FLAME RETARDANT POLYCARBONATE COMPOSITION, A METHOD OF MAKING AND OF USING THE SAME

In an embodiment, a composition comprises, based on the total weight of the composition, 55 to 85 wt % of a polycarbonate; 10 to 25 wt % of an organopolysiloxane-polycarbonate block copolymer; 5 to 15 wt % of a phosphine oxide; and 0 to 3 wt % of an impact modifier. In another embodiment, a method o...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: WEI, Zhenke, ZHENG, Yun, SHI, Hongtao, CHEN, Lin
Format: Patent
Sprache:eng ; fre ; ger
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator WEI, Zhenke
ZHENG, Yun
SHI, Hongtao
CHEN, Lin
description In an embodiment, a composition comprises, based on the total weight of the composition, 55 to 85 wt % of a polycarbonate; 10 to 25 wt % of an organopolysiloxane-polycarbonate block copolymer; 5 to 15 wt % of a phosphine oxide; and 0 to 3 wt % of an impact modifier. In another embodiment, a method of making a composition comprises extruding a mixture to form a composition comprising, based on the total weight of the composition, 55 to 85 wt % of a polycarbonate; 10 to 25 wt % of an organopolysiloxane-polycarbonate block copolymer; 5 to 15 wt % of a phosphine oxide; and 0 to 3 wt % of an impact modifier comprises extruding the polycarbonate, the organopolysiloxane-polycarbonate block copolymer, and the phosphine oxide to form the composition.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_EP3353242B1</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>EP3353242B1</sourcerecordid><originalsourceid>FETCH-epo_espacenet_EP3353242B13</originalsourceid><addsrcrecordid>eNrjZAh283H0dVUIcg1xDHJx9AtRCPD3iXR2DHLy93MMcVVw9vcN8A_2DPH099NRcFTwdQ3x8HdR8HdT8HX09vRzV3D0A_NCg0GcEA9XhWCgaTwMrGmJOcWpvFCam0HBzTXE2UM3tSA_PrW4IDE5NS-1JN41wNjY1NjIxMjJ0JgIJQBzPC7w</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>FLAME RETARDANT POLYCARBONATE COMPOSITION, A METHOD OF MAKING AND OF USING THE SAME</title><source>esp@cenet</source><creator>WEI, Zhenke ; ZHENG, Yun ; SHI, Hongtao ; CHEN, Lin</creator><creatorcontrib>WEI, Zhenke ; ZHENG, Yun ; SHI, Hongtao ; CHEN, Lin</creatorcontrib><description>In an embodiment, a composition comprises, based on the total weight of the composition, 55 to 85 wt % of a polycarbonate; 10 to 25 wt % of an organopolysiloxane-polycarbonate block copolymer; 5 to 15 wt % of a phosphine oxide; and 0 to 3 wt % of an impact modifier. In another embodiment, a method of making a composition comprises extruding a mixture to form a composition comprising, based on the total weight of the composition, 55 to 85 wt % of a polycarbonate; 10 to 25 wt % of an organopolysiloxane-polycarbonate block copolymer; 5 to 15 wt % of a phosphine oxide; and 0 to 3 wt % of an impact modifier comprises extruding the polycarbonate, the organopolysiloxane-polycarbonate block copolymer, and the phosphine oxide to form the composition.</description><language>eng ; fre ; ger</language><subject>CHEMISTRY ; COMPOSITIONS BASED THEREON ; COMPOSITIONS OF MACROMOLECULAR COMPOUNDS ; MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONSONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS ; METALLURGY ; ORGANIC MACROMOLECULAR COMPOUNDS ; THEIR PREPARATION OR CHEMICAL WORKING-UP</subject><creationdate>2019</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20191113&amp;DB=EPODOC&amp;CC=EP&amp;NR=3353242B1$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25563,76318</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20191113&amp;DB=EPODOC&amp;CC=EP&amp;NR=3353242B1$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>WEI, Zhenke</creatorcontrib><creatorcontrib>ZHENG, Yun</creatorcontrib><creatorcontrib>SHI, Hongtao</creatorcontrib><creatorcontrib>CHEN, Lin</creatorcontrib><title>FLAME RETARDANT POLYCARBONATE COMPOSITION, A METHOD OF MAKING AND OF USING THE SAME</title><description>In an embodiment, a composition comprises, based on the total weight of the composition, 55 to 85 wt % of a polycarbonate; 10 to 25 wt % of an organopolysiloxane-polycarbonate block copolymer; 5 to 15 wt % of a phosphine oxide; and 0 to 3 wt % of an impact modifier. In another embodiment, a method of making a composition comprises extruding a mixture to form a composition comprising, based on the total weight of the composition, 55 to 85 wt % of a polycarbonate; 10 to 25 wt % of an organopolysiloxane-polycarbonate block copolymer; 5 to 15 wt % of a phosphine oxide; and 0 to 3 wt % of an impact modifier comprises extruding the polycarbonate, the organopolysiloxane-polycarbonate block copolymer, and the phosphine oxide to form the composition.</description><subject>CHEMISTRY</subject><subject>COMPOSITIONS BASED THEREON</subject><subject>COMPOSITIONS OF MACROMOLECULAR COMPOUNDS</subject><subject>MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONSONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS</subject><subject>METALLURGY</subject><subject>ORGANIC MACROMOLECULAR COMPOUNDS</subject><subject>THEIR PREPARATION OR CHEMICAL WORKING-UP</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2019</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZAh283H0dVUIcg1xDHJx9AtRCPD3iXR2DHLy93MMcVVw9vcN8A_2DPH099NRcFTwdQ3x8HdR8HdT8HX09vRzV3D0A_NCg0GcEA9XhWCgaTwMrGmJOcWpvFCam0HBzTXE2UM3tSA_PrW4IDE5NS-1JN41wNjY1NjIxMjJ0JgIJQBzPC7w</recordid><startdate>20191113</startdate><enddate>20191113</enddate><creator>WEI, Zhenke</creator><creator>ZHENG, Yun</creator><creator>SHI, Hongtao</creator><creator>CHEN, Lin</creator><scope>EVB</scope></search><sort><creationdate>20191113</creationdate><title>FLAME RETARDANT POLYCARBONATE COMPOSITION, A METHOD OF MAKING AND OF USING THE SAME</title><author>WEI, Zhenke ; ZHENG, Yun ; SHI, Hongtao ; CHEN, Lin</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_EP3353242B13</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; fre ; ger</language><creationdate>2019</creationdate><topic>CHEMISTRY</topic><topic>COMPOSITIONS BASED THEREON</topic><topic>COMPOSITIONS OF MACROMOLECULAR COMPOUNDS</topic><topic>MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONSONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS</topic><topic>METALLURGY</topic><topic>ORGANIC MACROMOLECULAR COMPOUNDS</topic><topic>THEIR PREPARATION OR CHEMICAL WORKING-UP</topic><toplevel>online_resources</toplevel><creatorcontrib>WEI, Zhenke</creatorcontrib><creatorcontrib>ZHENG, Yun</creatorcontrib><creatorcontrib>SHI, Hongtao</creatorcontrib><creatorcontrib>CHEN, Lin</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>WEI, Zhenke</au><au>ZHENG, Yun</au><au>SHI, Hongtao</au><au>CHEN, Lin</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>FLAME RETARDANT POLYCARBONATE COMPOSITION, A METHOD OF MAKING AND OF USING THE SAME</title><date>2019-11-13</date><risdate>2019</risdate><abstract>In an embodiment, a composition comprises, based on the total weight of the composition, 55 to 85 wt % of a polycarbonate; 10 to 25 wt % of an organopolysiloxane-polycarbonate block copolymer; 5 to 15 wt % of a phosphine oxide; and 0 to 3 wt % of an impact modifier. In another embodiment, a method of making a composition comprises extruding a mixture to form a composition comprising, based on the total weight of the composition, 55 to 85 wt % of a polycarbonate; 10 to 25 wt % of an organopolysiloxane-polycarbonate block copolymer; 5 to 15 wt % of a phosphine oxide; and 0 to 3 wt % of an impact modifier comprises extruding the polycarbonate, the organopolysiloxane-polycarbonate block copolymer, and the phosphine oxide to form the composition.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng ; fre ; ger
recordid cdi_epo_espacenet_EP3353242B1
source esp@cenet
subjects CHEMISTRY
COMPOSITIONS BASED THEREON
COMPOSITIONS OF MACROMOLECULAR COMPOUNDS
MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONSONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
METALLURGY
ORGANIC MACROMOLECULAR COMPOUNDS
THEIR PREPARATION OR CHEMICAL WORKING-UP
title FLAME RETARDANT POLYCARBONATE COMPOSITION, A METHOD OF MAKING AND OF USING THE SAME
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-11T16%3A15%3A12IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=WEI,%20Zhenke&rft.date=2019-11-13&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EEP3353242B1%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true