MOLDED ARTICLE AND METHOD FOR PRODUCING SAME

There is provided a molded article containing an amorphous resin, wherein a peak position change rate r (%) of the molded article defined by Equation: Peak position change rate r (%) = 100 × (Q1-Q2)/Q2 is 1 or more. In the equation, Q1 and Q2 are peak positions (nm-1) of the molded article and a pre...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: BANDO, Akinori, KADOYA, Hidenori, TAKAGI, Yasuyuki, YASUTOMI, Yoichi
Format: Patent
Sprache:eng ; fre ; ger
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:There is provided a molded article containing an amorphous resin, wherein a peak position change rate r (%) of the molded article defined by Equation: Peak position change rate r (%) = 100 × (Q1-Q2)/Q2 is 1 or more. In the equation, Q1 and Q2 are peak positions (nm-1) of the molded article and a predetermined reference molded article, respectively, the peak position being determined by a wide angle X-ray diffraction method. The peak position is a peak derived from the amorphous resin in a scattering vector magnitude Q-intensity profile calculated from a diffraction image obtained by a transmission method and measured by the wide angle X-ray diffraction method and obtained after background correction and transmittance correction, and the peak position is a value of Q at a peak at which Q is the smallest among peaks at which Q is in a range of 5 nm-1 to 25 nm-1.