CONTINUOUS CASTING METHOD OF STEEL

To reduce an overall segregation level of center segregation of a continuously cast slab in a slab width direction and also reduce variation in a segregation degree in the slab width direction.A continuous casting method of steel according to the present invention includes the step of bulging wide s...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: ODAGAKI Tomoya, IKENO Shizuhiko, SANO Keisuke, ARAMAKI Norichika, TOISHI Keigo
Format: Patent
Sprache:eng ; fre ; ger
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator ODAGAKI Tomoya
IKENO Shizuhiko
SANO Keisuke
ARAMAKI Norichika
TOISHI Keigo
description To reduce an overall segregation level of center segregation of a continuously cast slab in a slab width direction and also reduce variation in a segregation degree in the slab width direction.A continuous casting method of steel according to the present invention includes the step of bulging wide side surfaces of a slab having thereinside an unsolidified layer with a total intentional bulging amount of 3 to 10 mm by increasing stepwise toward a downstream side in a casting direction a roller gap of a plurality of pairs of slab support rollers disposed in a continuous casting machine. The method also includes the step of performing rolling reduction on the wide side surfaces of the slab, performed after the bulging of the wide side surfaces of the slab, in a soft reduction zone in which the roller gap of a plurality of pairs of slab support rollers is reduced stepwise toward the downstream side in the casting direction. The wide side surfaces of the slab undergo rolling reduction at a rolling reduction speed of 0.3 to 2.0 mm/min with a total rolling reduction amount smaller than or equal to the total intentional bulging amount in the soft reduction zone. A solid phase fraction at a center of a thickness of the slab is smaller than 0.2, or is greater than or equal to a flow limit solid phase fraction and not greater than 1.0 in a reformation zone in which a shape of the slab in the casting direction is reformed from a circular arc shape into a linear shape.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_EP3782747A1</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>EP3782747A1</sourcerecordid><originalsourceid>FETCH-epo_espacenet_EP3782747A13</originalsourceid><addsrcrecordid>eNrjZFBy9vcL8fQL9Q8NVnB2DAYy3RV8XUM8_F0U_N0UgkNcXX14GFjTEnOKU3mhNDeDgptriLOHbmpBfnxqcUFicmpeakm8a4CxuYWRuYm5o6ExEUoAAnMiMA</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>CONTINUOUS CASTING METHOD OF STEEL</title><source>esp@cenet</source><creator>ODAGAKI Tomoya ; IKENO Shizuhiko ; SANO Keisuke ; ARAMAKI Norichika ; TOISHI Keigo</creator><creatorcontrib>ODAGAKI Tomoya ; IKENO Shizuhiko ; SANO Keisuke ; ARAMAKI Norichika ; TOISHI Keigo</creatorcontrib><description>To reduce an overall segregation level of center segregation of a continuously cast slab in a slab width direction and also reduce variation in a segregation degree in the slab width direction.A continuous casting method of steel according to the present invention includes the step of bulging wide side surfaces of a slab having thereinside an unsolidified layer with a total intentional bulging amount of 3 to 10 mm by increasing stepwise toward a downstream side in a casting direction a roller gap of a plurality of pairs of slab support rollers disposed in a continuous casting machine. The method also includes the step of performing rolling reduction on the wide side surfaces of the slab, performed after the bulging of the wide side surfaces of the slab, in a soft reduction zone in which the roller gap of a plurality of pairs of slab support rollers is reduced stepwise toward the downstream side in the casting direction. The wide side surfaces of the slab undergo rolling reduction at a rolling reduction speed of 0.3 to 2.0 mm/min with a total rolling reduction amount smaller than or equal to the total intentional bulging amount in the soft reduction zone. A solid phase fraction at a center of a thickness of the slab is smaller than 0.2, or is greater than or equal to a flow limit solid phase fraction and not greater than 1.0 in a reformation zone in which a shape of the slab in the casting direction is reformed from a circular arc shape into a linear shape.</description><language>eng ; fre ; ger</language><subject>CASTING ; CASTING OF METALS ; CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES ; MECHANICAL METAL-WORKING WITHOUT ESSENTIALLY REMOVINGMATERIAL ; PERFORMING OPERATIONS ; POWDER METALLURGY ; PUNCHING METAL ; ROLLING OF METAL ; TRANSPORTING</subject><creationdate>2021</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20210224&amp;DB=EPODOC&amp;CC=EP&amp;NR=3782747A1$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,777,882,25545,76296</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20210224&amp;DB=EPODOC&amp;CC=EP&amp;NR=3782747A1$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>ODAGAKI Tomoya</creatorcontrib><creatorcontrib>IKENO Shizuhiko</creatorcontrib><creatorcontrib>SANO Keisuke</creatorcontrib><creatorcontrib>ARAMAKI Norichika</creatorcontrib><creatorcontrib>TOISHI Keigo</creatorcontrib><title>CONTINUOUS CASTING METHOD OF STEEL</title><description>To reduce an overall segregation level of center segregation of a continuously cast slab in a slab width direction and also reduce variation in a segregation degree in the slab width direction.A continuous casting method of steel according to the present invention includes the step of bulging wide side surfaces of a slab having thereinside an unsolidified layer with a total intentional bulging amount of 3 to 10 mm by increasing stepwise toward a downstream side in a casting direction a roller gap of a plurality of pairs of slab support rollers disposed in a continuous casting machine. The method also includes the step of performing rolling reduction on the wide side surfaces of the slab, performed after the bulging of the wide side surfaces of the slab, in a soft reduction zone in which the roller gap of a plurality of pairs of slab support rollers is reduced stepwise toward the downstream side in the casting direction. The wide side surfaces of the slab undergo rolling reduction at a rolling reduction speed of 0.3 to 2.0 mm/min with a total rolling reduction amount smaller than or equal to the total intentional bulging amount in the soft reduction zone. A solid phase fraction at a center of a thickness of the slab is smaller than 0.2, or is greater than or equal to a flow limit solid phase fraction and not greater than 1.0 in a reformation zone in which a shape of the slab in the casting direction is reformed from a circular arc shape into a linear shape.</description><subject>CASTING</subject><subject>CASTING OF METALS</subject><subject>CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES</subject><subject>MECHANICAL METAL-WORKING WITHOUT ESSENTIALLY REMOVINGMATERIAL</subject><subject>PERFORMING OPERATIONS</subject><subject>POWDER METALLURGY</subject><subject>PUNCHING METAL</subject><subject>ROLLING OF METAL</subject><subject>TRANSPORTING</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2021</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZFBy9vcL8fQL9Q8NVnB2DAYy3RV8XUM8_F0U_N0UgkNcXX14GFjTEnOKU3mhNDeDgptriLOHbmpBfnxqcUFicmpeakm8a4CxuYWRuYm5o6ExEUoAAnMiMA</recordid><startdate>20210224</startdate><enddate>20210224</enddate><creator>ODAGAKI Tomoya</creator><creator>IKENO Shizuhiko</creator><creator>SANO Keisuke</creator><creator>ARAMAKI Norichika</creator><creator>TOISHI Keigo</creator><scope>EVB</scope></search><sort><creationdate>20210224</creationdate><title>CONTINUOUS CASTING METHOD OF STEEL</title><author>ODAGAKI Tomoya ; IKENO Shizuhiko ; SANO Keisuke ; ARAMAKI Norichika ; TOISHI Keigo</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_EP3782747A13</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; fre ; ger</language><creationdate>2021</creationdate><topic>CASTING</topic><topic>CASTING OF METALS</topic><topic>CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES</topic><topic>MECHANICAL METAL-WORKING WITHOUT ESSENTIALLY REMOVINGMATERIAL</topic><topic>PERFORMING OPERATIONS</topic><topic>POWDER METALLURGY</topic><topic>PUNCHING METAL</topic><topic>ROLLING OF METAL</topic><topic>TRANSPORTING</topic><toplevel>online_resources</toplevel><creatorcontrib>ODAGAKI Tomoya</creatorcontrib><creatorcontrib>IKENO Shizuhiko</creatorcontrib><creatorcontrib>SANO Keisuke</creatorcontrib><creatorcontrib>ARAMAKI Norichika</creatorcontrib><creatorcontrib>TOISHI Keigo</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>ODAGAKI Tomoya</au><au>IKENO Shizuhiko</au><au>SANO Keisuke</au><au>ARAMAKI Norichika</au><au>TOISHI Keigo</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>CONTINUOUS CASTING METHOD OF STEEL</title><date>2021-02-24</date><risdate>2021</risdate><abstract>To reduce an overall segregation level of center segregation of a continuously cast slab in a slab width direction and also reduce variation in a segregation degree in the slab width direction.A continuous casting method of steel according to the present invention includes the step of bulging wide side surfaces of a slab having thereinside an unsolidified layer with a total intentional bulging amount of 3 to 10 mm by increasing stepwise toward a downstream side in a casting direction a roller gap of a plurality of pairs of slab support rollers disposed in a continuous casting machine. The method also includes the step of performing rolling reduction on the wide side surfaces of the slab, performed after the bulging of the wide side surfaces of the slab, in a soft reduction zone in which the roller gap of a plurality of pairs of slab support rollers is reduced stepwise toward the downstream side in the casting direction. The wide side surfaces of the slab undergo rolling reduction at a rolling reduction speed of 0.3 to 2.0 mm/min with a total rolling reduction amount smaller than or equal to the total intentional bulging amount in the soft reduction zone. A solid phase fraction at a center of a thickness of the slab is smaller than 0.2, or is greater than or equal to a flow limit solid phase fraction and not greater than 1.0 in a reformation zone in which a shape of the slab in the casting direction is reformed from a circular arc shape into a linear shape.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng ; fre ; ger
recordid cdi_epo_espacenet_EP3782747A1
source esp@cenet
subjects CASTING
CASTING OF METALS
CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES
MECHANICAL METAL-WORKING WITHOUT ESSENTIALLY REMOVINGMATERIAL
PERFORMING OPERATIONS
POWDER METALLURGY
PUNCHING METAL
ROLLING OF METAL
TRANSPORTING
title CONTINUOUS CASTING METHOD OF STEEL
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-19T18%3A43%3A53IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=ODAGAKI%20Tomoya&rft.date=2021-02-24&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EEP3782747A1%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true