SEMI-AROMATIC POLYAMIDE FIBER

The present invention provides a semi-aromatic polyamide fiber having acid resistance and further having excellent long-term heat resistance and good spinning properties. The semi-aromatic polyamide fiber contains a semi-aromatic polyamide resin having a melting point of 280°C or less and satisfies...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: UEHATA, Akihiro, OKAMOTO, Tetsuya, TOMOSUGI, Tetsuya
Format: Patent
Sprache:eng ; fre ; ger
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator UEHATA, Akihiro
OKAMOTO, Tetsuya
TOMOSUGI, Tetsuya
description The present invention provides a semi-aromatic polyamide fiber having acid resistance and further having excellent long-term heat resistance and good spinning properties. The semi-aromatic polyamide fiber contains a semi-aromatic polyamide resin having a melting point of 280°C or less and satisfies all of the following conditions (1) to (3): (1) in the semi-aromatic polyamide, a dicarboxylic acid component is an aromatic dicarboxylic acid, and 40 mol% to 80 mol% of a diamine component is 2-methyl-1,8-octanediamine; (2) the semi-aromatic polyamide comprises 50 ppm to 500 ppm of a copper compound in terms of copper; and (3) the semi-aromatic polyamide fiber has a peak temperature of a glass transition point from 120°C to 140°C.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_EP3617352B1</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>EP3617352B1</sourcerecordid><originalsourceid>FETCH-epo_espacenet_EP3617352B13</originalsourceid><addsrcrecordid>eNrjZJANdvX11HUM8vd1DPF0Vgjw94l09PV0cVVw83RyDeJhYE1LzClO5YXS3AwKbq4hzh66qQX58anFBYnJqXmpJfGuAcZmhubGpkZOhsZEKAEATTUgmw</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>SEMI-AROMATIC POLYAMIDE FIBER</title><source>esp@cenet</source><creator>UEHATA, Akihiro ; OKAMOTO, Tetsuya ; TOMOSUGI, Tetsuya</creator><creatorcontrib>UEHATA, Akihiro ; OKAMOTO, Tetsuya ; TOMOSUGI, Tetsuya</creatorcontrib><description>The present invention provides a semi-aromatic polyamide fiber having acid resistance and further having excellent long-term heat resistance and good spinning properties. The semi-aromatic polyamide fiber contains a semi-aromatic polyamide resin having a melting point of 280°C or less and satisfies all of the following conditions (1) to (3): (1) in the semi-aromatic polyamide, a dicarboxylic acid component is an aromatic dicarboxylic acid, and 40 mol% to 80 mol% of a diamine component is 2-methyl-1,8-octanediamine; (2) the semi-aromatic polyamide comprises 50 ppm to 500 ppm of a copper compound in terms of copper; and (3) the semi-aromatic polyamide fiber has a peak temperature of a glass transition point from 120°C to 140°C.</description><language>eng ; fre ; ger</language><subject>APPARATUS SPECIALLY ADAPTED FOR THE MANUFACTURE OF CARBONFILAMENTS ; CHEMICAL FEATURES IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS,THREADS, FIBRES, BRISTLES OR RIBBONS ; CHEMISTRY ; COMPOSITIONS BASED THEREON ; MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONSONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS ; METALLURGY ; NATURAL OR ARTIFICIAL THREADS OR FIBRES ; ORGANIC MACROMOLECULAR COMPOUNDS ; SPINNING ; TEXTILES ; THEIR PREPARATION OR CHEMICAL WORKING-UP</subject><creationdate>2020</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20201125&amp;DB=EPODOC&amp;CC=EP&amp;NR=3617352B1$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76516</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20201125&amp;DB=EPODOC&amp;CC=EP&amp;NR=3617352B1$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>UEHATA, Akihiro</creatorcontrib><creatorcontrib>OKAMOTO, Tetsuya</creatorcontrib><creatorcontrib>TOMOSUGI, Tetsuya</creatorcontrib><title>SEMI-AROMATIC POLYAMIDE FIBER</title><description>The present invention provides a semi-aromatic polyamide fiber having acid resistance and further having excellent long-term heat resistance and good spinning properties. The semi-aromatic polyamide fiber contains a semi-aromatic polyamide resin having a melting point of 280°C or less and satisfies all of the following conditions (1) to (3): (1) in the semi-aromatic polyamide, a dicarboxylic acid component is an aromatic dicarboxylic acid, and 40 mol% to 80 mol% of a diamine component is 2-methyl-1,8-octanediamine; (2) the semi-aromatic polyamide comprises 50 ppm to 500 ppm of a copper compound in terms of copper; and (3) the semi-aromatic polyamide fiber has a peak temperature of a glass transition point from 120°C to 140°C.</description><subject>APPARATUS SPECIALLY ADAPTED FOR THE MANUFACTURE OF CARBONFILAMENTS</subject><subject>CHEMICAL FEATURES IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS,THREADS, FIBRES, BRISTLES OR RIBBONS</subject><subject>CHEMISTRY</subject><subject>COMPOSITIONS BASED THEREON</subject><subject>MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONSONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS</subject><subject>METALLURGY</subject><subject>NATURAL OR ARTIFICIAL THREADS OR FIBRES</subject><subject>ORGANIC MACROMOLECULAR COMPOUNDS</subject><subject>SPINNING</subject><subject>TEXTILES</subject><subject>THEIR PREPARATION OR CHEMICAL WORKING-UP</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2020</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZJANdvX11HUM8vd1DPF0Vgjw94l09PV0cVVw83RyDeJhYE1LzClO5YXS3AwKbq4hzh66qQX58anFBYnJqXmpJfGuAcZmhubGpkZOhsZEKAEATTUgmw</recordid><startdate>20201125</startdate><enddate>20201125</enddate><creator>UEHATA, Akihiro</creator><creator>OKAMOTO, Tetsuya</creator><creator>TOMOSUGI, Tetsuya</creator><scope>EVB</scope></search><sort><creationdate>20201125</creationdate><title>SEMI-AROMATIC POLYAMIDE FIBER</title><author>UEHATA, Akihiro ; OKAMOTO, Tetsuya ; TOMOSUGI, Tetsuya</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_EP3617352B13</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; fre ; ger</language><creationdate>2020</creationdate><topic>APPARATUS SPECIALLY ADAPTED FOR THE MANUFACTURE OF CARBONFILAMENTS</topic><topic>CHEMICAL FEATURES IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS,THREADS, FIBRES, BRISTLES OR RIBBONS</topic><topic>CHEMISTRY</topic><topic>COMPOSITIONS BASED THEREON</topic><topic>MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONSONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS</topic><topic>METALLURGY</topic><topic>NATURAL OR ARTIFICIAL THREADS OR FIBRES</topic><topic>ORGANIC MACROMOLECULAR COMPOUNDS</topic><topic>SPINNING</topic><topic>TEXTILES</topic><topic>THEIR PREPARATION OR CHEMICAL WORKING-UP</topic><toplevel>online_resources</toplevel><creatorcontrib>UEHATA, Akihiro</creatorcontrib><creatorcontrib>OKAMOTO, Tetsuya</creatorcontrib><creatorcontrib>TOMOSUGI, Tetsuya</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>UEHATA, Akihiro</au><au>OKAMOTO, Tetsuya</au><au>TOMOSUGI, Tetsuya</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>SEMI-AROMATIC POLYAMIDE FIBER</title><date>2020-11-25</date><risdate>2020</risdate><abstract>The present invention provides a semi-aromatic polyamide fiber having acid resistance and further having excellent long-term heat resistance and good spinning properties. The semi-aromatic polyamide fiber contains a semi-aromatic polyamide resin having a melting point of 280°C or less and satisfies all of the following conditions (1) to (3): (1) in the semi-aromatic polyamide, a dicarboxylic acid component is an aromatic dicarboxylic acid, and 40 mol% to 80 mol% of a diamine component is 2-methyl-1,8-octanediamine; (2) the semi-aromatic polyamide comprises 50 ppm to 500 ppm of a copper compound in terms of copper; and (3) the semi-aromatic polyamide fiber has a peak temperature of a glass transition point from 120°C to 140°C.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng ; fre ; ger
recordid cdi_epo_espacenet_EP3617352B1
source esp@cenet
subjects APPARATUS SPECIALLY ADAPTED FOR THE MANUFACTURE OF CARBONFILAMENTS
CHEMICAL FEATURES IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS,THREADS, FIBRES, BRISTLES OR RIBBONS
CHEMISTRY
COMPOSITIONS BASED THEREON
MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONSONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
METALLURGY
NATURAL OR ARTIFICIAL THREADS OR FIBRES
ORGANIC MACROMOLECULAR COMPOUNDS
SPINNING
TEXTILES
THEIR PREPARATION OR CHEMICAL WORKING-UP
title SEMI-AROMATIC POLYAMIDE FIBER
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-19T02%3A51%3A42IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=UEHATA,%20Akihiro&rft.date=2020-11-25&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EEP3617352B1%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true