METHOD OF MAKING AN EXTRUDED THIN FILM, AND THIN FILM SO PRODUCED

Method of making an extruded thin film comprising: melt filtering an amorphous thermoplastic composition comprising an amorphous thermoplastic polymer with a glass transition temperature Tg of 130° C. to 280° C. to form a melt filtered amorphous thermoplastic composition; extruding the melt filtered...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: GALLUCCI, Robert Russell, SANNER, Mark A, JOHNSON, Peter, EHRENSBECK, Franklin
Format: Patent
Sprache:eng ; fre ; ger
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator GALLUCCI, Robert Russell
SANNER, Mark A
JOHNSON, Peter
EHRENSBECK, Franklin
description Method of making an extruded thin film comprising: melt filtering an amorphous thermoplastic composition comprising an amorphous thermoplastic polymer with a glass transition temperature Tg of 130° C. to 280° C. to form a melt filtered amorphous thermoplastic composition; extruding the melt filtered amorphous thermoplastic composition into strands at a temperature TE; cooling the strands to a temperature Tc to form cooled strands; cutting the cooled strands into pellets having a length of 2.0 to 6.0 millimeters; treating the pellets at a temperature Ts to remove particulates having at least one of length, width, and height of less than 0.5 millimeters to form treated pellets; melting the treated pellets in an extruder at a temperature Tp to form a molten composition; and extruding the molten composition through a flat die to form a film having an average thickness less than or equal to 50 micrometers.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_EP3484682B1</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>EP3484682B1</sourcerecordid><originalsourceid>FETCH-epo_espacenet_EP3484682B13</originalsourceid><addsrcrecordid>eNrjZHD0dQ3x8HdR8HdT8HX09vRzV3D0U3CNCAkKdXF1UQjx8PRTcPP08dUBCiNxFYL9FQKC_F1CnV1deBhY0xJzilN5oTQ3g4Kba4izh25qQX58anFBYnJqXmpJvGuAsYmFiZmFkZOhMRFKADFlKeY</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>METHOD OF MAKING AN EXTRUDED THIN FILM, AND THIN FILM SO PRODUCED</title><source>esp@cenet</source><creator>GALLUCCI, Robert Russell ; SANNER, Mark A ; JOHNSON, Peter ; EHRENSBECK, Franklin</creator><creatorcontrib>GALLUCCI, Robert Russell ; SANNER, Mark A ; JOHNSON, Peter ; EHRENSBECK, Franklin</creatorcontrib><description>Method of making an extruded thin film comprising: melt filtering an amorphous thermoplastic composition comprising an amorphous thermoplastic polymer with a glass transition temperature Tg of 130° C. to 280° C. to form a melt filtered amorphous thermoplastic composition; extruding the melt filtered amorphous thermoplastic composition into strands at a temperature TE; cooling the strands to a temperature Tc to form cooled strands; cutting the cooled strands into pellets having a length of 2.0 to 6.0 millimeters; treating the pellets at a temperature Ts to remove particulates having at least one of length, width, and height of less than 0.5 millimeters to form treated pellets; melting the treated pellets in an extruder at a temperature Tp to form a molten composition; and extruding the molten composition through a flat die to form a film having an average thickness less than or equal to 50 micrometers.</description><language>eng ; fre ; ger</language><subject>AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F,C08G ; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING ; CHEMISTRY ; COMPOSITIONS BASED THEREON ; GENERAL PROCESSES OF COMPOUNDING ; MAKING GRANULES OR PREFORMS ; METALLURGY ; ORGANIC MACROMOLECULAR COMPOUNDS ; PERFORMING OPERATIONS ; PREPARATION OR PRETREATMENT OF THE MATERIAL TO BESHAPED ; RECOVERY OF PLASTICS OR OTHER CONSTITUENTS OF WASTE MATERIALCONTAINING PLASTICS ; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDEDFOR ; SHAPING OR JOINING OF PLASTICS ; THEIR PREPARATION OR CHEMICAL WORKING-UP ; TRANSPORTING ; WORKING OF PLASTICS ; WORKING OF SUBSTANCES IN A PLASTIC STATE, IN GENERAL ; WORKING-UP</subject><creationdate>2021</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20211027&amp;DB=EPODOC&amp;CC=EP&amp;NR=3484682B1$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20211027&amp;DB=EPODOC&amp;CC=EP&amp;NR=3484682B1$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>GALLUCCI, Robert Russell</creatorcontrib><creatorcontrib>SANNER, Mark A</creatorcontrib><creatorcontrib>JOHNSON, Peter</creatorcontrib><creatorcontrib>EHRENSBECK, Franklin</creatorcontrib><title>METHOD OF MAKING AN EXTRUDED THIN FILM, AND THIN FILM SO PRODUCED</title><description>Method of making an extruded thin film comprising: melt filtering an amorphous thermoplastic composition comprising an amorphous thermoplastic polymer with a glass transition temperature Tg of 130° C. to 280° C. to form a melt filtered amorphous thermoplastic composition; extruding the melt filtered amorphous thermoplastic composition into strands at a temperature TE; cooling the strands to a temperature Tc to form cooled strands; cutting the cooled strands into pellets having a length of 2.0 to 6.0 millimeters; treating the pellets at a temperature Ts to remove particulates having at least one of length, width, and height of less than 0.5 millimeters to form treated pellets; melting the treated pellets in an extruder at a temperature Tp to form a molten composition; and extruding the molten composition through a flat die to form a film having an average thickness less than or equal to 50 micrometers.</description><subject>AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F,C08G</subject><subject>AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING</subject><subject>CHEMISTRY</subject><subject>COMPOSITIONS BASED THEREON</subject><subject>GENERAL PROCESSES OF COMPOUNDING</subject><subject>MAKING GRANULES OR PREFORMS</subject><subject>METALLURGY</subject><subject>ORGANIC MACROMOLECULAR COMPOUNDS</subject><subject>PERFORMING OPERATIONS</subject><subject>PREPARATION OR PRETREATMENT OF THE MATERIAL TO BESHAPED</subject><subject>RECOVERY OF PLASTICS OR OTHER CONSTITUENTS OF WASTE MATERIALCONTAINING PLASTICS</subject><subject>SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDEDFOR</subject><subject>SHAPING OR JOINING OF PLASTICS</subject><subject>THEIR PREPARATION OR CHEMICAL WORKING-UP</subject><subject>TRANSPORTING</subject><subject>WORKING OF PLASTICS</subject><subject>WORKING OF SUBSTANCES IN A PLASTIC STATE, IN GENERAL</subject><subject>WORKING-UP</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2021</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZHD0dQ3x8HdR8HdT8HX09vRzV3D0U3CNCAkKdXF1UQjx8PRTcPP08dUBCiNxFYL9FQKC_F1CnV1deBhY0xJzilN5oTQ3g4Kba4izh25qQX58anFBYnJqXmpJvGuAsYmFiZmFkZOhMRFKADFlKeY</recordid><startdate>20211027</startdate><enddate>20211027</enddate><creator>GALLUCCI, Robert Russell</creator><creator>SANNER, Mark A</creator><creator>JOHNSON, Peter</creator><creator>EHRENSBECK, Franklin</creator><scope>EVB</scope></search><sort><creationdate>20211027</creationdate><title>METHOD OF MAKING AN EXTRUDED THIN FILM, AND THIN FILM SO PRODUCED</title><author>GALLUCCI, Robert Russell ; SANNER, Mark A ; JOHNSON, Peter ; EHRENSBECK, Franklin</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_EP3484682B13</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; fre ; ger</language><creationdate>2021</creationdate><topic>AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F,C08G</topic><topic>AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING</topic><topic>CHEMISTRY</topic><topic>COMPOSITIONS BASED THEREON</topic><topic>GENERAL PROCESSES OF COMPOUNDING</topic><topic>MAKING GRANULES OR PREFORMS</topic><topic>METALLURGY</topic><topic>ORGANIC MACROMOLECULAR COMPOUNDS</topic><topic>PERFORMING OPERATIONS</topic><topic>PREPARATION OR PRETREATMENT OF THE MATERIAL TO BESHAPED</topic><topic>RECOVERY OF PLASTICS OR OTHER CONSTITUENTS OF WASTE MATERIALCONTAINING PLASTICS</topic><topic>SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDEDFOR</topic><topic>SHAPING OR JOINING OF PLASTICS</topic><topic>THEIR PREPARATION OR CHEMICAL WORKING-UP</topic><topic>TRANSPORTING</topic><topic>WORKING OF PLASTICS</topic><topic>WORKING OF SUBSTANCES IN A PLASTIC STATE, IN GENERAL</topic><topic>WORKING-UP</topic><toplevel>online_resources</toplevel><creatorcontrib>GALLUCCI, Robert Russell</creatorcontrib><creatorcontrib>SANNER, Mark A</creatorcontrib><creatorcontrib>JOHNSON, Peter</creatorcontrib><creatorcontrib>EHRENSBECK, Franklin</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>GALLUCCI, Robert Russell</au><au>SANNER, Mark A</au><au>JOHNSON, Peter</au><au>EHRENSBECK, Franklin</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>METHOD OF MAKING AN EXTRUDED THIN FILM, AND THIN FILM SO PRODUCED</title><date>2021-10-27</date><risdate>2021</risdate><abstract>Method of making an extruded thin film comprising: melt filtering an amorphous thermoplastic composition comprising an amorphous thermoplastic polymer with a glass transition temperature Tg of 130° C. to 280° C. to form a melt filtered amorphous thermoplastic composition; extruding the melt filtered amorphous thermoplastic composition into strands at a temperature TE; cooling the strands to a temperature Tc to form cooled strands; cutting the cooled strands into pellets having a length of 2.0 to 6.0 millimeters; treating the pellets at a temperature Ts to remove particulates having at least one of length, width, and height of less than 0.5 millimeters to form treated pellets; melting the treated pellets in an extruder at a temperature Tp to form a molten composition; and extruding the molten composition through a flat die to form a film having an average thickness less than or equal to 50 micrometers.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng ; fre ; ger
recordid cdi_epo_espacenet_EP3484682B1
source esp@cenet
subjects AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F,C08G
AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING
CHEMISTRY
COMPOSITIONS BASED THEREON
GENERAL PROCESSES OF COMPOUNDING
MAKING GRANULES OR PREFORMS
METALLURGY
ORGANIC MACROMOLECULAR COMPOUNDS
PERFORMING OPERATIONS
PREPARATION OR PRETREATMENT OF THE MATERIAL TO BESHAPED
RECOVERY OF PLASTICS OR OTHER CONSTITUENTS OF WASTE MATERIALCONTAINING PLASTICS
SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDEDFOR
SHAPING OR JOINING OF PLASTICS
THEIR PREPARATION OR CHEMICAL WORKING-UP
TRANSPORTING
WORKING OF PLASTICS
WORKING OF SUBSTANCES IN A PLASTIC STATE, IN GENERAL
WORKING-UP
title METHOD OF MAKING AN EXTRUDED THIN FILM, AND THIN FILM SO PRODUCED
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-28T02%3A21%3A10IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=GALLUCCI,%20Robert%20Russell&rft.date=2021-10-27&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EEP3484682B1%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true