordid><startdate>19910710</startdate><enddate>19910710</enddate><creator>STEFKA KIRILOVA FILIPOVA</creator><creator>EVGENI BOGDANOV BUDEVSKI</creator><creator>LYUBE KRESTANOV YANKOV</creator><creator>IVO YORDANOV ZLATANOV</creator><scope>EVB</scope></search><sort><creationdate>19910710</creationdate><title>MOULDING COMPOSITION SUITABLE FOR THE PRODUCTION OF MICROPOROUS BATTERY SEPARATORS</title><author>STEFKA KIRILOVA FILIPOVA ; EVGENI BOGDANOV BUDEVSKI ; LYUBE KRESTANOV YANKOV ; IVO YORDANOV ZLATANOV</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_GB2212509B3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>1991</creationdate><topic>BASIC ELECTRIC ELEMENTS</topic><topic>CHEMISTRY</topic><topic>COMPOSITIONS BASED THEREON</topic><topic>COMPOSITIONS OF MACROMOLECULAR COMPOUNDS</topic><topic>ELECTRICITY</topic><topic>METALLURGY</topic><topic>ORGANIC MACROMOLECULAR COMPOUNDS</topic><topic>PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY</topic><topic>THEIR PREPARATION OR CHEMICAL WORKING-UP</topic><topic>USE OF INORGANIC OR NON-MACROMOLECULAR ORGANIC SUBSTANCES ASCOMPOUNDING INGREDIENTS</topic><toplevel>online_resources</toplevel><creatorcontrib>STEFKA KIRILOVA FILIPOVA</creatorcontrib><creatorcontrib>EVGENI BOGDANOV BUDEVSKI</creatorcontrib><creatorcontrib>LYUBE KRESTANOV YANKOV</creatorcontrib><creatorcontrib>IVO YORDANOV ZLATANOV</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>STEFKA KIRILOVA FILIPOVA</au><au>EVGENI BOGDANOV BUDEVSKI</au><au>LYUBE KRESTANOV YANKOV</au><au>IVO YORDANOV ZLATANOV</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>MOULDING COMPOSITION SUITABLE FOR THE PRODUCTION OF MICROPOROUS BATTERY SEPARATORS</title><date>1991-07-10</date><risdate>1991</risdate><abstract>The composition comprises polyolefins, fillers and a plasticizer. It contains 0.2 to 20 wt. % etoxysiloxane, 5 to 60 wt. % polyolefin, 10 to 60 wt. % white black filler, and 10 to 75 wt. % polyethyleneglycol, petroleum oil or dioctylphtalate. The polyolefin can be high-density polyethylene with a melt index at a standard charging up to 6, superhigh-molecular polyethylene, polypropylene, or a mixture of polypropylene and polyethylene, or of high-density polyethylene and super-high-molecular polyethylene at as ratio of 0 to 100 wt. parts high-density polyethylene for every 100 wt. parts super-high-molecular polyethylene. The composition is prepared by treating the filler with etoxysiloxane at room temperature, then adding the polyolefin and the plasticizer to form a mixture, and then homogenizing the mixture in a cold state or with heating. With this composition are prepared microporous separators having an average pore size of below 0.05 mu , and having high physicomechanical properties.</abstract><edition>5</edition><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | eng |
recordid | cdi_epo_espacenet_GB2212509B |
source | esp@cenet |
subjects | BASIC ELECTRIC ELEMENTS CHEMISTRY COMPOSITIONS BASED THEREON COMPOSITIONS OF MACROMOLECULAR COMPOUNDS ELECTRICITY METALLURGY ORGANIC MACROMOLECULAR COMPOUNDS PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY THEIR PREPARATION OR CHEMICAL WORKING-UP USE OF INORGANIC OR NON-MACROMOLECULAR ORGANIC SUBSTANCES ASCOMPOUNDING INGREDIENTS |
title | MOULDING COMPOSITION SUITABLE FOR THE PRODUCTION OF MICROPOROUS BATTERY SEPARATORS |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-11T00%3A07%3A50IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=STEFKA%20KIRILOVA%20FILIPOVA&rft.date=1991-07-10&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EGB2212509B%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |