METHOD FOR PREPARING HIGH-CONCENTRATION PENTA-TWINNED GOLD NANOPARTICLES

The present invention concerns a method for preparing penta-twinned gold nanoparticles comprising at least the following steps: i) providing a suspension of gold seeds comprising gold seeds, a cationic surfactant and at least one inert solvent, the temperature of the suspension being between 30 and...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: PAROLA, Stéphane, SANTUCCI, Stéphane, CHATEAU, Denis
Format: Patent
Sprache:eng ; fre ; ger
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator PAROLA, Stéphane
SANTUCCI, Stéphane
CHATEAU, Denis
description The present invention concerns a method for preparing penta-twinned gold nanoparticles comprising at least the following steps: i) providing a suspension of gold seeds comprising gold seeds, a cationic surfactant and at least one inert solvent, the temperature of the suspension being between 30 and 75°C; ii) providing a growth solution comprising a gold salt, a cationic surfactant, a reducing agent, the reducing agent being an aromatic compound comprising at least one aromatic ring carrying at least one hydroxyl group, and optionally at least one base; iii) subjecting the suspension of gold seeds from step i) to a growth treatment comprising the following steps: iii1) adding the growth solution from step ii) in a controlled manner to the suspension of gold seeds from step i); iii2) maintaining the temperature of the mixture obtained in step iii1) at a temperature of between 30°C and 75°C for at least 5 minutes. The invention also concerns a nanosuspension likely to be obtained according to the method of the invention, and the use of same for manufacturing an optical sensor.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_EP3987086A1</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>EP3987086A1</sourcerecordid><originalsourceid>FETCH-epo_espacenet_EP3987086A13</originalsourceid><addsrcrecordid>eNrjZPDwdQ3x8HdRcPMPUggIcg1wDPL0c1fw8HT30HX293N29QsJcgzx9PdTCAAyHXVDwj39_FxdFNz9fVwU_Bz9_IEaQjydfVyDeRhY0xJzilN5oTQ3g4Kba4izh25qQX58anFBYnJqXmpJvGuAsaWFuYGFmaOhMRFKAM7nLNQ</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>METHOD FOR PREPARING HIGH-CONCENTRATION PENTA-TWINNED GOLD NANOPARTICLES</title><source>esp@cenet</source><creator>PAROLA, Stéphane ; SANTUCCI, Stéphane ; CHATEAU, Denis</creator><creatorcontrib>PAROLA, Stéphane ; SANTUCCI, Stéphane ; CHATEAU, Denis</creatorcontrib><description>The present invention concerns a method for preparing penta-twinned gold nanoparticles comprising at least the following steps: i) providing a suspension of gold seeds comprising gold seeds, a cationic surfactant and at least one inert solvent, the temperature of the suspension being between 30 and 75°C; ii) providing a growth solution comprising a gold salt, a cationic surfactant, a reducing agent, the reducing agent being an aromatic compound comprising at least one aromatic ring carrying at least one hydroxyl group, and optionally at least one base; iii) subjecting the suspension of gold seeds from step i) to a growth treatment comprising the following steps: iii1) adding the growth solution from step ii) in a controlled manner to the suspension of gold seeds from step i); iii2) maintaining the temperature of the mixture obtained in step iii1) at a temperature of between 30°C and 75°C for at least 5 minutes. The invention also concerns a nanosuspension likely to be obtained according to the method of the invention, and the use of same for manufacturing an optical sensor.</description><language>eng ; fre ; ger</language><subject>AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUSPOLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE ; APPARATUS THEREFOR ; CHEMISTRY ; CRYSTAL GROWTH ; METALLURGY ; PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITHDEFINED STRUCTURE ; REFINING BY ZONE-MELTING OF MATERIAL ; SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITHDEFINED STRUCTURE ; SINGLE-CRYSTAL-GROWTH ; UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL ORUNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL</subject><creationdate>2022</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20220427&amp;DB=EPODOC&amp;CC=EP&amp;NR=3987086A1$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20220427&amp;DB=EPODOC&amp;CC=EP&amp;NR=3987086A1$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>PAROLA, Stéphane</creatorcontrib><creatorcontrib>SANTUCCI, Stéphane</creatorcontrib><creatorcontrib>CHATEAU, Denis</creatorcontrib><title>METHOD FOR PREPARING HIGH-CONCENTRATION PENTA-TWINNED GOLD NANOPARTICLES</title><description>The present invention concerns a method for preparing penta-twinned gold nanoparticles comprising at least the following steps: i) providing a suspension of gold seeds comprising gold seeds, a cationic surfactant and at least one inert solvent, the temperature of the suspension being between 30 and 75°C; ii) providing a growth solution comprising a gold salt, a cationic surfactant, a reducing agent, the reducing agent being an aromatic compound comprising at least one aromatic ring carrying at least one hydroxyl group, and optionally at least one base; iii) subjecting the suspension of gold seeds from step i) to a growth treatment comprising the following steps: iii1) adding the growth solution from step ii) in a controlled manner to the suspension of gold seeds from step i); iii2) maintaining the temperature of the mixture obtained in step iii1) at a temperature of between 30°C and 75°C for at least 5 minutes. The invention also concerns a nanosuspension likely to be obtained according to the method of the invention, and the use of same for manufacturing an optical sensor.</description><subject>AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUSPOLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE</subject><subject>APPARATUS THEREFOR</subject><subject>CHEMISTRY</subject><subject>CRYSTAL GROWTH</subject><subject>METALLURGY</subject><subject>PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITHDEFINED STRUCTURE</subject><subject>REFINING BY ZONE-MELTING OF MATERIAL</subject><subject>SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITHDEFINED STRUCTURE</subject><subject>SINGLE-CRYSTAL-GROWTH</subject><subject>UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL ORUNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2022</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZPDwdQ3x8HdRcPMPUggIcg1wDPL0c1fw8HT30HX293N29QsJcgzx9PdTCAAyHXVDwj39_FxdFNz9fVwU_Bz9_IEaQjydfVyDeRhY0xJzilN5oTQ3g4Kba4izh25qQX58anFBYnJqXmpJvGuAsaWFuYGFmaOhMRFKAM7nLNQ</recordid><startdate>20220427</startdate><enddate>20220427</enddate><creator>PAROLA, Stéphane</creator><creator>SANTUCCI, Stéphane</creator><creator>CHATEAU, Denis</creator><scope>EVB</scope></search><sort><creationdate>20220427</creationdate><title>METHOD FOR PREPARING HIGH-CONCENTRATION PENTA-TWINNED GOLD NANOPARTICLES</title><author>PAROLA, Stéphane ; SANTUCCI, Stéphane ; CHATEAU, Denis</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_EP3987086A13</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; fre ; ger</language><creationdate>2022</creationdate><topic>AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUSPOLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE</topic><topic>APPARATUS THEREFOR</topic><topic>CHEMISTRY</topic><topic>CRYSTAL GROWTH</topic><topic>METALLURGY</topic><topic>PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITHDEFINED STRUCTURE</topic><topic>REFINING BY ZONE-MELTING OF MATERIAL</topic><topic>SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITHDEFINED STRUCTURE</topic><topic>SINGLE-CRYSTAL-GROWTH</topic><topic>UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL ORUNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL</topic><toplevel>online_resources</toplevel><creatorcontrib>PAROLA, Stéphane</creatorcontrib><creatorcontrib>SANTUCCI, Stéphane</creatorcontrib><creatorcontrib>CHATEAU, Denis</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>PAROLA, Stéphane</au><au>SANTUCCI, Stéphane</au><au>CHATEAU, Denis</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>METHOD FOR PREPARING HIGH-CONCENTRATION PENTA-TWINNED GOLD NANOPARTICLES</title><date>2022-04-27</date><risdate>2022</risdate><abstract>The present invention concerns a method for preparing penta-twinned gold nanoparticles comprising at least the following steps: i) providing a suspension of gold seeds comprising gold seeds, a cationic surfactant and at least one inert solvent, the temperature of the suspension being between 30 and 75°C; ii) providing a growth solution comprising a gold salt, a cationic surfactant, a reducing agent, the reducing agent being an aromatic compound comprising at least one aromatic ring carrying at least one hydroxyl group, and optionally at least one base; iii) subjecting the suspension of gold seeds from step i) to a growth treatment comprising the following steps: iii1) adding the growth solution from step ii) in a controlled manner to the suspension of gold seeds from step i); iii2) maintaining the temperature of the mixture obtained in step iii1) at a temperature of between 30°C and 75°C for at least 5 minutes. The invention also concerns a nanosuspension likely to be obtained according to the method of the invention, and the use of same for manufacturing an optical sensor.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng ; fre ; ger
recordid cdi_epo_espacenet_EP3987086A1
source esp@cenet
subjects AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUSPOLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE
APPARATUS THEREFOR
CHEMISTRY
CRYSTAL GROWTH
METALLURGY
PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITHDEFINED STRUCTURE
REFINING BY ZONE-MELTING OF MATERIAL
SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITHDEFINED STRUCTURE
SINGLE-CRYSTAL-GROWTH
UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL ORUNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL
title METHOD FOR PREPARING HIGH-CONCENTRATION PENTA-TWINNED GOLD NANOPARTICLES
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-07T12%3A56%3A29IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=PAROLA,%20St%C3%A9phane&rft.date=2022-04-27&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EEP3987086A1%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true