Method of explosive hardening a cast portion of acute angle frogs of railroad switches

A method of explosive hardening a cast portion of acute angle railroad frogs of high-manganese steel residing in that a charge of sheet explosive is placed on the roll surface and side surfaces of a core 1 and guard rails 3 of this cast portion in the area where train wheels roll on the frog element...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: KONSTANTIN IVANOVICH KRASIKOV, EVGENY EVGENIEVICH ZUBKOV, ALEXANDR VASILIEVICH VODYANOV, ANDREI ANDREEVICH DERIBAS, ALEXANDR GRIGORIEVICH TSARENKO, NIKOLAI NIKITOVICH PUTRYA, VLADIMIR ALEXANDROVICH PRYAKHIN, TATYANA MAXIMOVNA SOBOLENKO, ROMAN ZAKHAROVICH KATS
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator KONSTANTIN IVANOVICH KRASIKOV
EVGENY EVGENIEVICH ZUBKOV
ALEXANDR VASILIEVICH VODYANOV
ANDREI ANDREEVICH DERIBAS
ALEXANDR GRIGORIEVICH TSARENKO
NIKOLAI NIKITOVICH PUTRYA
VLADIMIR ALEXANDROVICH PRYAKHIN
TATYANA MAXIMOVNA SOBOLENKO
ROMAN ZAKHAROVICH KATS
description A method of explosive hardening a cast portion of acute angle railroad frogs of high-manganese steel residing in that a charge of sheet explosive is placed on the roll surface and side surfaces of a core 1 and guard rails 3 of this cast portion in the area where train wheels roll on the frog elements, and the charge is detonated to attack the surfaces by a slanted detonation wave front with a pressure of 50x10 to 250x10 Pa to act on said surfaces during 10 to 10 sec.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_GB2172234A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>GB2172234A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_GB2172234A3</originalsourceid><addsrcrecordid>eNqFyrsKAjEQQNFtLET9BucHLMwK1q74aOzEdhmSyQNCJmTGx-fLgr3VhcuZd48baWQH7IE-NbOkF0HE5qikEgDBoihUbpq4TArtUwmwhEzgGweZZsOUG6MDeSe1kWTZzTxmodWvi259Pt2P1w1VHkkqWiqk42Uw270x_e7Q_xdfGUU4aw</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Method of explosive hardening a cast portion of acute angle frogs of railroad switches</title><source>esp@cenet</source><creator>KONSTANTIN IVANOVICH KRASIKOV ; EVGENY EVGENIEVICH ZUBKOV ; ALEXANDR VASILIEVICH VODYANOV ; ANDREI ANDREEVICH DERIBAS ; ALEXANDR GRIGORIEVICH TSARENKO ; NIKOLAI NIKITOVICH PUTRYA ; VLADIMIR ALEXANDROVICH PRYAKHIN ; TATYANA MAXIMOVNA SOBOLENKO ; ROMAN ZAKHAROVICH KATS</creator><creatorcontrib>KONSTANTIN IVANOVICH KRASIKOV ; EVGENY EVGENIEVICH ZUBKOV ; ALEXANDR VASILIEVICH VODYANOV ; ANDREI ANDREEVICH DERIBAS ; ALEXANDR GRIGORIEVICH TSARENKO ; NIKOLAI NIKITOVICH PUTRYA ; VLADIMIR ALEXANDROVICH PRYAKHIN ; TATYANA MAXIMOVNA SOBOLENKO ; ROMAN ZAKHAROVICH KATS</creatorcontrib><description>A method of explosive hardening a cast portion of acute angle railroad frogs of high-manganese steel residing in that a charge of sheet explosive is placed on the roll surface and side surfaces of a core 1 and guard rails 3 of this cast portion in the area where train wheels roll on the frog elements, and the charge is detonated to attack the surfaces by a slanted detonation wave front with a pressure of 50x10 to 250x10 Pa to act on said surfaces during 10 to 10 sec.</description><edition>4</edition><language>eng</language><subject>CHEMISTRY ; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS ; MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS ; MECHANICAL METAL-WORKING WITHOUT ESSENTIALLY REMOVINGMATERIAL ; METALLURGY ; METALLURGY OF IRON ; MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS ; PERFORMING OPERATIONS ; PUNCHING METAL ; TRANSPORTING ; WORKING OR PROCESSING OF SHEET METAL OR METAL TUBES, RODS ORPROFILES WITHOUT ESSENTIALLY REMOVING MATERIAL</subject><creationdate>1986</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19860917&amp;DB=EPODOC&amp;CC=GB&amp;NR=2172234A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25543,76293</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19860917&amp;DB=EPODOC&amp;CC=GB&amp;NR=2172234A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>KONSTANTIN IVANOVICH KRASIKOV</creatorcontrib><creatorcontrib>EVGENY EVGENIEVICH ZUBKOV</creatorcontrib><creatorcontrib>ALEXANDR VASILIEVICH VODYANOV</creatorcontrib><creatorcontrib>ANDREI ANDREEVICH DERIBAS</creatorcontrib><creatorcontrib>ALEXANDR GRIGORIEVICH TSARENKO</creatorcontrib><creatorcontrib>NIKOLAI NIKITOVICH PUTRYA</creatorcontrib><creatorcontrib>VLADIMIR ALEXANDROVICH PRYAKHIN</creatorcontrib><creatorcontrib>TATYANA MAXIMOVNA SOBOLENKO</creatorcontrib><creatorcontrib>ROMAN ZAKHAROVICH KATS</creatorcontrib><title>Method of explosive hardening a cast portion of acute angle frogs of railroad switches</title><description>A method of explosive hardening a cast portion of acute angle railroad frogs of high-manganese steel residing in that a charge of sheet explosive is placed on the roll surface and side surfaces of a core 1 and guard rails 3 of this cast portion in the area where train wheels roll on the frog elements, and the charge is detonated to attack the surfaces by a slanted detonation wave front with a pressure of 50x10 to 250x10 Pa to act on said surfaces during 10 to 10 sec.</description><subject>CHEMISTRY</subject><subject>GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS</subject><subject>MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS</subject><subject>MECHANICAL METAL-WORKING WITHOUT ESSENTIALLY REMOVINGMATERIAL</subject><subject>METALLURGY</subject><subject>METALLURGY OF IRON</subject><subject>MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS</subject><subject>PERFORMING OPERATIONS</subject><subject>PUNCHING METAL</subject><subject>TRANSPORTING</subject><subject>WORKING OR PROCESSING OF SHEET METAL OR METAL TUBES, RODS ORPROFILES WITHOUT ESSENTIALLY REMOVING MATERIAL</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>1986</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqFyrsKAjEQQNFtLET9BucHLMwK1q74aOzEdhmSyQNCJmTGx-fLgr3VhcuZd48baWQH7IE-NbOkF0HE5qikEgDBoihUbpq4TArtUwmwhEzgGweZZsOUG6MDeSe1kWTZzTxmodWvi259Pt2P1w1VHkkqWiqk42Uw270x_e7Q_xdfGUU4aw</recordid><startdate>19860917</startdate><enddate>19860917</enddate><creator>KONSTANTIN IVANOVICH KRASIKOV</creator><creator>EVGENY EVGENIEVICH ZUBKOV</creator><creator>ALEXANDR VASILIEVICH VODYANOV</creator><creator>ANDREI ANDREEVICH DERIBAS</creator><creator>ALEXANDR GRIGORIEVICH TSARENKO</creator><creator>NIKOLAI NIKITOVICH PUTRYA</creator><creator>VLADIMIR ALEXANDROVICH PRYAKHIN</creator><creator>TATYANA MAXIMOVNA SOBOLENKO</creator><creator>ROMAN ZAKHAROVICH KATS</creator><scope>EVB</scope></search><sort><creationdate>19860917</creationdate><title>Method of explosive hardening a cast portion of acute angle frogs of railroad switches</title><author>KONSTANTIN IVANOVICH KRASIKOV ; EVGENY EVGENIEVICH ZUBKOV ; ALEXANDR VASILIEVICH VODYANOV ; ANDREI ANDREEVICH DERIBAS ; ALEXANDR GRIGORIEVICH TSARENKO ; NIKOLAI NIKITOVICH PUTRYA ; VLADIMIR ALEXANDROVICH PRYAKHIN ; TATYANA MAXIMOVNA SOBOLENKO ; ROMAN ZAKHAROVICH KATS</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_GB2172234A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>1986</creationdate><topic>CHEMISTRY</topic><topic>GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS</topic><topic>MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS</topic><topic>MECHANICAL METAL-WORKING WITHOUT ESSENTIALLY REMOVINGMATERIAL</topic><topic>METALLURGY</topic><topic>METALLURGY OF IRON</topic><topic>MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS</topic><topic>PERFORMING OPERATIONS</topic><topic>PUNCHING METAL</topic><topic>TRANSPORTING</topic><topic>WORKING OR PROCESSING OF SHEET METAL OR METAL TUBES, RODS ORPROFILES WITHOUT ESSENTIALLY REMOVING MATERIAL</topic><toplevel>online_resources</toplevel><creatorcontrib>KONSTANTIN IVANOVICH KRASIKOV</creatorcontrib><creatorcontrib>EVGENY EVGENIEVICH ZUBKOV</creatorcontrib><creatorcontrib>ALEXANDR VASILIEVICH VODYANOV</creatorcontrib><creatorcontrib>ANDREI ANDREEVICH DERIBAS</creatorcontrib><creatorcontrib>ALEXANDR GRIGORIEVICH TSARENKO</creatorcontrib><creatorcontrib>NIKOLAI NIKITOVICH PUTRYA</creatorcontrib><creatorcontrib>VLADIMIR ALEXANDROVICH PRYAKHIN</creatorcontrib><creatorcontrib>TATYANA MAXIMOVNA SOBOLENKO</creatorcontrib><creatorcontrib>ROMAN ZAKHAROVICH KATS</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>KONSTANTIN IVANOVICH KRASIKOV</au><au>EVGENY EVGENIEVICH ZUBKOV</au><au>ALEXANDR VASILIEVICH VODYANOV</au><au>ANDREI ANDREEVICH DERIBAS</au><au>ALEXANDR GRIGORIEVICH TSARENKO</au><au>NIKOLAI NIKITOVICH PUTRYA</au><au>VLADIMIR ALEXANDROVICH PRYAKHIN</au><au>TATYANA MAXIMOVNA SOBOLENKO</au><au>ROMAN ZAKHAROVICH KATS</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Method of explosive hardening a cast portion of acute angle frogs of railroad switches</title><date>1986-09-17</date><risdate>1986</risdate><abstract>A method of explosive hardening a cast portion of acute angle railroad frogs of high-manganese steel residing in that a charge of sheet explosive is placed on the roll surface and side surfaces of a core 1 and guard rails 3 of this cast portion in the area where train wheels roll on the frog elements, and the charge is detonated to attack the surfaces by a slanted detonation wave front with a pressure of 50x10 to 250x10 Pa to act on said surfaces during 10 to 10 sec.</abstract><edition>4</edition><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_GB2172234A
source esp@cenet
subjects CHEMISTRY
GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS
MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS
MECHANICAL METAL-WORKING WITHOUT ESSENTIALLY REMOVINGMATERIAL
METALLURGY
METALLURGY OF IRON
MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS
PERFORMING OPERATIONS
PUNCHING METAL
TRANSPORTING
WORKING OR PROCESSING OF SHEET METAL OR METAL TUBES, RODS ORPROFILES WITHOUT ESSENTIALLY REMOVING MATERIAL
title Method of explosive hardening a cast portion of acute angle frogs of railroad switches
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-24T22%3A41%3A48IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=KONSTANTIN%20IVANOVICH%20KRASIKOV&rft.date=1986-09-17&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EGB2172234A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true