POLAR RESIN COMPOSITION AND MULTILAYER BODY
[Problem] To provide a laminate having a polar resin layer, which is excellent in transparency and mechanical strength (in particular impact resistance), and a polar resin composition for forming the polar resin layer of the laminate having such properties.[Solution] A polar resin composition includ...
Gespeichert in:
Hauptverfasser: | , , , , |
---|---|
Format: | Patent |
Sprache: | eng ; fre ; ger |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | EGAWA, Makoto HOYA, Hiroshi SHIOZAKI, Nao NODA, Kiminori KAI, Yuki |
description | [Problem] To provide a laminate having a polar resin layer, which is excellent in transparency and mechanical strength (in particular impact resistance), and a polar resin composition for forming the polar resin layer of the laminate having such properties.[Solution] A polar resin composition including 5 to 30% by mass of an ethylenic polymer (A), 40 to 85% by mass of a polar resin component (B), and 10 to 40% by mass of a modified ethylene/α-olefin copolymer (C) obtained by modifying an ethylene/α-olefin copolymer (C0) with an unsaturated carboxylic acid or a derivative thereof and having a melt flow rate (190°C, 2.16 kg load) of 0.1 to 50 g/10 minutes, provided that the sum of proportions of the (A), (B), and (C) is 100% by mass. |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_EP4317326A1</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>EP4317326A1</sourcerecordid><originalsourceid>FETCH-epo_espacenet_EP4317326A13</originalsourceid><addsrcrecordid>eNrjZNAO8PdxDFIIcg329FNw9vcN8A_2DPH091Nw9HNR8A31CfH0cYx0DVJw8neJ5GFgTUvMKU7lhdLcDApuriHOHrqpBfnxqcUFicmpeakl8a4BJsaG5sZGZo6GxkQoAQA-4CSq</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>POLAR RESIN COMPOSITION AND MULTILAYER BODY</title><source>esp@cenet</source><creator>EGAWA, Makoto ; HOYA, Hiroshi ; SHIOZAKI, Nao ; NODA, Kiminori ; KAI, Yuki</creator><creatorcontrib>EGAWA, Makoto ; HOYA, Hiroshi ; SHIOZAKI, Nao ; NODA, Kiminori ; KAI, Yuki</creatorcontrib><description>[Problem] To provide a laminate having a polar resin layer, which is excellent in transparency and mechanical strength (in particular impact resistance), and a polar resin composition for forming the polar resin layer of the laminate having such properties.[Solution] A polar resin composition including 5 to 30% by mass of an ethylenic polymer (A), 40 to 85% by mass of a polar resin component (B), and 10 to 40% by mass of a modified ethylene/α-olefin copolymer (C) obtained by modifying an ethylene/α-olefin copolymer (C0) with an unsaturated carboxylic acid or a derivative thereof and having a melt flow rate (190°C, 2.16 kg load) of 0.1 to 50 g/10 minutes, provided that the sum of proportions of the (A), (B), and (C) is 100% by mass.</description><language>eng ; fre ; ger</language><subject>CHEMISTRY ; COMPOSITIONS BASED THEREON ; COMPOSITIONS OF MACROMOLECULAR COMPOUNDS ; LAYERED PRODUCTS ; LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT ORNON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM ; METALLURGY ; ORGANIC MACROMOLECULAR COMPOUNDS ; PERFORMING OPERATIONS ; THEIR PREPARATION OR CHEMICAL WORKING-UP ; TRANSPORTING</subject><creationdate>2024</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20240207&DB=EPODOC&CC=EP&NR=4317326A1$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25543,76293</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20240207&DB=EPODOC&CC=EP&NR=4317326A1$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>EGAWA, Makoto</creatorcontrib><creatorcontrib>HOYA, Hiroshi</creatorcontrib><creatorcontrib>SHIOZAKI, Nao</creatorcontrib><creatorcontrib>NODA, Kiminori</creatorcontrib><creatorcontrib>KAI, Yuki</creatorcontrib><title>POLAR RESIN COMPOSITION AND MULTILAYER BODY</title><description>[Problem] To provide a laminate having a polar resin layer, which is excellent in transparency and mechanical strength (in particular impact resistance), and a polar resin composition for forming the polar resin layer of the laminate having such properties.[Solution] A polar resin composition including 5 to 30% by mass of an ethylenic polymer (A), 40 to 85% by mass of a polar resin component (B), and 10 to 40% by mass of a modified ethylene/α-olefin copolymer (C) obtained by modifying an ethylene/α-olefin copolymer (C0) with an unsaturated carboxylic acid or a derivative thereof and having a melt flow rate (190°C, 2.16 kg load) of 0.1 to 50 g/10 minutes, provided that the sum of proportions of the (A), (B), and (C) is 100% by mass.</description><subject>CHEMISTRY</subject><subject>COMPOSITIONS BASED THEREON</subject><subject>COMPOSITIONS OF MACROMOLECULAR COMPOUNDS</subject><subject>LAYERED PRODUCTS</subject><subject>LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT ORNON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM</subject><subject>METALLURGY</subject><subject>ORGANIC MACROMOLECULAR COMPOUNDS</subject><subject>PERFORMING OPERATIONS</subject><subject>THEIR PREPARATION OR CHEMICAL WORKING-UP</subject><subject>TRANSPORTING</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2024</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZNAO8PdxDFIIcg329FNw9vcN8A_2DPH091Nw9HNR8A31CfH0cYx0DVJw8neJ5GFgTUvMKU7lhdLcDApuriHOHrqpBfnxqcUFicmpeakl8a4BJsaG5sZGZo6GxkQoAQA-4CSq</recordid><startdate>20240207</startdate><enddate>20240207</enddate><creator>EGAWA, Makoto</creator><creator>HOYA, Hiroshi</creator><creator>SHIOZAKI, Nao</creator><creator>NODA, Kiminori</creator><creator>KAI, Yuki</creator><scope>EVB</scope></search><sort><creationdate>20240207</creationdate><title>POLAR RESIN COMPOSITION AND MULTILAYER BODY</title><author>EGAWA, Makoto ; HOYA, Hiroshi ; SHIOZAKI, Nao ; NODA, Kiminori ; KAI, Yuki</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_EP4317326A13</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; fre ; ger</language><creationdate>2024</creationdate><topic>CHEMISTRY</topic><topic>COMPOSITIONS BASED THEREON</topic><topic>COMPOSITIONS OF MACROMOLECULAR COMPOUNDS</topic><topic>LAYERED PRODUCTS</topic><topic>LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT ORNON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM</topic><topic>METALLURGY</topic><topic>ORGANIC MACROMOLECULAR COMPOUNDS</topic><topic>PERFORMING OPERATIONS</topic><topic>THEIR PREPARATION OR CHEMICAL WORKING-UP</topic><topic>TRANSPORTING</topic><toplevel>online_resources</toplevel><creatorcontrib>EGAWA, Makoto</creatorcontrib><creatorcontrib>HOYA, Hiroshi</creatorcontrib><creatorcontrib>SHIOZAKI, Nao</creatorcontrib><creatorcontrib>NODA, Kiminori</creatorcontrib><creatorcontrib>KAI, Yuki</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>EGAWA, Makoto</au><au>HOYA, Hiroshi</au><au>SHIOZAKI, Nao</au><au>NODA, Kiminori</au><au>KAI, Yuki</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>POLAR RESIN COMPOSITION AND MULTILAYER BODY</title><date>2024-02-07</date><risdate>2024</risdate><abstract>[Problem] To provide a laminate having a polar resin layer, which is excellent in transparency and mechanical strength (in particular impact resistance), and a polar resin composition for forming the polar resin layer of the laminate having such properties.[Solution] A polar resin composition including 5 to 30% by mass of an ethylenic polymer (A), 40 to 85% by mass of a polar resin component (B), and 10 to 40% by mass of a modified ethylene/α-olefin copolymer (C) obtained by modifying an ethylene/α-olefin copolymer (C0) with an unsaturated carboxylic acid or a derivative thereof and having a melt flow rate (190°C, 2.16 kg load) of 0.1 to 50 g/10 minutes, provided that the sum of proportions of the (A), (B), and (C) is 100% by mass.</abstract><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | eng ; fre ; ger |
recordid | cdi_epo_espacenet_EP4317326A1 |
source | esp@cenet |
subjects | CHEMISTRY COMPOSITIONS BASED THEREON COMPOSITIONS OF MACROMOLECULAR COMPOUNDS LAYERED PRODUCTS LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT ORNON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM METALLURGY ORGANIC MACROMOLECULAR COMPOUNDS PERFORMING OPERATIONS THEIR PREPARATION OR CHEMICAL WORKING-UP TRANSPORTING |
title | POLAR RESIN COMPOSITION AND MULTILAYER BODY |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-26T05%3A27%3A27IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=EGAWA,%20Makoto&rft.date=2024-02-07&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EEP4317326A1%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |