METHOD FOR CONTINUOUS STEEL CASTING

Provided is a method for continuously casting steel capable of reducing center segregation that occurs in a slab.In the method for continuously casting steel according to the present invention, in a section in a continuous casting machine in a slab withdrawal direction, a section from a start point...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: KOKUFU Sho, SUGIHARA Hirokazu, MATSUI Akitoshi, OSUKA Kenichi, FUKUDA Hiroyuki, IRIE Shuhei, UEOKA Satoshi, ARAMAKI Norichika
Format: Patent
Sprache:eng ; fre ; ger
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator KOKUFU Sho
SUGIHARA Hirokazu
MATSUI Akitoshi
OSUKA Kenichi
FUKUDA Hiroyuki
IRIE Shuhei
UEOKA Satoshi
ARAMAKI Norichika
description Provided is a method for continuously casting steel capable of reducing center segregation that occurs in a slab.In the method for continuously casting steel according to the present invention, in a section in a continuous casting machine in a slab withdrawal direction, a section from a start point at which the average value of solid phase ratios along a thickness direction at a widthwise center of a slab 18 is within a range of 0.4 or more and 0.8 or less to an end point at which the average value of solid phase ratios along the thickness direction at the widthwise center of the slab is greater than the average value of solid phase ratios at the start point and is 1.0 or less is set as a first section, and the slab is cooled by water in the first section at a water flow rate per surface area of the slab within a range of 50 L/(m2×min) or more and 2,000 L/(m2×min) or less.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_EP3932586A1</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>EP3932586A1</sourcerecordid><originalsourceid>FETCH-epo_espacenet_EP3932586A13</originalsourceid><addsrcrecordid>eNrjZFD2dQ3x8HdRcPMPUnD29wvx9Av1Dw1WCA5xdfVRcHYMBgq48zCwpiXmFKfyQmluBgU31xBnD93Ugvz41OKCxOTUvNSSeNcAY0tjI1MLM0dDYyKUAAAkUCJ_</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>METHOD FOR CONTINUOUS STEEL CASTING</title><source>esp@cenet</source><creator>KOKUFU Sho ; SUGIHARA Hirokazu ; MATSUI Akitoshi ; OSUKA Kenichi ; FUKUDA Hiroyuki ; IRIE Shuhei ; UEOKA Satoshi ; ARAMAKI Norichika</creator><creatorcontrib>KOKUFU Sho ; SUGIHARA Hirokazu ; MATSUI Akitoshi ; OSUKA Kenichi ; FUKUDA Hiroyuki ; IRIE Shuhei ; UEOKA Satoshi ; ARAMAKI Norichika</creatorcontrib><description>Provided is a method for continuously casting steel capable of reducing center segregation that occurs in a slab.In the method for continuously casting steel according to the present invention, in a section in a continuous casting machine in a slab withdrawal direction, a section from a start point at which the average value of solid phase ratios along a thickness direction at a widthwise center of a slab 18 is within a range of 0.4 or more and 0.8 or less to an end point at which the average value of solid phase ratios along the thickness direction at the widthwise center of the slab is greater than the average value of solid phase ratios at the start point and is 1.0 or less is set as a first section, and the slab is cooled by water in the first section at a water flow rate per surface area of the slab within a range of 50 L/(m2×min) or more and 2,000 L/(m2×min) or less.</description><language>eng ; fre ; ger</language><subject>CASTING ; CASTING OF METALS ; CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES ; PERFORMING OPERATIONS ; POWDER METALLURGY ; TRANSPORTING</subject><creationdate>2022</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20220105&amp;DB=EPODOC&amp;CC=EP&amp;NR=3932586A1$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76419</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20220105&amp;DB=EPODOC&amp;CC=EP&amp;NR=3932586A1$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>KOKUFU Sho</creatorcontrib><creatorcontrib>SUGIHARA Hirokazu</creatorcontrib><creatorcontrib>MATSUI Akitoshi</creatorcontrib><creatorcontrib>OSUKA Kenichi</creatorcontrib><creatorcontrib>FUKUDA Hiroyuki</creatorcontrib><creatorcontrib>IRIE Shuhei</creatorcontrib><creatorcontrib>UEOKA Satoshi</creatorcontrib><creatorcontrib>ARAMAKI Norichika</creatorcontrib><title>METHOD FOR CONTINUOUS STEEL CASTING</title><description>Provided is a method for continuously casting steel capable of reducing center segregation that occurs in a slab.In the method for continuously casting steel according to the present invention, in a section in a continuous casting machine in a slab withdrawal direction, a section from a start point at which the average value of solid phase ratios along a thickness direction at a widthwise center of a slab 18 is within a range of 0.4 or more and 0.8 or less to an end point at which the average value of solid phase ratios along the thickness direction at the widthwise center of the slab is greater than the average value of solid phase ratios at the start point and is 1.0 or less is set as a first section, and the slab is cooled by water in the first section at a water flow rate per surface area of the slab within a range of 50 L/(m2×min) or more and 2,000 L/(m2×min) or less.</description><subject>CASTING</subject><subject>CASTING OF METALS</subject><subject>CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES</subject><subject>PERFORMING OPERATIONS</subject><subject>POWDER METALLURGY</subject><subject>TRANSPORTING</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2022</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZFD2dQ3x8HdRcPMPUnD29wvx9Av1Dw1WCA5xdfVRcHYMBgq48zCwpiXmFKfyQmluBgU31xBnD93Ugvz41OKCxOTUvNSSeNcAY0tjI1MLM0dDYyKUAAAkUCJ_</recordid><startdate>20220105</startdate><enddate>20220105</enddate><creator>KOKUFU Sho</creator><creator>SUGIHARA Hirokazu</creator><creator>MATSUI Akitoshi</creator><creator>OSUKA Kenichi</creator><creator>FUKUDA Hiroyuki</creator><creator>IRIE Shuhei</creator><creator>UEOKA Satoshi</creator><creator>ARAMAKI Norichika</creator><scope>EVB</scope></search><sort><creationdate>20220105</creationdate><title>METHOD FOR CONTINUOUS STEEL CASTING</title><author>KOKUFU Sho ; SUGIHARA Hirokazu ; MATSUI Akitoshi ; OSUKA Kenichi ; FUKUDA Hiroyuki ; IRIE Shuhei ; UEOKA Satoshi ; ARAMAKI Norichika</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_EP3932586A13</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; fre ; ger</language><creationdate>2022</creationdate><topic>CASTING</topic><topic>CASTING OF METALS</topic><topic>CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES</topic><topic>PERFORMING OPERATIONS</topic><topic>POWDER METALLURGY</topic><topic>TRANSPORTING</topic><toplevel>online_resources</toplevel><creatorcontrib>KOKUFU Sho</creatorcontrib><creatorcontrib>SUGIHARA Hirokazu</creatorcontrib><creatorcontrib>MATSUI Akitoshi</creatorcontrib><creatorcontrib>OSUKA Kenichi</creatorcontrib><creatorcontrib>FUKUDA Hiroyuki</creatorcontrib><creatorcontrib>IRIE Shuhei</creatorcontrib><creatorcontrib>UEOKA Satoshi</creatorcontrib><creatorcontrib>ARAMAKI Norichika</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>KOKUFU Sho</au><au>SUGIHARA Hirokazu</au><au>MATSUI Akitoshi</au><au>OSUKA Kenichi</au><au>FUKUDA Hiroyuki</au><au>IRIE Shuhei</au><au>UEOKA Satoshi</au><au>ARAMAKI Norichika</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>METHOD FOR CONTINUOUS STEEL CASTING</title><date>2022-01-05</date><risdate>2022</risdate><abstract>Provided is a method for continuously casting steel capable of reducing center segregation that occurs in a slab.In the method for continuously casting steel according to the present invention, in a section in a continuous casting machine in a slab withdrawal direction, a section from a start point at which the average value of solid phase ratios along a thickness direction at a widthwise center of a slab 18 is within a range of 0.4 or more and 0.8 or less to an end point at which the average value of solid phase ratios along the thickness direction at the widthwise center of the slab is greater than the average value of solid phase ratios at the start point and is 1.0 or less is set as a first section, and the slab is cooled by water in the first section at a water flow rate per surface area of the slab within a range of 50 L/(m2×min) or more and 2,000 L/(m2×min) or less.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng ; fre ; ger
recordid cdi_epo_espacenet_EP3932586A1
source esp@cenet
subjects CASTING
CASTING OF METALS
CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES
PERFORMING OPERATIONS
POWDER METALLURGY
TRANSPORTING
title METHOD FOR CONTINUOUS STEEL CASTING
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-07T20%3A02%3A05IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=KOKUFU%20Sho&rft.date=2022-01-05&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EEP3932586A1%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true