METHOD OF MANUFACTURING AN AL-MG-MN ALLOY PLATE PRODUCT

The invention relates to a method of manufacturing a rolled Al-Mg-Mn alloy plate product comprising the steps of: (a) providing a rolling feedstock material of an Al-Mg-Mn alloy having a composition comprising of, in wt.%, Mg 4.8-6.0%, Mn 0.3-1.25%, Zn up to 0.9%, Fe up to 0.4%, Si up to 0.3%, Cu up...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: Jacoby, Bernd, Knaack, Nele Mareike, Bach, Andreas Harald
Format: Patent
Sprache:eng ; fre ; ger
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator Jacoby, Bernd
Knaack, Nele Mareike
Bach, Andreas Harald
description The invention relates to a method of manufacturing a rolled Al-Mg-Mn alloy plate product comprising the steps of: (a) providing a rolling feedstock material of an Al-Mg-Mn alloy having a composition comprising of, in wt.%, Mg 4.8-6.0%, Mn 0.3-1.25%, Zn up to 0.9%, Fe up to 0.4%, Si up to 0.3%, Cu up to 0.2%, Cr up to 0.25%, Zr up to 0.25%, Ti up to 0.25%, unavoidable impurities and balance aluminium; (b) heating the rolling feedstock to a temperature in a range of 480-550°C; (c) hot-rolling of the heated rolling feedstock to a hot-rolled plate having a final gauge in a range of 3-15 mm, and wherein the hot-mill entry temperature is in a range of 400-550°C, and the hot-mill exit temperature is in a range of 130-285°C; and wherein the hot rolling of the rolling feedstock to final gauge is without cold rolling the rolling feedstock prior to the final gauge; (d) annealing of the hot-rolled plate at final gauge at an annealing temperature in a range of 300-550°C; and (e) cooling to ambient temperature.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_EP3569721A1</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>EP3569721A1</sourcerecordid><originalsourceid>FETCH-epo_espacenet_EP3569721A13</originalsourceid><addsrcrecordid>eNrjZDD3dQ3x8HdR8HdT8HX0C3VzdA4JDfL0c1dw9FNw9NH1ddf1BTF8_CMVAnwcQ1wVAoL8XUKdQ3gYWNMSc4pTeaE0N4OCm2uIs4duakF-fGpxQWJyal5qSbxrgLGpmaW5kaGjoTERSgDNsSeP</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>METHOD OF MANUFACTURING AN AL-MG-MN ALLOY PLATE PRODUCT</title><source>esp@cenet</source><creator>Jacoby, Bernd ; Knaack, Nele Mareike ; Bach, Andreas Harald</creator><creatorcontrib>Jacoby, Bernd ; Knaack, Nele Mareike ; Bach, Andreas Harald</creatorcontrib><description>The invention relates to a method of manufacturing a rolled Al-Mg-Mn alloy plate product comprising the steps of: (a) providing a rolling feedstock material of an Al-Mg-Mn alloy having a composition comprising of, in wt.%, Mg 4.8-6.0%, Mn 0.3-1.25%, Zn up to 0.9%, Fe up to 0.4%, Si up to 0.3%, Cu up to 0.2%, Cr up to 0.25%, Zr up to 0.25%, Ti up to 0.25%, unavoidable impurities and balance aluminium; (b) heating the rolling feedstock to a temperature in a range of 480-550°C; (c) hot-rolling of the heated rolling feedstock to a hot-rolled plate having a final gauge in a range of 3-15 mm, and wherein the hot-mill entry temperature is in a range of 400-550°C, and the hot-mill exit temperature is in a range of 130-285°C; and wherein the hot rolling of the rolling feedstock to final gauge is without cold rolling the rolling feedstock prior to the final gauge; (d) annealing of the hot-rolled plate at final gauge at an annealing temperature in a range of 300-550°C; and (e) cooling to ambient temperature.</description><language>eng ; fre ; ger</language><subject>ALLOYS ; CHEMISTRY ; FERROUS OR NON-FERROUS ALLOYS ; METALLURGY ; TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><creationdate>2019</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20191120&amp;DB=EPODOC&amp;CC=EP&amp;NR=3569721A1$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25563,76418</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20191120&amp;DB=EPODOC&amp;CC=EP&amp;NR=3569721A1$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>Jacoby, Bernd</creatorcontrib><creatorcontrib>Knaack, Nele Mareike</creatorcontrib><creatorcontrib>Bach, Andreas Harald</creatorcontrib><title>METHOD OF MANUFACTURING AN AL-MG-MN ALLOY PLATE PRODUCT</title><description>The invention relates to a method of manufacturing a rolled Al-Mg-Mn alloy plate product comprising the steps of: (a) providing a rolling feedstock material of an Al-Mg-Mn alloy having a composition comprising of, in wt.%, Mg 4.8-6.0%, Mn 0.3-1.25%, Zn up to 0.9%, Fe up to 0.4%, Si up to 0.3%, Cu up to 0.2%, Cr up to 0.25%, Zr up to 0.25%, Ti up to 0.25%, unavoidable impurities and balance aluminium; (b) heating the rolling feedstock to a temperature in a range of 480-550°C; (c) hot-rolling of the heated rolling feedstock to a hot-rolled plate having a final gauge in a range of 3-15 mm, and wherein the hot-mill entry temperature is in a range of 400-550°C, and the hot-mill exit temperature is in a range of 130-285°C; and wherein the hot rolling of the rolling feedstock to final gauge is without cold rolling the rolling feedstock prior to the final gauge; (d) annealing of the hot-rolled plate at final gauge at an annealing temperature in a range of 300-550°C; and (e) cooling to ambient temperature.</description><subject>ALLOYS</subject><subject>CHEMISTRY</subject><subject>FERROUS OR NON-FERROUS ALLOYS</subject><subject>METALLURGY</subject><subject>TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2019</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZDD3dQ3x8HdR8HdT8HX0C3VzdA4JDfL0c1dw9FNw9NH1ddf1BTF8_CMVAnwcQ1wVAoL8XUKdQ3gYWNMSc4pTeaE0N4OCm2uIs4duakF-fGpxQWJyal5qSbxrgLGpmaW5kaGjoTERSgDNsSeP</recordid><startdate>20191120</startdate><enddate>20191120</enddate><creator>Jacoby, Bernd</creator><creator>Knaack, Nele Mareike</creator><creator>Bach, Andreas Harald</creator><scope>EVB</scope></search><sort><creationdate>20191120</creationdate><title>METHOD OF MANUFACTURING AN AL-MG-MN ALLOY PLATE PRODUCT</title><author>Jacoby, Bernd ; Knaack, Nele Mareike ; Bach, Andreas Harald</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_EP3569721A13</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; fre ; ger</language><creationdate>2019</creationdate><topic>ALLOYS</topic><topic>CHEMISTRY</topic><topic>FERROUS OR NON-FERROUS ALLOYS</topic><topic>METALLURGY</topic><topic>TREATMENT OF ALLOYS OR NON-FERROUS METALS</topic><toplevel>online_resources</toplevel><creatorcontrib>Jacoby, Bernd</creatorcontrib><creatorcontrib>Knaack, Nele Mareike</creatorcontrib><creatorcontrib>Bach, Andreas Harald</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>Jacoby, Bernd</au><au>Knaack, Nele Mareike</au><au>Bach, Andreas Harald</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>METHOD OF MANUFACTURING AN AL-MG-MN ALLOY PLATE PRODUCT</title><date>2019-11-20</date><risdate>2019</risdate><abstract>The invention relates to a method of manufacturing a rolled Al-Mg-Mn alloy plate product comprising the steps of: (a) providing a rolling feedstock material of an Al-Mg-Mn alloy having a composition comprising of, in wt.%, Mg 4.8-6.0%, Mn 0.3-1.25%, Zn up to 0.9%, Fe up to 0.4%, Si up to 0.3%, Cu up to 0.2%, Cr up to 0.25%, Zr up to 0.25%, Ti up to 0.25%, unavoidable impurities and balance aluminium; (b) heating the rolling feedstock to a temperature in a range of 480-550°C; (c) hot-rolling of the heated rolling feedstock to a hot-rolled plate having a final gauge in a range of 3-15 mm, and wherein the hot-mill entry temperature is in a range of 400-550°C, and the hot-mill exit temperature is in a range of 130-285°C; and wherein the hot rolling of the rolling feedstock to final gauge is without cold rolling the rolling feedstock prior to the final gauge; (d) annealing of the hot-rolled plate at final gauge at an annealing temperature in a range of 300-550°C; and (e) cooling to ambient temperature.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng ; fre ; ger
recordid cdi_epo_espacenet_EP3569721A1
source esp@cenet
subjects ALLOYS
CHEMISTRY
FERROUS OR NON-FERROUS ALLOYS
METALLURGY
TREATMENT OF ALLOYS OR NON-FERROUS METALS
title METHOD OF MANUFACTURING AN AL-MG-MN ALLOY PLATE PRODUCT
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-08T13%3A50%3A58IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=Jacoby,%20Bernd&rft.date=2019-11-20&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EEP3569721A1%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true