METHOD FOR PRODUCING R-T-B SINTERED MAGNET
A step is provided which performs a heat treatment at the sintering temperature of a sintered R-T-B based magnet or lower, while a powder of an RLM alloy (where RL is Nd and/or Pr; M is one or more selected from among Cu, Fe, Ga, Co and Ni) and a powder of an RH fluoride (where RH is Dy and/or Tb) a...
Gespeichert in:
1. Verfasser: | |
---|---|
Format: | Patent |
Sprache: | eng ; fre ; ger |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | A step is provided which performs a heat treatment at the sintering temperature of a sintered R-T-B based magnet or lower, while a powder of an RLM alloy (where RL is Nd and/or Pr; M is one or more selected from among Cu, Fe, Ga, Co and Ni) and a powder of an RH fluoride (where RH is Dy and/or Tb) are present on a surface of the sintered R-T-B based magnet. The RLM alloy contains RL in an amount of 50 at% or more, and a melting point of the RLM alloy is equal to or less than a temperature of the heat treatment. The heat treatment is performed while the RLM alloy powder and the RH fluoride powder are present on the surface of the sintered R-T-B based magnet at a mass ratio of RLM alloy: RH fluoride = 96:4 to 5:5. |
---|