METHOD FOR PRODUCING COMMINGLED YARN

Provided is a method for manufacturing a commingled yarn that is capable of keeping a high level of dispersion of the continuous reinforcing fiber and the continuous resin fiber, moderately flexible, and less likely to cause fiber separation, and a commingled yarn a wind-up article and a woven fabri...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: MATSUMOTO Nobuhiko, TAKAGI Mitsuro, NAKAI Asami, KAJI Masataka, OOTANI Akio
Format: Patent
Sprache:eng ; fre ; ger
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator MATSUMOTO Nobuhiko
TAKAGI Mitsuro
NAKAI Asami
KAJI Masataka
OOTANI Akio
description Provided is a method for manufacturing a commingled yarn that is capable of keeping a high level of dispersion of the continuous reinforcing fiber and the continuous resin fiber, moderately flexible, and less likely to cause fiber separation, and a commingled yarn a wind-up article and a woven fabric. The method for manufacturing a commingled yarn includes commingling a thermoplastic resin fiber having a treatment agent for the thermoplastic resin fiber on a surface thereof, and a continuous reinforcing fiber having a treatment agent for the continuous reinforcing fiber on a surface thereof, and heating the commingled fibers at a temperature in a range from a melting point of the thermoplastic resin composing the thermoplastic resin fiber, up to 30K higher than the melting point, wherein the thermoplastic resin has a product of the melting point thereof and a thermal conductivity thereof of 100 to 150, where the thermal conductivity is measured in compliance with ASTM D177, the continuous Reinforcing fiber has an amount of the treatment agent therefore of 0.01 to 2.0% by weight thereof, and the thermoplastic resin fiber has an amount of the treatment agent therefor of 0.1 to 2.0% by weight thereof; where the melting point is given in kelvins (K), and the thermal conductivity is given in M/m·K.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_EP3192904B1</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>EP3192904B1</sourcerecordid><originalsourceid>FETCH-epo_espacenet_EP3192904B13</originalsourceid><addsrcrecordid>eNrjZFDxdQ3x8HdRcPMPUggI8ncJdfb0c1dw9vf1BdI-ri4KkY5BfjwMrGmJOcWpvFCam0HBzTXE2UM3tSA_PrW4IDE5NS-1JN41wNjQ0sjSwMTJ0JgIJQA41CKZ</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>METHOD FOR PRODUCING COMMINGLED YARN</title><source>esp@cenet</source><creator>MATSUMOTO Nobuhiko ; TAKAGI Mitsuro ; NAKAI Asami ; KAJI Masataka ; OOTANI Akio</creator><creatorcontrib>MATSUMOTO Nobuhiko ; TAKAGI Mitsuro ; NAKAI Asami ; KAJI Masataka ; OOTANI Akio</creatorcontrib><description>Provided is a method for manufacturing a commingled yarn that is capable of keeping a high level of dispersion of the continuous reinforcing fiber and the continuous resin fiber, moderately flexible, and less likely to cause fiber separation, and a commingled yarn a wind-up article and a woven fabric. The method for manufacturing a commingled yarn includes commingling a thermoplastic resin fiber having a treatment agent for the thermoplastic resin fiber on a surface thereof, and a continuous reinforcing fiber having a treatment agent for the continuous reinforcing fiber on a surface thereof, and heating the commingled fibers at a temperature in a range from a melting point of the thermoplastic resin composing the thermoplastic resin fiber, up to 30K higher than the melting point, wherein the thermoplastic resin has a product of the melting point thereof and a thermal conductivity thereof of 100 to 150, where the thermal conductivity is measured in compliance with ASTM D177, the continuous Reinforcing fiber has an amount of the treatment agent therefore of 0.01 to 2.0% by weight thereof, and the thermoplastic resin fiber has an amount of the treatment agent therefor of 0.1 to 2.0% by weight thereof; where the melting point is given in kelvins (K), and the thermal conductivity is given in M/m·K.</description><language>eng ; fre ; ger</language><subject>CRIMPING OR CURLING FIBRES, FILAMENTS, THREADS, ORYARNS ; LOOMS ; MECHANICAL FINISHING OF YARNS OR ROPES ; METHODS OF WEAVING ; TEXTILES ; WARPING OR BEAMING ; WEAVING ; WOVEN FABRICS ; YARNS ; YARNS OR THREADS</subject><creationdate>2024</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20241127&amp;DB=EPODOC&amp;CC=EP&amp;NR=3192904B1$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20241127&amp;DB=EPODOC&amp;CC=EP&amp;NR=3192904B1$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>MATSUMOTO Nobuhiko</creatorcontrib><creatorcontrib>TAKAGI Mitsuro</creatorcontrib><creatorcontrib>NAKAI Asami</creatorcontrib><creatorcontrib>KAJI Masataka</creatorcontrib><creatorcontrib>OOTANI Akio</creatorcontrib><title>METHOD FOR PRODUCING COMMINGLED YARN</title><description>Provided is a method for manufacturing a commingled yarn that is capable of keeping a high level of dispersion of the continuous reinforcing fiber and the continuous resin fiber, moderately flexible, and less likely to cause fiber separation, and a commingled yarn a wind-up article and a woven fabric. The method for manufacturing a commingled yarn includes commingling a thermoplastic resin fiber having a treatment agent for the thermoplastic resin fiber on a surface thereof, and a continuous reinforcing fiber having a treatment agent for the continuous reinforcing fiber on a surface thereof, and heating the commingled fibers at a temperature in a range from a melting point of the thermoplastic resin composing the thermoplastic resin fiber, up to 30K higher than the melting point, wherein the thermoplastic resin has a product of the melting point thereof and a thermal conductivity thereof of 100 to 150, where the thermal conductivity is measured in compliance with ASTM D177, the continuous Reinforcing fiber has an amount of the treatment agent therefore of 0.01 to 2.0% by weight thereof, and the thermoplastic resin fiber has an amount of the treatment agent therefor of 0.1 to 2.0% by weight thereof; where the melting point is given in kelvins (K), and the thermal conductivity is given in M/m·K.</description><subject>CRIMPING OR CURLING FIBRES, FILAMENTS, THREADS, ORYARNS</subject><subject>LOOMS</subject><subject>MECHANICAL FINISHING OF YARNS OR ROPES</subject><subject>METHODS OF WEAVING</subject><subject>TEXTILES</subject><subject>WARPING OR BEAMING</subject><subject>WEAVING</subject><subject>WOVEN FABRICS</subject><subject>YARNS</subject><subject>YARNS OR THREADS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2024</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZFDxdQ3x8HdRcPMPUggI8ncJdfb0c1dw9vf1BdI-ri4KkY5BfjwMrGmJOcWpvFCam0HBzTXE2UM3tSA_PrW4IDE5NS-1JN41wNjQ0sjSwMTJ0JgIJQA41CKZ</recordid><startdate>20241127</startdate><enddate>20241127</enddate><creator>MATSUMOTO Nobuhiko</creator><creator>TAKAGI Mitsuro</creator><creator>NAKAI Asami</creator><creator>KAJI Masataka</creator><creator>OOTANI Akio</creator><scope>EVB</scope></search><sort><creationdate>20241127</creationdate><title>METHOD FOR PRODUCING COMMINGLED YARN</title><author>MATSUMOTO Nobuhiko ; TAKAGI Mitsuro ; NAKAI Asami ; KAJI Masataka ; OOTANI Akio</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_EP3192904B13</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; fre ; ger</language><creationdate>2024</creationdate><topic>CRIMPING OR CURLING FIBRES, FILAMENTS, THREADS, ORYARNS</topic><topic>LOOMS</topic><topic>MECHANICAL FINISHING OF YARNS OR ROPES</topic><topic>METHODS OF WEAVING</topic><topic>TEXTILES</topic><topic>WARPING OR BEAMING</topic><topic>WEAVING</topic><topic>WOVEN FABRICS</topic><topic>YARNS</topic><topic>YARNS OR THREADS</topic><toplevel>online_resources</toplevel><creatorcontrib>MATSUMOTO Nobuhiko</creatorcontrib><creatorcontrib>TAKAGI Mitsuro</creatorcontrib><creatorcontrib>NAKAI Asami</creatorcontrib><creatorcontrib>KAJI Masataka</creatorcontrib><creatorcontrib>OOTANI Akio</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>MATSUMOTO Nobuhiko</au><au>TAKAGI Mitsuro</au><au>NAKAI Asami</au><au>KAJI Masataka</au><au>OOTANI Akio</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>METHOD FOR PRODUCING COMMINGLED YARN</title><date>2024-11-27</date><risdate>2024</risdate><abstract>Provided is a method for manufacturing a commingled yarn that is capable of keeping a high level of dispersion of the continuous reinforcing fiber and the continuous resin fiber, moderately flexible, and less likely to cause fiber separation, and a commingled yarn a wind-up article and a woven fabric. The method for manufacturing a commingled yarn includes commingling a thermoplastic resin fiber having a treatment agent for the thermoplastic resin fiber on a surface thereof, and a continuous reinforcing fiber having a treatment agent for the continuous reinforcing fiber on a surface thereof, and heating the commingled fibers at a temperature in a range from a melting point of the thermoplastic resin composing the thermoplastic resin fiber, up to 30K higher than the melting point, wherein the thermoplastic resin has a product of the melting point thereof and a thermal conductivity thereof of 100 to 150, where the thermal conductivity is measured in compliance with ASTM D177, the continuous Reinforcing fiber has an amount of the treatment agent therefore of 0.01 to 2.0% by weight thereof, and the thermoplastic resin fiber has an amount of the treatment agent therefor of 0.1 to 2.0% by weight thereof; where the melting point is given in kelvins (K), and the thermal conductivity is given in M/m·K.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng ; fre ; ger
recordid cdi_epo_espacenet_EP3192904B1
source esp@cenet
subjects CRIMPING OR CURLING FIBRES, FILAMENTS, THREADS, ORYARNS
LOOMS
MECHANICAL FINISHING OF YARNS OR ROPES
METHODS OF WEAVING
TEXTILES
WARPING OR BEAMING
WEAVING
WOVEN FABRICS
YARNS
YARNS OR THREADS
title METHOD FOR PRODUCING COMMINGLED YARN
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-21T13%3A02%3A11IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=MATSUMOTO%20Nobuhiko&rft.date=2024-11-27&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EEP3192904B1%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true