METHOD OF MAKING TITANIA-SILICA GLASS WITH UNIFORM HYDROXIDE CONCENTRATION
A process of forming a titania-silica glass body, the process including exposing a titania-doped silica soot body to a first thermal treatment by heating the body to a first temperature T1 between about 800°C and about 1100°C for a first time duration tl calculated using the equation: t1>Lc24α, w...
Gespeichert in:
Hauptverfasser: | , , |
---|---|
Format: | Patent |
Sprache: | eng ; fre ; ger |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | TANDON, Pushkar CAMPION, Michael John SHUBIN, Sergey Nikolaevich |
description | A process of forming a titania-silica glass body, the process including exposing a titania-doped silica soot body to a first thermal treatment by heating the body to a first temperature T1 between about 800°C and about 1100°C for a first time duration tl calculated using the equation: t1>Lc24α, wherein Lc is the characteristic length (cm) of the body and α is the thermal diffusivity (cm2/sec) of the body. The process further including exposing the body to a second thermal treatment by heating the body to a second temperature T2 between about 1050°C and about 1250°C wherein, after the second thermal treatment, a peak-to-valley difference of hydroxide concentration amongst a plurality of segments of the body is about 70 ppm or less. |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_EP4406921A1</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>EP4406921A1</sourcerecordid><originalsourceid>FETCH-epo_espacenet_EP4406921A13</originalsourceid><addsrcrecordid>eNqNyr0KwjAQAOAsDqK-w71AwWoRHI_8NKdNTpITdSpF4iRaqO-Piw_g9C3fXB2CFc8G2EHAI8UWhAQjYZWpI43QdpgzXEg8nCM5TgH8zSS-krGgOWobJaEQx6WaPYbnVFY_FwqcFe2rMr77Mo3DvbzKp7enplnv9psa6-0f5QsNoS0j</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>METHOD OF MAKING TITANIA-SILICA GLASS WITH UNIFORM HYDROXIDE CONCENTRATION</title><source>esp@cenet</source><creator>TANDON, Pushkar ; CAMPION, Michael John ; SHUBIN, Sergey Nikolaevich</creator><creatorcontrib>TANDON, Pushkar ; CAMPION, Michael John ; SHUBIN, Sergey Nikolaevich</creatorcontrib><description>A process of forming a titania-silica glass body, the process including exposing a titania-doped silica soot body to a first thermal treatment by heating the body to a first temperature T1 between about 800°C and about 1100°C for a first time duration tl calculated using the equation: t1>Lc24α, wherein Lc is the characteristic length (cm) of the body and α is the thermal diffusivity (cm2/sec) of the body. The process further including exposing the body to a second thermal treatment by heating the body to a second temperature T2 between about 1050°C and about 1250°C wherein, after the second thermal treatment, a peak-to-valley difference of hydroxide concentration amongst a plurality of segments of the body is about 70 ppm or less.</description><language>eng ; fre ; ger</language><subject>CHEMISTRY ; GLASS ; MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES ; METALLURGY ; MINERAL OR SLAG WOOL</subject><creationdate>2024</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20240731&DB=EPODOC&CC=EP&NR=4406921A1$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,309,781,886,25569,76552</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20240731&DB=EPODOC&CC=EP&NR=4406921A1$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>TANDON, Pushkar</creatorcontrib><creatorcontrib>CAMPION, Michael John</creatorcontrib><creatorcontrib>SHUBIN, Sergey Nikolaevich</creatorcontrib><title>METHOD OF MAKING TITANIA-SILICA GLASS WITH UNIFORM HYDROXIDE CONCENTRATION</title><description>A process of forming a titania-silica glass body, the process including exposing a titania-doped silica soot body to a first thermal treatment by heating the body to a first temperature T1 between about 800°C and about 1100°C for a first time duration tl calculated using the equation: t1>Lc24α, wherein Lc is the characteristic length (cm) of the body and α is the thermal diffusivity (cm2/sec) of the body. The process further including exposing the body to a second thermal treatment by heating the body to a second temperature T2 between about 1050°C and about 1250°C wherein, after the second thermal treatment, a peak-to-valley difference of hydroxide concentration amongst a plurality of segments of the body is about 70 ppm or less.</description><subject>CHEMISTRY</subject><subject>GLASS</subject><subject>MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES</subject><subject>METALLURGY</subject><subject>MINERAL OR SLAG WOOL</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2024</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNyr0KwjAQAOAsDqK-w71AwWoRHI_8NKdNTpITdSpF4iRaqO-Piw_g9C3fXB2CFc8G2EHAI8UWhAQjYZWpI43QdpgzXEg8nCM5TgH8zSS-krGgOWobJaEQx6WaPYbnVFY_FwqcFe2rMr77Mo3DvbzKp7enplnv9psa6-0f5QsNoS0j</recordid><startdate>20240731</startdate><enddate>20240731</enddate><creator>TANDON, Pushkar</creator><creator>CAMPION, Michael John</creator><creator>SHUBIN, Sergey Nikolaevich</creator><scope>EVB</scope></search><sort><creationdate>20240731</creationdate><title>METHOD OF MAKING TITANIA-SILICA GLASS WITH UNIFORM HYDROXIDE CONCENTRATION</title><author>TANDON, Pushkar ; CAMPION, Michael John ; SHUBIN, Sergey Nikolaevich</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_EP4406921A13</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; fre ; ger</language><creationdate>2024</creationdate><topic>CHEMISTRY</topic><topic>GLASS</topic><topic>MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES</topic><topic>METALLURGY</topic><topic>MINERAL OR SLAG WOOL</topic><toplevel>online_resources</toplevel><creatorcontrib>TANDON, Pushkar</creatorcontrib><creatorcontrib>CAMPION, Michael John</creatorcontrib><creatorcontrib>SHUBIN, Sergey Nikolaevich</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>TANDON, Pushkar</au><au>CAMPION, Michael John</au><au>SHUBIN, Sergey Nikolaevich</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>METHOD OF MAKING TITANIA-SILICA GLASS WITH UNIFORM HYDROXIDE CONCENTRATION</title><date>2024-07-31</date><risdate>2024</risdate><abstract>A process of forming a titania-silica glass body, the process including exposing a titania-doped silica soot body to a first thermal treatment by heating the body to a first temperature T1 between about 800°C and about 1100°C for a first time duration tl calculated using the equation: t1>Lc24α, wherein Lc is the characteristic length (cm) of the body and α is the thermal diffusivity (cm2/sec) of the body. The process further including exposing the body to a second thermal treatment by heating the body to a second temperature T2 between about 1050°C and about 1250°C wherein, after the second thermal treatment, a peak-to-valley difference of hydroxide concentration amongst a plurality of segments of the body is about 70 ppm or less.</abstract><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | eng ; fre ; ger |
recordid | cdi_epo_espacenet_EP4406921A1 |
source | esp@cenet |
subjects | CHEMISTRY GLASS MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES METALLURGY MINERAL OR SLAG WOOL |
title | METHOD OF MAKING TITANIA-SILICA GLASS WITH UNIFORM HYDROXIDE CONCENTRATION |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-15T04%3A37%3A34IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=TANDON,%20Pushkar&rft.date=2024-07-31&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EEP4406921A1%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |