TRANSPARENT HYDROPHOBIC MIXED OXIDE COATINGS AND METHODS
A hydrophobic coating and a method for applying such a coating to a surface of a substrate. The method includes applying a coating composition to the surface and heating the coated surface at a cure temperature from about 450° C. to about 600° C. for a time from about 8 hours to about 48 hours. The...