Alunite treatment to obtain useful components - by oxidative roasting, reducing, leaching with sodium hydroxide soln., and calcining pptd. aluminium

The alunite is roasted at 580-620 degrees C in the presence of oxygen for 1-3 hrs. The roasted alunite is contacted with a reducing agent (e.g. kerosene oil) at above this temperature and the resulting reduced alunite is leached with an aq. soln. contg. NaOH. Aluminium hydroxide is thus pptd. with d...