Method for manufacturing a piezoelectric composite material

This process consists in making the composite material from a mixture of powder of piezoelectric ceramic of a particle size less than 400 m and of a hardenable liquid dielectric binder placed, during hardening of the binder, in a mould provided with orifices 44 for liquid overflow and installed betw...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
1. Verfasser: JEAN-PIERRE BESOMBES ET ROGER THANNBERGER
Format: Patent
Sprache:eng ; fre
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator JEAN-PIERRE BESOMBES ET ROGER THANNBERGER
description This process consists in making the composite material from a mixture of powder of piezoelectric ceramic of a particle size less than 400 m and of a hardenable liquid dielectric binder placed, during hardening of the binder, in a mould provided with orifices 44 for liquid overflow and installed between the plates 45, 46 of a press exerting on it a pressure greater than 40 bars. The figure gives an example of mould for making a piezoelectric composite disc according to the method. This mould, placed between the plates 45, 46 of a press, comprises an annular lateral wall 41, a matching bottom 42 and a lid 43 fitted with orifices 44 for liquid overflow. By virtue of the method, a piezoelectric composite material is obtained which is particularly advantageous for making a piezoelectric sensor sensitive to hydrostatic pressures. CE PROCEDE CONSISTE A REALISER LE MATERIAU COMPOSITE A PARTIR D'UN MELANGE DE POUDRE DE CERAMIQUE PIEZO-ELECTRIQUE DE GRANULOMETRIE INFERIEURE A 400MM ET D'UN LIANT DIELECTRIQUE LIQUIDE DURCISSABLE PLACE, PENDANT LE DURCISSEMENT DU LIANT, DANS UN MOULE POURVU D'ORIFICES 44 DE TROP-PLEIN DE LIQUIDE ET INSTALLE ENTRE LES PLATEAUX 45, 46 D'UNE PRESSE EXERCANT SUR LUI UNE PRESSION SUPERIEURE A 40BARS. LA FIGURE DONNE UN EXEMPLE DE MOULE POUR LA REALISATION D'UN DISQUE COMPOSITE PIEZO-ELECTRIQUE SELON LE PROCEDE. CE MOULE, PLACE ENTRE LES PLATEAUX 45, 46 D'UNE PRESSE COMPORTE UNE PAROI LATERALE ANNULAIRE 41, UN FOND AJUSTE 42 ET UN COUVERCLE 43 MUNI D'ORIFICES DE TROP-PLEIN DE LIQUIDE 44. GRACE AU PROCEDE ON OBTIENT UN MATERIAU COMPOSITE PIEZO-ELECTRIQUE PARTICULIEREMENT AVANTAGEUX POUR LA REALISATION D'UN CAPTEUR PIEZO-ELECTRIQUE SENSIBLE AUX PRESSIONS HYDROSTATIQUES.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_FR2554758A1</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>FR2554758A1</sourcerecordid><originalsourceid>FETCH-epo_espacenet_FR2554758A13</originalsourceid><addsrcrecordid>eNrjZLD2TS3JyE9RSMsvUshNzCtNS0wuKS3KzEtXSFQoyEytyk_NSU0uKcpMVkjOzy3IL84sSQWqK0ktykzM4WFgTUvMKU7lhdLcDApuriHOHrqpBfnxqcUFicmpeakl8W5BRqamJuamFo6GxkQoAQCN6i-p</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Method for manufacturing a piezoelectric composite material</title><source>esp@cenet</source><creator>JEAN-PIERRE BESOMBES ET ROGER THANNBERGER</creator><creatorcontrib>JEAN-PIERRE BESOMBES ET ROGER THANNBERGER</creatorcontrib><description>This process consists in making the composite material from a mixture of powder of piezoelectric ceramic of a particle size less than 400 m and of a hardenable liquid dielectric binder placed, during hardening of the binder, in a mould provided with orifices 44 for liquid overflow and installed between the plates 45, 46 of a press exerting on it a pressure greater than 40 bars. The figure gives an example of mould for making a piezoelectric composite disc according to the method. This mould, placed between the plates 45, 46 of a press, comprises an annular lateral wall 41, a matching bottom 42 and a lid 43 fitted with orifices 44 for liquid overflow. By virtue of the method, a piezoelectric composite material is obtained which is particularly advantageous for making a piezoelectric sensor sensitive to hydrostatic pressures. CE PROCEDE CONSISTE A REALISER LE MATERIAU COMPOSITE A PARTIR D'UN MELANGE DE POUDRE DE CERAMIQUE PIEZO-ELECTRIQUE DE GRANULOMETRIE INFERIEURE A 400MM ET D'UN LIANT DIELECTRIQUE LIQUIDE DURCISSABLE PLACE, PENDANT LE DURCISSEMENT DU LIANT, DANS UN MOULE POURVU D'ORIFICES 44 DE TROP-PLEIN DE LIQUIDE ET INSTALLE ENTRE LES PLATEAUX 45, 46 D'UNE PRESSE EXERCANT SUR LUI UNE PRESSION SUPERIEURE A 40BARS. LA FIGURE DONNE UN EXEMPLE DE MOULE POUR LA REALISATION D'UN DISQUE COMPOSITE PIEZO-ELECTRIQUE SELON LE PROCEDE. CE MOULE, PLACE ENTRE LES PLATEAUX 45, 46 D'UNE PRESSE COMPORTE UNE PAROI LATERALE ANNULAIRE 41, UN FOND AJUSTE 42 ET UN COUVERCLE 43 MUNI D'ORIFICES DE TROP-PLEIN DE LIQUIDE 44. GRACE AU PROCEDE ON OBTIENT UN MATERIAU COMPOSITE PIEZO-ELECTRIQUE PARTICULIEREMENT AVANTAGEUX POUR LA REALISATION D'UN CAPTEUR PIEZO-ELECTRIQUE SENSIBLE AUX PRESSIONS HYDROSTATIQUES.</description><edition>4</edition><language>eng ; fre</language><subject>ARTIFICIAL STONE ; CEMENTS ; CERAMICS ; CHEMISTRY ; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS ; CONCRETE ; ELECTRICITY ; LIME, MAGNESIA ; METALLURGY ; PERFORMING OPERATIONS ; REFRACTORIES ; SHAPING CLAY OR OTHER CERAMIC COMPOSITIONS, SLAG, OR MIXTURESCONTAINING CEMENTITIOUS MATERIAL, e.g. PLASTER ; SLAG ; TRANSPORTING ; TREATMENT OF NATURAL STONE ; WORKING CEMENT, CLAY, OR STONE</subject><creationdate>1985</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19850517&amp;DB=EPODOC&amp;CC=FR&amp;NR=2554758A1$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25562,76317</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19850517&amp;DB=EPODOC&amp;CC=FR&amp;NR=2554758A1$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>JEAN-PIERRE BESOMBES ET ROGER THANNBERGER</creatorcontrib><title>Method for manufacturing a piezoelectric composite material</title><description>This process consists in making the composite material from a mixture of powder of piezoelectric ceramic of a particle size less than 400 m and of a hardenable liquid dielectric binder placed, during hardening of the binder, in a mould provided with orifices 44 for liquid overflow and installed between the plates 45, 46 of a press exerting on it a pressure greater than 40 bars. The figure gives an example of mould for making a piezoelectric composite disc according to the method. This mould, placed between the plates 45, 46 of a press, comprises an annular lateral wall 41, a matching bottom 42 and a lid 43 fitted with orifices 44 for liquid overflow. By virtue of the method, a piezoelectric composite material is obtained which is particularly advantageous for making a piezoelectric sensor sensitive to hydrostatic pressures. CE PROCEDE CONSISTE A REALISER LE MATERIAU COMPOSITE A PARTIR D'UN MELANGE DE POUDRE DE CERAMIQUE PIEZO-ELECTRIQUE DE GRANULOMETRIE INFERIEURE A 400MM ET D'UN LIANT DIELECTRIQUE LIQUIDE DURCISSABLE PLACE, PENDANT LE DURCISSEMENT DU LIANT, DANS UN MOULE POURVU D'ORIFICES 44 DE TROP-PLEIN DE LIQUIDE ET INSTALLE ENTRE LES PLATEAUX 45, 46 D'UNE PRESSE EXERCANT SUR LUI UNE PRESSION SUPERIEURE A 40BARS. LA FIGURE DONNE UN EXEMPLE DE MOULE POUR LA REALISATION D'UN DISQUE COMPOSITE PIEZO-ELECTRIQUE SELON LE PROCEDE. CE MOULE, PLACE ENTRE LES PLATEAUX 45, 46 D'UNE PRESSE COMPORTE UNE PAROI LATERALE ANNULAIRE 41, UN FOND AJUSTE 42 ET UN COUVERCLE 43 MUNI D'ORIFICES DE TROP-PLEIN DE LIQUIDE 44. GRACE AU PROCEDE ON OBTIENT UN MATERIAU COMPOSITE PIEZO-ELECTRIQUE PARTICULIEREMENT AVANTAGEUX POUR LA REALISATION D'UN CAPTEUR PIEZO-ELECTRIQUE SENSIBLE AUX PRESSIONS HYDROSTATIQUES.</description><subject>ARTIFICIAL STONE</subject><subject>CEMENTS</subject><subject>CERAMICS</subject><subject>CHEMISTRY</subject><subject>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</subject><subject>CONCRETE</subject><subject>ELECTRICITY</subject><subject>LIME, MAGNESIA</subject><subject>METALLURGY</subject><subject>PERFORMING OPERATIONS</subject><subject>REFRACTORIES</subject><subject>SHAPING CLAY OR OTHER CERAMIC COMPOSITIONS, SLAG, OR MIXTURESCONTAINING CEMENTITIOUS MATERIAL, e.g. PLASTER</subject><subject>SLAG</subject><subject>TRANSPORTING</subject><subject>TREATMENT OF NATURAL STONE</subject><subject>WORKING CEMENT, CLAY, OR STONE</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>1985</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZLD2TS3JyE9RSMsvUshNzCtNS0wuKS3KzEtXSFQoyEytyk_NSU0uKcpMVkjOzy3IL84sSQWqK0ktykzM4WFgTUvMKU7lhdLcDApuriHOHrqpBfnxqcUFicmpeakl8W5BRqamJuamFo6GxkQoAQCN6i-p</recordid><startdate>19850517</startdate><enddate>19850517</enddate><creator>JEAN-PIERRE BESOMBES ET ROGER THANNBERGER</creator><scope>EVB</scope></search><sort><creationdate>19850517</creationdate><title>Method for manufacturing a piezoelectric composite material</title><author>JEAN-PIERRE BESOMBES ET ROGER THANNBERGER</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_FR2554758A13</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; fre</language><creationdate>1985</creationdate><topic>ARTIFICIAL STONE</topic><topic>CEMENTS</topic><topic>CERAMICS</topic><topic>CHEMISTRY</topic><topic>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</topic><topic>CONCRETE</topic><topic>ELECTRICITY</topic><topic>LIME, MAGNESIA</topic><topic>METALLURGY</topic><topic>PERFORMING OPERATIONS</topic><topic>REFRACTORIES</topic><topic>SHAPING CLAY OR OTHER CERAMIC COMPOSITIONS, SLAG, OR MIXTURESCONTAINING CEMENTITIOUS MATERIAL, e.g. PLASTER</topic><topic>SLAG</topic><topic>TRANSPORTING</topic><topic>TREATMENT OF NATURAL STONE</topic><topic>WORKING CEMENT, CLAY, OR STONE</topic><toplevel>online_resources</toplevel><creatorcontrib>JEAN-PIERRE BESOMBES ET ROGER THANNBERGER</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>JEAN-PIERRE BESOMBES ET ROGER THANNBERGER</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Method for manufacturing a piezoelectric composite material</title><date>1985-05-17</date><risdate>1985</risdate><abstract>This process consists in making the composite material from a mixture of powder of piezoelectric ceramic of a particle size less than 400 m and of a hardenable liquid dielectric binder placed, during hardening of the binder, in a mould provided with orifices 44 for liquid overflow and installed between the plates 45, 46 of a press exerting on it a pressure greater than 40 bars. The figure gives an example of mould for making a piezoelectric composite disc according to the method. This mould, placed between the plates 45, 46 of a press, comprises an annular lateral wall 41, a matching bottom 42 and a lid 43 fitted with orifices 44 for liquid overflow. By virtue of the method, a piezoelectric composite material is obtained which is particularly advantageous for making a piezoelectric sensor sensitive to hydrostatic pressures. CE PROCEDE CONSISTE A REALISER LE MATERIAU COMPOSITE A PARTIR D'UN MELANGE DE POUDRE DE CERAMIQUE PIEZO-ELECTRIQUE DE GRANULOMETRIE INFERIEURE A 400MM ET D'UN LIANT DIELECTRIQUE LIQUIDE DURCISSABLE PLACE, PENDANT LE DURCISSEMENT DU LIANT, DANS UN MOULE POURVU D'ORIFICES 44 DE TROP-PLEIN DE LIQUIDE ET INSTALLE ENTRE LES PLATEAUX 45, 46 D'UNE PRESSE EXERCANT SUR LUI UNE PRESSION SUPERIEURE A 40BARS. LA FIGURE DONNE UN EXEMPLE DE MOULE POUR LA REALISATION D'UN DISQUE COMPOSITE PIEZO-ELECTRIQUE SELON LE PROCEDE. CE MOULE, PLACE ENTRE LES PLATEAUX 45, 46 D'UNE PRESSE COMPORTE UNE PAROI LATERALE ANNULAIRE 41, UN FOND AJUSTE 42 ET UN COUVERCLE 43 MUNI D'ORIFICES DE TROP-PLEIN DE LIQUIDE 44. GRACE AU PROCEDE ON OBTIENT UN MATERIAU COMPOSITE PIEZO-ELECTRIQUE PARTICULIEREMENT AVANTAGEUX POUR LA REALISATION D'UN CAPTEUR PIEZO-ELECTRIQUE SENSIBLE AUX PRESSIONS HYDROSTATIQUES.</abstract><edition>4</edition><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng ; fre
recordid cdi_epo_espacenet_FR2554758A1
source esp@cenet
subjects ARTIFICIAL STONE
CEMENTS
CERAMICS
CHEMISTRY
COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS
CONCRETE
ELECTRICITY
LIME, MAGNESIA
METALLURGY
PERFORMING OPERATIONS
REFRACTORIES
SHAPING CLAY OR OTHER CERAMIC COMPOSITIONS, SLAG, OR MIXTURESCONTAINING CEMENTITIOUS MATERIAL, e.g. PLASTER
SLAG
TRANSPORTING
TREATMENT OF NATURAL STONE
WORKING CEMENT, CLAY, OR STONE
title Method for manufacturing a piezoelectric composite material
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-09T21%3A56%3A39IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=JEAN-PIERRE%20BESOMBES%20ET%20ROGER%20THANNBERGER&rft.date=1985-05-17&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EFR2554758A1%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true