METHOD FOR MANUFACTURING LITHIUM-TITANIUM COMPOSITE OXIDE BY CONTROLLING PARTICLE SIZE OF SLURRY THROUGH WET MILLING

The present invention relates to a lithium-titanium complex oxide used in an electrode active material. A preparation method of a lithium-titanium complex oxide according to the present invention comprises the steps of: preparing a slurry mixture in which a titanium oxide, lithium and zirconium are...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: JEONG, Seung Chang, LEE, Jae An, KIM, Jeong Han, KANG, Chun Gu, CHOI, Su Bong, CHOI, Jeong Eun
Format: Patent
Sprache:eng ; fre ; ger
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator JEONG, Seung Chang
LEE, Jae An
KIM, Jeong Han
KANG, Chun Gu
CHOI, Su Bong
CHOI, Jeong Eun
description The present invention relates to a lithium-titanium complex oxide used in an electrode active material. A preparation method of a lithium-titanium complex oxide according to the present invention comprises the steps of: preparing a slurry mixture in which a titanium oxide, lithium and zirconium are mixed; wet-milling the mixture using beads having a size of 0.30 mm or less to obtain a wet-milled mixture; spray drying the wet-milled mixture to obtain a spray dried mixture; and calcining the spray dried mixture.The preparation method according to the present invention has an effect that the particle sizes can be adjusted through the milling process by controlling particle sizes of the precursor slurry through wet-milling.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_EP3543215A4</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>EP3543215A4</sourcerecordid><originalsourceid>FETCH-epo_espacenet_EP3543215A43</originalsourceid><addsrcrecordid>eNqNyk0KwjAQhuFuXIh6h7lAF9p6gJgmzUB-ynSC1k0pEleihfb-WMUDuPpePp51NjvFJlSgA4ETPmohORL6GiyywehyRhZ-CZDBNaFFVhAuWCk4dcvlmYK1H98IYpRWQYvXhWhobSTqgA2FWBs4KwaHX7vNVvfhMaXdbzcZaMXS5Gl89Wkah1t6prlXTXEsi8P-KMriD_IGqe05Kw</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>METHOD FOR MANUFACTURING LITHIUM-TITANIUM COMPOSITE OXIDE BY CONTROLLING PARTICLE SIZE OF SLURRY THROUGH WET MILLING</title><source>esp@cenet</source><creator>JEONG, Seung Chang ; LEE, Jae An ; KIM, Jeong Han ; KANG, Chun Gu ; CHOI, Su Bong ; CHOI, Jeong Eun</creator><creatorcontrib>JEONG, Seung Chang ; LEE, Jae An ; KIM, Jeong Han ; KANG, Chun Gu ; CHOI, Su Bong ; CHOI, Jeong Eun</creatorcontrib><description>The present invention relates to a lithium-titanium complex oxide used in an electrode active material. A preparation method of a lithium-titanium complex oxide according to the present invention comprises the steps of: preparing a slurry mixture in which a titanium oxide, lithium and zirconium are mixed; wet-milling the mixture using beads having a size of 0.30 mm or less to obtain a wet-milled mixture; spray drying the wet-milled mixture to obtain a spray dried mixture; and calcining the spray dried mixture.The preparation method according to the present invention has an effect that the particle sizes can be adjusted through the milling process by controlling particle sizes of the precursor slurry through wet-milling.</description><language>eng ; fre ; ger</language><subject>ARTIFICIAL STONE ; BASIC ELECTRIC ELEMENTS ; CEMENTS ; CERAMICS ; CHEMISTRY ; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS ; COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSESC01D OR C01F ; CONCRETE ; ELECTRICITY ; INORGANIC CHEMISTRY ; LIME, MAGNESIA ; METALLURGY ; PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY ; REFRACTORIES ; SLAG ; TREATMENT OF NATURAL STONE</subject><creationdate>2020</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20200729&amp;DB=EPODOC&amp;CC=EP&amp;NR=3543215A4$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76289</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20200729&amp;DB=EPODOC&amp;CC=EP&amp;NR=3543215A4$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>JEONG, Seung Chang</creatorcontrib><creatorcontrib>LEE, Jae An</creatorcontrib><creatorcontrib>KIM, Jeong Han</creatorcontrib><creatorcontrib>KANG, Chun Gu</creatorcontrib><creatorcontrib>CHOI, Su Bong</creatorcontrib><creatorcontrib>CHOI, Jeong Eun</creatorcontrib><title>METHOD FOR MANUFACTURING LITHIUM-TITANIUM COMPOSITE OXIDE BY CONTROLLING PARTICLE SIZE OF SLURRY THROUGH WET MILLING</title><description>The present invention relates to a lithium-titanium complex oxide used in an electrode active material. A preparation method of a lithium-titanium complex oxide according to the present invention comprises the steps of: preparing a slurry mixture in which a titanium oxide, lithium and zirconium are mixed; wet-milling the mixture using beads having a size of 0.30 mm or less to obtain a wet-milled mixture; spray drying the wet-milled mixture to obtain a spray dried mixture; and calcining the spray dried mixture.The preparation method according to the present invention has an effect that the particle sizes can be adjusted through the milling process by controlling particle sizes of the precursor slurry through wet-milling.</description><subject>ARTIFICIAL STONE</subject><subject>BASIC ELECTRIC ELEMENTS</subject><subject>CEMENTS</subject><subject>CERAMICS</subject><subject>CHEMISTRY</subject><subject>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</subject><subject>COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSESC01D OR C01F</subject><subject>CONCRETE</subject><subject>ELECTRICITY</subject><subject>INORGANIC CHEMISTRY</subject><subject>LIME, MAGNESIA</subject><subject>METALLURGY</subject><subject>PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY</subject><subject>REFRACTORIES</subject><subject>SLAG</subject><subject>TREATMENT OF NATURAL STONE</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2020</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNyk0KwjAQhuFuXIh6h7lAF9p6gJgmzUB-ynSC1k0pEleihfb-WMUDuPpePp51NjvFJlSgA4ETPmohORL6GiyywehyRhZ-CZDBNaFFVhAuWCk4dcvlmYK1H98IYpRWQYvXhWhobSTqgA2FWBs4KwaHX7vNVvfhMaXdbzcZaMXS5Gl89Wkah1t6prlXTXEsi8P-KMriD_IGqe05Kw</recordid><startdate>20200729</startdate><enddate>20200729</enddate><creator>JEONG, Seung Chang</creator><creator>LEE, Jae An</creator><creator>KIM, Jeong Han</creator><creator>KANG, Chun Gu</creator><creator>CHOI, Su Bong</creator><creator>CHOI, Jeong Eun</creator><scope>EVB</scope></search><sort><creationdate>20200729</creationdate><title>METHOD FOR MANUFACTURING LITHIUM-TITANIUM COMPOSITE OXIDE BY CONTROLLING PARTICLE SIZE OF SLURRY THROUGH WET MILLING</title><author>JEONG, Seung Chang ; LEE, Jae An ; KIM, Jeong Han ; KANG, Chun Gu ; CHOI, Su Bong ; CHOI, Jeong Eun</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_EP3543215A43</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; fre ; ger</language><creationdate>2020</creationdate><topic>ARTIFICIAL STONE</topic><topic>BASIC ELECTRIC ELEMENTS</topic><topic>CEMENTS</topic><topic>CERAMICS</topic><topic>CHEMISTRY</topic><topic>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</topic><topic>COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSESC01D OR C01F</topic><topic>CONCRETE</topic><topic>ELECTRICITY</topic><topic>INORGANIC CHEMISTRY</topic><topic>LIME, MAGNESIA</topic><topic>METALLURGY</topic><topic>PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY</topic><topic>REFRACTORIES</topic><topic>SLAG</topic><topic>TREATMENT OF NATURAL STONE</topic><toplevel>online_resources</toplevel><creatorcontrib>JEONG, Seung Chang</creatorcontrib><creatorcontrib>LEE, Jae An</creatorcontrib><creatorcontrib>KIM, Jeong Han</creatorcontrib><creatorcontrib>KANG, Chun Gu</creatorcontrib><creatorcontrib>CHOI, Su Bong</creatorcontrib><creatorcontrib>CHOI, Jeong Eun</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>JEONG, Seung Chang</au><au>LEE, Jae An</au><au>KIM, Jeong Han</au><au>KANG, Chun Gu</au><au>CHOI, Su Bong</au><au>CHOI, Jeong Eun</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>METHOD FOR MANUFACTURING LITHIUM-TITANIUM COMPOSITE OXIDE BY CONTROLLING PARTICLE SIZE OF SLURRY THROUGH WET MILLING</title><date>2020-07-29</date><risdate>2020</risdate><abstract>The present invention relates to a lithium-titanium complex oxide used in an electrode active material. A preparation method of a lithium-titanium complex oxide according to the present invention comprises the steps of: preparing a slurry mixture in which a titanium oxide, lithium and zirconium are mixed; wet-milling the mixture using beads having a size of 0.30 mm or less to obtain a wet-milled mixture; spray drying the wet-milled mixture to obtain a spray dried mixture; and calcining the spray dried mixture.The preparation method according to the present invention has an effect that the particle sizes can be adjusted through the milling process by controlling particle sizes of the precursor slurry through wet-milling.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng ; fre ; ger
recordid cdi_epo_espacenet_EP3543215A4
source esp@cenet
subjects ARTIFICIAL STONE
BASIC ELECTRIC ELEMENTS
CEMENTS
CERAMICS
CHEMISTRY
COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS
COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSESC01D OR C01F
CONCRETE
ELECTRICITY
INORGANIC CHEMISTRY
LIME, MAGNESIA
METALLURGY
PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY
REFRACTORIES
SLAG
TREATMENT OF NATURAL STONE
title METHOD FOR MANUFACTURING LITHIUM-TITANIUM COMPOSITE OXIDE BY CONTROLLING PARTICLE SIZE OF SLURRY THROUGH WET MILLING
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-12T11%3A56%3A41IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=JEONG,%20Seung%20Chang&rft.date=2020-07-29&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EEP3543215A4%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true