PROCEDE D'ENRICHISSEMENT DE MINERAIS DE CUIVRE OXYDES DIFFICILEMENT ENRICHISSABLES

The method provides for preparation of a pulp, its sulphidizing and floatation. The sulphidizing of the pulp is effected with melted sulphur at a temperature of 115-180 DEG C and at a pressure of 1.5-10 atm in the presence of sodium sulphate or sodium chloride at a mass ratio between the sulphur and...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
1. Verfasser: N. S. BEKTURGANOV, S. V. BELYAEV, D. N. ABISHEV, V. P. MALYSHEV, G. K. KHAIROVA, S. P. SIM, D. V. SOLOGUB, ZH. M. MAKHMUTOV, A. F. CHUNIN, V. I. REVNIVTSEV, I. SH. SATAEV, M. Y. RYSKIN, S. I. SOBOL, V. V. POPKOV, S. I. KAPITONOV, P. T. ZHMURKO, N. V. MATVEENKO, B. S. ZADOVA, L. A. STRELSKAYA, V. S. CHECHETKIN, G. N. SMIRNOV ET V. K. LAIKIN
Format: Patent
Sprache:fre
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator N. S. BEKTURGANOV, S. V. BELYAEV, D. N. ABISHEV, V. P. MALYSHEV, G. K. KHAIROVA, S. P. SIM, D. V. SOLOGUB, ZH. M. MAKHMUTOV, A. F. CHUNIN, V. I. REVNIVTSEV, I. SH. SATAEV, M. Y. RYSKIN, S. I. SOBOL, V. V. POPKOV, S. I. KAPITONOV, P. T. ZHMURKO, N. V. MATVEENKO, B. S. ZADOVA, L. A. STRELSKAYA, V. S. CHECHETKIN, G. N. SMIRNOV ET V. K. LAIKIN
description The method provides for preparation of a pulp, its sulphidizing and floatation. The sulphidizing of the pulp is effected with melted sulphur at a temperature of 115-180 DEG C and at a pressure of 1.5-10 atm in the presence of sodium sulphate or sodium chloride at a mass ratio between the sulphur and the oxidized copper of (0.2-1.5):1. L'INVENTION CONCERNE LA METALLURGIE DES METAUX NON FERREUX, ET PLUS SPECIALEMENT UN PROCEDE D'ENRICHISSEMENT DE MINERAIS DE CUIVRE OXYDES DIFFICILEMENT ENRICHISSABLES.LE PROCEDE COMPORTE LA PREPARATION D'UNE PULPE, SA SULFURATION ET SA FLOTTATION. LA SULFURATION DE LA PULPE EST EFFECTUEE PAR DU SOUFRE FONDU UNE TEMPERATURE DE 115 A 180C ET UNE PRESSION DE 1,5 A 10ATM. LA SULFURATION PEUT ETRE OPEREE EN PRESENCE DE SULFATE OU DE CHLORURE DE SODIUM.L'INVENTION PEUT TROUVER DES APPLICATIONS EN METALLURGIE DES METAUX NON FERREUX POUR L'OBTENTION DU CUIVRE ET DE PRODUITS DE VALEUR ASSOCIES, NOTAMMENT L'ARGENT.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_FR2602797A1</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>FR2602797A1</sourcerecordid><originalsourceid>FETCH-epo_espacenet_FR2602797A13</originalsourceid><addsrcrecordid>eNrjZAgKCPJ3dnVxVXBRd_UL8nT28AwOdvV19QtRAIr5evq5Bjl6BoPYzqGeYUGuCv4RkS6uQAFPNzdPZ08fiFK4TkcnH9dgHgbWtMSc4lReKM3NoODmGuLsoZtakB-fWlyQmJyal1oS7xZkZGZgZG5p7mhoTIQSAHH9L00</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>PROCEDE D'ENRICHISSEMENT DE MINERAIS DE CUIVRE OXYDES DIFFICILEMENT ENRICHISSABLES</title><source>esp@cenet</source><creator>N. S. BEKTURGANOV, S. V. BELYAEV, D. N. ABISHEV, V. P. MALYSHEV, G. K. KHAIROVA, S. P. SIM, D. V. SOLOGUB, ZH. M. MAKHMUTOV, A. F. CHUNIN, V. I. REVNIVTSEV, I. SH. SATAEV, M. Y. RYSKIN, S. I. SOBOL, V. V. POPKOV, S. I. KAPITONOV, P. T. ZHMURKO, N. V. MATVEENKO, B. S. ZADOVA, L. A. STRELSKAYA, V. S. CHECHETKIN, G. N. SMIRNOV ET V. K. LAIKIN</creator><creatorcontrib>N. S. BEKTURGANOV, S. V. BELYAEV, D. N. ABISHEV, V. P. MALYSHEV, G. K. KHAIROVA, S. P. SIM, D. V. SOLOGUB, ZH. M. MAKHMUTOV, A. F. CHUNIN, V. I. REVNIVTSEV, I. SH. SATAEV, M. Y. RYSKIN, S. I. SOBOL, V. V. POPKOV, S. I. KAPITONOV, P. T. ZHMURKO, N. V. MATVEENKO, B. S. ZADOVA, L. A. STRELSKAYA, V. S. CHECHETKIN, G. N. SMIRNOV ET V. K. LAIKIN</creatorcontrib><description>The method provides for preparation of a pulp, its sulphidizing and floatation. The sulphidizing of the pulp is effected with melted sulphur at a temperature of 115-180 DEG C and at a pressure of 1.5-10 atm in the presence of sodium sulphate or sodium chloride at a mass ratio between the sulphur and the oxidized copper of (0.2-1.5):1. L'INVENTION CONCERNE LA METALLURGIE DES METAUX NON FERREUX, ET PLUS SPECIALEMENT UN PROCEDE D'ENRICHISSEMENT DE MINERAIS DE CUIVRE OXYDES DIFFICILEMENT ENRICHISSABLES.LE PROCEDE COMPORTE LA PREPARATION D'UNE PULPE, SA SULFURATION ET SA FLOTTATION. LA SULFURATION DE LA PULPE EST EFFECTUEE PAR DU SOUFRE FONDU UNE TEMPERATURE DE 115 A 180C ET UNE PRESSION DE 1,5 A 10ATM. LA SULFURATION PEUT ETRE OPEREE EN PRESENCE DE SULFATE OU DE CHLORURE DE SODIUM.L'INVENTION PEUT TROUVER DES APPLICATIONS EN METALLURGIE DES METAUX NON FERREUX POUR L'OBTENTION DU CUIVRE ET DE PRODUITS DE VALEUR ASSOCIES, NOTAMMENT L'ARGENT.</description><edition>4</edition><language>fre</language><subject>CHEMISTRY ; COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSESC01D OR C01F ; DIFFERENTIAL SEDIMENTATION ; FERROUS OR NON-FERROUS ALLOYS ; FLOTATION ; INORGANIC CHEMISTRY ; MAGNETIC OR ELECTROSTATIC SEPARATION OF SOLID MATERIALS FROM SOLIDMATERIALS OR FLUIDS ; METALLURGY ; PERFORMING OPERATIONS ; PRETREATMENT OF RAW MATERIALS ; PRODUCTION AND REFINING OF METALS ; SEPARATING SOLID MATERIALS USING LIQUIDS OR USING PNEUMATICTABLES OR JIGS ; SEPARATION BY HIGH-VOLTAGE ELECTRIC FIELDS ; SEPARATION OF SOLID MATERIALS USING LIQUIDS OR USING PNEUMATICTABLES OR JIGS ; TRANSPORTING ; TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><creationdate>1988</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19880219&amp;DB=EPODOC&amp;CC=FR&amp;NR=2602797A1$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,777,882,25545,76296</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19880219&amp;DB=EPODOC&amp;CC=FR&amp;NR=2602797A1$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>N. S. BEKTURGANOV, S. V. BELYAEV, D. N. ABISHEV, V. P. MALYSHEV, G. K. KHAIROVA, S. P. SIM, D. V. SOLOGUB, ZH. M. MAKHMUTOV, A. F. CHUNIN, V. I. REVNIVTSEV, I. SH. SATAEV, M. Y. RYSKIN, S. I. SOBOL, V. V. POPKOV, S. I. KAPITONOV, P. T. ZHMURKO, N. V. MATVEENKO, B. S. ZADOVA, L. A. STRELSKAYA, V. S. CHECHETKIN, G. N. SMIRNOV ET V. K. LAIKIN</creatorcontrib><title>PROCEDE D'ENRICHISSEMENT DE MINERAIS DE CUIVRE OXYDES DIFFICILEMENT ENRICHISSABLES</title><description>The method provides for preparation of a pulp, its sulphidizing and floatation. The sulphidizing of the pulp is effected with melted sulphur at a temperature of 115-180 DEG C and at a pressure of 1.5-10 atm in the presence of sodium sulphate or sodium chloride at a mass ratio between the sulphur and the oxidized copper of (0.2-1.5):1. L'INVENTION CONCERNE LA METALLURGIE DES METAUX NON FERREUX, ET PLUS SPECIALEMENT UN PROCEDE D'ENRICHISSEMENT DE MINERAIS DE CUIVRE OXYDES DIFFICILEMENT ENRICHISSABLES.LE PROCEDE COMPORTE LA PREPARATION D'UNE PULPE, SA SULFURATION ET SA FLOTTATION. LA SULFURATION DE LA PULPE EST EFFECTUEE PAR DU SOUFRE FONDU UNE TEMPERATURE DE 115 A 180C ET UNE PRESSION DE 1,5 A 10ATM. LA SULFURATION PEUT ETRE OPEREE EN PRESENCE DE SULFATE OU DE CHLORURE DE SODIUM.L'INVENTION PEUT TROUVER DES APPLICATIONS EN METALLURGIE DES METAUX NON FERREUX POUR L'OBTENTION DU CUIVRE ET DE PRODUITS DE VALEUR ASSOCIES, NOTAMMENT L'ARGENT.</description><subject>CHEMISTRY</subject><subject>COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSESC01D OR C01F</subject><subject>DIFFERENTIAL SEDIMENTATION</subject><subject>FERROUS OR NON-FERROUS ALLOYS</subject><subject>FLOTATION</subject><subject>INORGANIC CHEMISTRY</subject><subject>MAGNETIC OR ELECTROSTATIC SEPARATION OF SOLID MATERIALS FROM SOLIDMATERIALS OR FLUIDS</subject><subject>METALLURGY</subject><subject>PERFORMING OPERATIONS</subject><subject>PRETREATMENT OF RAW MATERIALS</subject><subject>PRODUCTION AND REFINING OF METALS</subject><subject>SEPARATING SOLID MATERIALS USING LIQUIDS OR USING PNEUMATICTABLES OR JIGS</subject><subject>SEPARATION BY HIGH-VOLTAGE ELECTRIC FIELDS</subject><subject>SEPARATION OF SOLID MATERIALS USING LIQUIDS OR USING PNEUMATICTABLES OR JIGS</subject><subject>TRANSPORTING</subject><subject>TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>1988</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZAgKCPJ3dnVxVXBRd_UL8nT28AwOdvV19QtRAIr5evq5Bjl6BoPYzqGeYUGuCv4RkS6uQAFPNzdPZ08fiFK4TkcnH9dgHgbWtMSc4lReKM3NoODmGuLsoZtakB-fWlyQmJyal1oS7xZkZGZgZG5p7mhoTIQSAHH9L00</recordid><startdate>19880219</startdate><enddate>19880219</enddate><creator>N. S. BEKTURGANOV, S. V. BELYAEV, D. N. ABISHEV, V. P. MALYSHEV, G. K. KHAIROVA, S. P. SIM, D. V. SOLOGUB, ZH. M. MAKHMUTOV, A. F. CHUNIN, V. I. REVNIVTSEV, I. SH. SATAEV, M. Y. RYSKIN, S. I. SOBOL, V. V. POPKOV, S. I. KAPITONOV, P. T. ZHMURKO, N. V. MATVEENKO, B. S. ZADOVA, L. A. STRELSKAYA, V. S. CHECHETKIN, G. N. SMIRNOV ET V. K. LAIKIN</creator><scope>EVB</scope></search><sort><creationdate>19880219</creationdate><title>PROCEDE D'ENRICHISSEMENT DE MINERAIS DE CUIVRE OXYDES DIFFICILEMENT ENRICHISSABLES</title><author>N. S. BEKTURGANOV, S. V. BELYAEV, D. N. ABISHEV, V. P. MALYSHEV, G. K. KHAIROVA, S. P. SIM, D. V. SOLOGUB, ZH. M. MAKHMUTOV, A. F. CHUNIN, V. I. REVNIVTSEV, I. SH. SATAEV, M. Y. RYSKIN, S. I. SOBOL, V. V. POPKOV, S. I. KAPITONOV, P. T. ZHMURKO, N. V. MATVEENKO, B. S. ZADOVA, L. A. STRELSKAYA, V. S. CHECHETKIN, G. N. SMIRNOV ET V. K. LAIKIN</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_FR2602797A13</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>fre</language><creationdate>1988</creationdate><topic>CHEMISTRY</topic><topic>COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSESC01D OR C01F</topic><topic>DIFFERENTIAL SEDIMENTATION</topic><topic>FERROUS OR NON-FERROUS ALLOYS</topic><topic>FLOTATION</topic><topic>INORGANIC CHEMISTRY</topic><topic>MAGNETIC OR ELECTROSTATIC SEPARATION OF SOLID MATERIALS FROM SOLIDMATERIALS OR FLUIDS</topic><topic>METALLURGY</topic><topic>PERFORMING OPERATIONS</topic><topic>PRETREATMENT OF RAW MATERIALS</topic><topic>PRODUCTION AND REFINING OF METALS</topic><topic>SEPARATING SOLID MATERIALS USING LIQUIDS OR USING PNEUMATICTABLES OR JIGS</topic><topic>SEPARATION BY HIGH-VOLTAGE ELECTRIC FIELDS</topic><topic>SEPARATION OF SOLID MATERIALS USING LIQUIDS OR USING PNEUMATICTABLES OR JIGS</topic><topic>TRANSPORTING</topic><topic>TREATMENT OF ALLOYS OR NON-FERROUS METALS</topic><toplevel>online_resources</toplevel><creatorcontrib>N. S. BEKTURGANOV, S. V. BELYAEV, D. N. ABISHEV, V. P. MALYSHEV, G. K. KHAIROVA, S. P. SIM, D. V. SOLOGUB, ZH. M. MAKHMUTOV, A. F. CHUNIN, V. I. REVNIVTSEV, I. SH. SATAEV, M. Y. RYSKIN, S. I. SOBOL, V. V. POPKOV, S. I. KAPITONOV, P. T. ZHMURKO, N. V. MATVEENKO, B. S. ZADOVA, L. A. STRELSKAYA, V. S. CHECHETKIN, G. N. SMIRNOV ET V. K. LAIKIN</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>N. S. BEKTURGANOV, S. V. BELYAEV, D. N. ABISHEV, V. P. MALYSHEV, G. K. KHAIROVA, S. P. SIM, D. V. SOLOGUB, ZH. M. MAKHMUTOV, A. F. CHUNIN, V. I. REVNIVTSEV, I. SH. SATAEV, M. Y. RYSKIN, S. I. SOBOL, V. V. POPKOV, S. I. KAPITONOV, P. T. ZHMURKO, N. V. MATVEENKO, B. S. ZADOVA, L. A. STRELSKAYA, V. S. CHECHETKIN, G. N. SMIRNOV ET V. K. LAIKIN</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>PROCEDE D'ENRICHISSEMENT DE MINERAIS DE CUIVRE OXYDES DIFFICILEMENT ENRICHISSABLES</title><date>1988-02-19</date><risdate>1988</risdate><abstract>The method provides for preparation of a pulp, its sulphidizing and floatation. The sulphidizing of the pulp is effected with melted sulphur at a temperature of 115-180 DEG C and at a pressure of 1.5-10 atm in the presence of sodium sulphate or sodium chloride at a mass ratio between the sulphur and the oxidized copper of (0.2-1.5):1. L'INVENTION CONCERNE LA METALLURGIE DES METAUX NON FERREUX, ET PLUS SPECIALEMENT UN PROCEDE D'ENRICHISSEMENT DE MINERAIS DE CUIVRE OXYDES DIFFICILEMENT ENRICHISSABLES.LE PROCEDE COMPORTE LA PREPARATION D'UNE PULPE, SA SULFURATION ET SA FLOTTATION. LA SULFURATION DE LA PULPE EST EFFECTUEE PAR DU SOUFRE FONDU UNE TEMPERATURE DE 115 A 180C ET UNE PRESSION DE 1,5 A 10ATM. LA SULFURATION PEUT ETRE OPEREE EN PRESENCE DE SULFATE OU DE CHLORURE DE SODIUM.L'INVENTION PEUT TROUVER DES APPLICATIONS EN METALLURGIE DES METAUX NON FERREUX POUR L'OBTENTION DU CUIVRE ET DE PRODUITS DE VALEUR ASSOCIES, NOTAMMENT L'ARGENT.</abstract><edition>4</edition><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language fre
recordid cdi_epo_espacenet_FR2602797A1
source esp@cenet
subjects CHEMISTRY
COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSESC01D OR C01F
DIFFERENTIAL SEDIMENTATION
FERROUS OR NON-FERROUS ALLOYS
FLOTATION
INORGANIC CHEMISTRY
MAGNETIC OR ELECTROSTATIC SEPARATION OF SOLID MATERIALS FROM SOLIDMATERIALS OR FLUIDS
METALLURGY
PERFORMING OPERATIONS
PRETREATMENT OF RAW MATERIALS
PRODUCTION AND REFINING OF METALS
SEPARATING SOLID MATERIALS USING LIQUIDS OR USING PNEUMATICTABLES OR JIGS
SEPARATION BY HIGH-VOLTAGE ELECTRIC FIELDS
SEPARATION OF SOLID MATERIALS USING LIQUIDS OR USING PNEUMATICTABLES OR JIGS
TRANSPORTING
TREATMENT OF ALLOYS OR NON-FERROUS METALS
title PROCEDE D'ENRICHISSEMENT DE MINERAIS DE CUIVRE OXYDES DIFFICILEMENT ENRICHISSABLES
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-21T02%3A21%3A59IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=N.%20S.%20BEKTURGANOV,%20S.%20V.%20BELYAEV,%20D.%20N.%20ABISHEV,%20V.%20P.%20MALYSHEV,%20G.%20K.%20KHAIROVA,%20S.%20P.%20SIM,%20D.%20V.%20SOLOGUB,%20ZH.%20M.%20MAKHMUTOV,%20A.%20F.%20CHUNIN,%20V.%20I.%20REVNIVTSEV,%20I.%20SH.%20SATAEV,%20M.%20Y.%20RYSKIN,%20S.%20I.%20SOBOL,%20V.%20V.%20POPKOV,%20S.%20I.%20KAPITONOV,%20P.%20T.%20ZHMURKO,%20N.%20V.%20MATVEENKO,%20B.%20S.%20ZADOVA,%20L.%20A.%20STRELSKAYA,%20V.%20S.%20CHECHETKIN,%20G.%20N.%20SMIRNOV%20ET%20V.%20K.%20LAIKIN&rft.date=1988-02-19&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EFR2602797A1%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true