FIBER-REINFORCED PROPYLENE POLYMER COMPOSITION

A fiber-reinforced polymer composition comprising from about 60 wt. % to about 90 wt. % of a polymer matrix that contains a propylene polymer and from about 10 wt. % to about 40 wt. % of a plurality of long reinforcing fibers that are distributed within the polymer matrix, is provided. The polymer c...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: EASTEP, David W, JOHNSON, Aaron H
Format: Patent
Sprache:eng ; fre ; ger
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator EASTEP, David W
JOHNSON, Aaron H
description A fiber-reinforced polymer composition comprising from about 60 wt. % to about 90 wt. % of a polymer matrix that contains a propylene polymer and from about 10 wt. % to about 40 wt. % of a plurality of long reinforcing fibers that are distributed within the polymer matrix, is provided. The polymer composition exhibits a dielectric constant of about 4 or less and dissipation factor of about 0.01 or less at a frequency of 2 GHz. Further, the polymer composition exhibits a Charpy unnotched impact strength of about 20 kJ/m2 or more as determined in accordance with ISO Test No. 179-1:2010 at a temperature of about 23° C., and a Limiting Oxygen Index of about 25 or more as determined in accordance with ISO 4589:2017.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_EP4263632A1</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>EP4263632A1</sourcerecordid><originalsourceid>FETCH-epo_espacenet_EP4263632A13</originalsourceid><addsrcrecordid>eNrjZNBz83RyDdINcvX0c_MPcnZ1UQgI8g-I9HH1c1UI8PeJ9HUNUnD29w3wD_YM8fT342FgTUvMKU7lhdLcDApuriHOHrqpBfnxqcUFicmpeakl8a4BJkZmxmbGRo6GxkQoAQDElSXB</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>FIBER-REINFORCED PROPYLENE POLYMER COMPOSITION</title><source>esp@cenet</source><creator>EASTEP, David W ; JOHNSON, Aaron H</creator><creatorcontrib>EASTEP, David W ; JOHNSON, Aaron H</creatorcontrib><description>A fiber-reinforced polymer composition comprising from about 60 wt. % to about 90 wt. % of a polymer matrix that contains a propylene polymer and from about 10 wt. % to about 40 wt. % of a plurality of long reinforcing fibers that are distributed within the polymer matrix, is provided. The polymer composition exhibits a dielectric constant of about 4 or less and dissipation factor of about 0.01 or less at a frequency of 2 GHz. Further, the polymer composition exhibits a Charpy unnotched impact strength of about 20 kJ/m2 or more as determined in accordance with ISO Test No. 179-1:2010 at a temperature of about 23° C., and a Limiting Oxygen Index of about 25 or more as determined in accordance with ISO 4589:2017.</description><language>eng ; fre ; ger</language><subject>AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F,C08G ; CHEMISTRY ; COMPOSITIONS BASED THEREON ; GENERAL PROCESSES OF COMPOUNDING ; MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVINGCARBON-TO-CARBON UNSATURATED BONDS ; METALLURGY ; ORGANIC MACROMOLECULAR COMPOUNDS ; THEIR PREPARATION OR CHEMICAL WORKING-UP ; USE OF INORGANIC OR NON-MACROMOLECULAR ORGANIC SUBSTANCES ASCOMPOUNDING INGREDIENTS ; WORKING-UP</subject><creationdate>2023</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20231025&amp;DB=EPODOC&amp;CC=EP&amp;NR=4263632A1$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76290</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20231025&amp;DB=EPODOC&amp;CC=EP&amp;NR=4263632A1$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>EASTEP, David W</creatorcontrib><creatorcontrib>JOHNSON, Aaron H</creatorcontrib><title>FIBER-REINFORCED PROPYLENE POLYMER COMPOSITION</title><description>A fiber-reinforced polymer composition comprising from about 60 wt. % to about 90 wt. % of a polymer matrix that contains a propylene polymer and from about 10 wt. % to about 40 wt. % of a plurality of long reinforcing fibers that are distributed within the polymer matrix, is provided. The polymer composition exhibits a dielectric constant of about 4 or less and dissipation factor of about 0.01 or less at a frequency of 2 GHz. Further, the polymer composition exhibits a Charpy unnotched impact strength of about 20 kJ/m2 or more as determined in accordance with ISO Test No. 179-1:2010 at a temperature of about 23° C., and a Limiting Oxygen Index of about 25 or more as determined in accordance with ISO 4589:2017.</description><subject>AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F,C08G</subject><subject>CHEMISTRY</subject><subject>COMPOSITIONS BASED THEREON</subject><subject>GENERAL PROCESSES OF COMPOUNDING</subject><subject>MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVINGCARBON-TO-CARBON UNSATURATED BONDS</subject><subject>METALLURGY</subject><subject>ORGANIC MACROMOLECULAR COMPOUNDS</subject><subject>THEIR PREPARATION OR CHEMICAL WORKING-UP</subject><subject>USE OF INORGANIC OR NON-MACROMOLECULAR ORGANIC SUBSTANCES ASCOMPOUNDING INGREDIENTS</subject><subject>WORKING-UP</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2023</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZNBz83RyDdINcvX0c_MPcnZ1UQgI8g-I9HH1c1UI8PeJ9HUNUnD29w3wD_YM8fT342FgTUvMKU7lhdLcDApuriHOHrqpBfnxqcUFicmpeakl8a4BJkZmxmbGRo6GxkQoAQDElSXB</recordid><startdate>20231025</startdate><enddate>20231025</enddate><creator>EASTEP, David W</creator><creator>JOHNSON, Aaron H</creator><scope>EVB</scope></search><sort><creationdate>20231025</creationdate><title>FIBER-REINFORCED PROPYLENE POLYMER COMPOSITION</title><author>EASTEP, David W ; JOHNSON, Aaron H</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_EP4263632A13</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; fre ; ger</language><creationdate>2023</creationdate><topic>AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F,C08G</topic><topic>CHEMISTRY</topic><topic>COMPOSITIONS BASED THEREON</topic><topic>GENERAL PROCESSES OF COMPOUNDING</topic><topic>MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVINGCARBON-TO-CARBON UNSATURATED BONDS</topic><topic>METALLURGY</topic><topic>ORGANIC MACROMOLECULAR COMPOUNDS</topic><topic>THEIR PREPARATION OR CHEMICAL WORKING-UP</topic><topic>USE OF INORGANIC OR NON-MACROMOLECULAR ORGANIC SUBSTANCES ASCOMPOUNDING INGREDIENTS</topic><topic>WORKING-UP</topic><toplevel>online_resources</toplevel><creatorcontrib>EASTEP, David W</creatorcontrib><creatorcontrib>JOHNSON, Aaron H</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>EASTEP, David W</au><au>JOHNSON, Aaron H</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>FIBER-REINFORCED PROPYLENE POLYMER COMPOSITION</title><date>2023-10-25</date><risdate>2023</risdate><abstract>A fiber-reinforced polymer composition comprising from about 60 wt. % to about 90 wt. % of a polymer matrix that contains a propylene polymer and from about 10 wt. % to about 40 wt. % of a plurality of long reinforcing fibers that are distributed within the polymer matrix, is provided. The polymer composition exhibits a dielectric constant of about 4 or less and dissipation factor of about 0.01 or less at a frequency of 2 GHz. Further, the polymer composition exhibits a Charpy unnotched impact strength of about 20 kJ/m2 or more as determined in accordance with ISO Test No. 179-1:2010 at a temperature of about 23° C., and a Limiting Oxygen Index of about 25 or more as determined in accordance with ISO 4589:2017.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng ; fre ; ger
recordid cdi_epo_espacenet_EP4263632A1
source esp@cenet
subjects AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F,C08G
CHEMISTRY
COMPOSITIONS BASED THEREON
GENERAL PROCESSES OF COMPOUNDING
MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVINGCARBON-TO-CARBON UNSATURATED BONDS
METALLURGY
ORGANIC MACROMOLECULAR COMPOUNDS
THEIR PREPARATION OR CHEMICAL WORKING-UP
USE OF INORGANIC OR NON-MACROMOLECULAR ORGANIC SUBSTANCES ASCOMPOUNDING INGREDIENTS
WORKING-UP
title FIBER-REINFORCED PROPYLENE POLYMER COMPOSITION
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-02T16%3A58%3A46IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=EASTEP,%20David%20W&rft.date=2023-10-25&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EEP4263632A1%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true