COVER PANE WITH AN ANOMALOUS STRESS PROFILE, METHOD FOR ITS PRODUCTION AND ITS USE

Die Erfindung betrifft allgemein Deckscheiben, insbesondere Deckscheiben für elektronische Anzeigegeräte. Weiterhin betrifft die Erfindung ein Verfahren zur Herstellung einer solchen Deckscheibe sowie deren Verwendung. A cover glass is provided that includes a silica based glass ceramic with a thick...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: KOCH, Julian, MÜLLER, Dr. Lars, PFEIFFER, Dr. Thomas, RÜDINGER, Bernd Dr, SCHNEIDER, Meike Dr, ALKEMPER, Dr. Jochen, DIETRICH, Dr. Rüdiger
Format: Patent
Sprache:eng ; fre ; ger
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator KOCH, Julian
MÜLLER, Dr. Lars
PFEIFFER, Dr. Thomas
RÜDINGER, Bernd Dr
SCHNEIDER, Meike Dr
ALKEMPER, Dr. Jochen
DIETRICH, Dr. Rüdiger
description Die Erfindung betrifft allgemein Deckscheiben, insbesondere Deckscheiben für elektronische Anzeigegeräte. Weiterhin betrifft die Erfindung ein Verfahren zur Herstellung einer solchen Deckscheibe sowie deren Verwendung. A cover glass is provided that includes a silica based glass ceramic with a thickness between 0.4 mm and 0.85 mm. The glass ceramic has a transmittance of more than 80% from 380 nm to 780 nm and a stress attribute selected from: an overall compressive stress (CS) of at least 250 MPa and at most 1500 MPa, a compressive stress at a depth of 30 μm (CS30) from one of the two faces of at least 160 MPa and at most 525 MPa, a depth of the compression layer (DoCL) of at least 0.2 times the thickness and less than 0.5 times the thickness, and any combinations thereof. The glass ceramic has at least one silica based crystal phase having in a near-surface layer a unit cell volume of at least 1% by volume larger than that of a core where the crystal phase has minimum stresses.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_EP4194414A1</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>EP4194414A1</sourcerecordid><originalsourceid>FETCH-epo_espacenet_EP4194414A13</originalsourceid><addsrcrecordid>eNrjZAhy9g9zDVIIcPRzVQj3DPFQcPQDIn9fRx__0GCF4JAg1-BghYAgfzdPH1cdBV_XEA9_FwU3_yAFzxCwuEuoc4inP0iPC1goNNiVh4E1LTGnOJUXSnMzKLi5hjh76KYW5MenFhckJqfmpZbEuwaYGFqamBiaOBoaE6EEAF68LwQ</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>COVER PANE WITH AN ANOMALOUS STRESS PROFILE, METHOD FOR ITS PRODUCTION AND ITS USE</title><source>esp@cenet</source><creator>KOCH, Julian ; MÜLLER, Dr. Lars ; PFEIFFER, Dr. Thomas ; RÜDINGER, Bernd Dr ; SCHNEIDER, Meike Dr ; ALKEMPER, Dr. Jochen ; DIETRICH, Dr. Rüdiger</creator><creatorcontrib>KOCH, Julian ; MÜLLER, Dr. Lars ; PFEIFFER, Dr. Thomas ; RÜDINGER, Bernd Dr ; SCHNEIDER, Meike Dr ; ALKEMPER, Dr. Jochen ; DIETRICH, Dr. Rüdiger</creatorcontrib><description>Die Erfindung betrifft allgemein Deckscheiben, insbesondere Deckscheiben für elektronische Anzeigegeräte. Weiterhin betrifft die Erfindung ein Verfahren zur Herstellung einer solchen Deckscheibe sowie deren Verwendung. A cover glass is provided that includes a silica based glass ceramic with a thickness between 0.4 mm and 0.85 mm. The glass ceramic has a transmittance of more than 80% from 380 nm to 780 nm and a stress attribute selected from: an overall compressive stress (CS) of at least 250 MPa and at most 1500 MPa, a compressive stress at a depth of 30 μm (CS30) from one of the two faces of at least 160 MPa and at most 525 MPa, a depth of the compression layer (DoCL) of at least 0.2 times the thickness and less than 0.5 times the thickness, and any combinations thereof. The glass ceramic has at least one silica based crystal phase having in a near-surface layer a unit cell volume of at least 1% by volume larger than that of a core where the crystal phase has minimum stresses.</description><language>eng ; fre ; ger</language><subject>CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS ; CHEMISTRY ; GLASS ; JOINING GLASS TO GLASS OR OTHER MATERIALS ; METALLURGY ; MINERAL OR SLAG WOOL ; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS ; SURFACE TREATMENT OF GLASS</subject><creationdate>2023</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20230614&amp;DB=EPODOC&amp;CC=EP&amp;NR=4194414A1$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20230614&amp;DB=EPODOC&amp;CC=EP&amp;NR=4194414A1$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>KOCH, Julian</creatorcontrib><creatorcontrib>MÜLLER, Dr. Lars</creatorcontrib><creatorcontrib>PFEIFFER, Dr. Thomas</creatorcontrib><creatorcontrib>RÜDINGER, Bernd Dr</creatorcontrib><creatorcontrib>SCHNEIDER, Meike Dr</creatorcontrib><creatorcontrib>ALKEMPER, Dr. Jochen</creatorcontrib><creatorcontrib>DIETRICH, Dr. Rüdiger</creatorcontrib><title>COVER PANE WITH AN ANOMALOUS STRESS PROFILE, METHOD FOR ITS PRODUCTION AND ITS USE</title><description>Die Erfindung betrifft allgemein Deckscheiben, insbesondere Deckscheiben für elektronische Anzeigegeräte. Weiterhin betrifft die Erfindung ein Verfahren zur Herstellung einer solchen Deckscheibe sowie deren Verwendung. A cover glass is provided that includes a silica based glass ceramic with a thickness between 0.4 mm and 0.85 mm. The glass ceramic has a transmittance of more than 80% from 380 nm to 780 nm and a stress attribute selected from: an overall compressive stress (CS) of at least 250 MPa and at most 1500 MPa, a compressive stress at a depth of 30 μm (CS30) from one of the two faces of at least 160 MPa and at most 525 MPa, a depth of the compression layer (DoCL) of at least 0.2 times the thickness and less than 0.5 times the thickness, and any combinations thereof. The glass ceramic has at least one silica based crystal phase having in a near-surface layer a unit cell volume of at least 1% by volume larger than that of a core where the crystal phase has minimum stresses.</description><subject>CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS</subject><subject>CHEMISTRY</subject><subject>GLASS</subject><subject>JOINING GLASS TO GLASS OR OTHER MATERIALS</subject><subject>METALLURGY</subject><subject>MINERAL OR SLAG WOOL</subject><subject>SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS</subject><subject>SURFACE TREATMENT OF GLASS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2023</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZAhy9g9zDVIIcPRzVQj3DPFQcPQDIn9fRx__0GCF4JAg1-BghYAgfzdPH1cdBV_XEA9_FwU3_yAFzxCwuEuoc4inP0iPC1goNNiVh4E1LTGnOJUXSnMzKLi5hjh76KYW5MenFhckJqfmpZbEuwaYGFqamBiaOBoaE6EEAF68LwQ</recordid><startdate>20230614</startdate><enddate>20230614</enddate><creator>KOCH, Julian</creator><creator>MÜLLER, Dr. Lars</creator><creator>PFEIFFER, Dr. Thomas</creator><creator>RÜDINGER, Bernd Dr</creator><creator>SCHNEIDER, Meike Dr</creator><creator>ALKEMPER, Dr. Jochen</creator><creator>DIETRICH, Dr. Rüdiger</creator><scope>EVB</scope></search><sort><creationdate>20230614</creationdate><title>COVER PANE WITH AN ANOMALOUS STRESS PROFILE, METHOD FOR ITS PRODUCTION AND ITS USE</title><author>KOCH, Julian ; MÜLLER, Dr. Lars ; PFEIFFER, Dr. Thomas ; RÜDINGER, Bernd Dr ; SCHNEIDER, Meike Dr ; ALKEMPER, Dr. Jochen ; DIETRICH, Dr. Rüdiger</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_EP4194414A13</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; fre ; ger</language><creationdate>2023</creationdate><topic>CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS</topic><topic>CHEMISTRY</topic><topic>GLASS</topic><topic>JOINING GLASS TO GLASS OR OTHER MATERIALS</topic><topic>METALLURGY</topic><topic>MINERAL OR SLAG WOOL</topic><topic>SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS</topic><topic>SURFACE TREATMENT OF GLASS</topic><toplevel>online_resources</toplevel><creatorcontrib>KOCH, Julian</creatorcontrib><creatorcontrib>MÜLLER, Dr. Lars</creatorcontrib><creatorcontrib>PFEIFFER, Dr. Thomas</creatorcontrib><creatorcontrib>RÜDINGER, Bernd Dr</creatorcontrib><creatorcontrib>SCHNEIDER, Meike Dr</creatorcontrib><creatorcontrib>ALKEMPER, Dr. Jochen</creatorcontrib><creatorcontrib>DIETRICH, Dr. Rüdiger</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>KOCH, Julian</au><au>MÜLLER, Dr. Lars</au><au>PFEIFFER, Dr. Thomas</au><au>RÜDINGER, Bernd Dr</au><au>SCHNEIDER, Meike Dr</au><au>ALKEMPER, Dr. Jochen</au><au>DIETRICH, Dr. Rüdiger</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>COVER PANE WITH AN ANOMALOUS STRESS PROFILE, METHOD FOR ITS PRODUCTION AND ITS USE</title><date>2023-06-14</date><risdate>2023</risdate><abstract>Die Erfindung betrifft allgemein Deckscheiben, insbesondere Deckscheiben für elektronische Anzeigegeräte. Weiterhin betrifft die Erfindung ein Verfahren zur Herstellung einer solchen Deckscheibe sowie deren Verwendung. A cover glass is provided that includes a silica based glass ceramic with a thickness between 0.4 mm and 0.85 mm. The glass ceramic has a transmittance of more than 80% from 380 nm to 780 nm and a stress attribute selected from: an overall compressive stress (CS) of at least 250 MPa and at most 1500 MPa, a compressive stress at a depth of 30 μm (CS30) from one of the two faces of at least 160 MPa and at most 525 MPa, a depth of the compression layer (DoCL) of at least 0.2 times the thickness and less than 0.5 times the thickness, and any combinations thereof. The glass ceramic has at least one silica based crystal phase having in a near-surface layer a unit cell volume of at least 1% by volume larger than that of a core where the crystal phase has minimum stresses.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng ; fre ; ger
recordid cdi_epo_espacenet_EP4194414A1
source esp@cenet
subjects CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS
CHEMISTRY
GLASS
JOINING GLASS TO GLASS OR OTHER MATERIALS
METALLURGY
MINERAL OR SLAG WOOL
SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS
SURFACE TREATMENT OF GLASS
title COVER PANE WITH AN ANOMALOUS STRESS PROFILE, METHOD FOR ITS PRODUCTION AND ITS USE
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-29T16%3A26%3A38IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=KOCH,%20Julian&rft.date=2023-06-14&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EEP4194414A1%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true