SEMICONDUCTIVE POLYMER COMPOSITION FOR ELECTRIC POWER CABLES

The invention provides a novel semiconductive polymer composition with improved smoothness and dispersibility of carbon black when compounding the polymer composition and feasible balance with other properties such as volume resistivity. The semiconductive polymer composition comprises (a) from 30 t...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: WALTER, PETER, JOHANSSON, MALIN, NOYENS, KOENRAAD, SVANBERG, CHRISTER, SKOGMAN, FREDRIK, JÄGER, KARL-MICHAEL, UEMATSU, TAKASHI
Format: Patent
Sprache:eng ; fre ; ger
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator WALTER, PETER
JOHANSSON, MALIN
NOYENS, KOENRAAD
SVANBERG, CHRISTER
SKOGMAN, FREDRIK
JÄGER, KARL-MICHAEL
UEMATSU, TAKASHI
description The invention provides a novel semiconductive polymer composition with improved smoothness and dispersibility of carbon black when compounding the polymer composition and feasible balance with other properties such as volume resistivity. The semiconductive polymer composition comprises (a) from 30 to 90 wt% of a polymer component, (b) from 10 to 70 wt% of carbon black and the carbon black (b) has a mass pellet strength (MPS) according to ASTM D1937-13 of from 50 to 250 N. The invention further relates to a process for preparing the semiconductive polymer composition comprising the steps of: i) introducing 30-90 wt% of a polymer component as defined above and 0-8 wt% additives in a mixer device and mixing the polymer component and additives at elevated temperature such that a polymer melt is obtained; ii) adding 10-70 wt% of a carbon black as defined above to the polymer melt and further mixing of the polymer melt.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_EP3083768A1</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>EP3083768A1</sourcerecordid><originalsourceid>FETCH-epo_espacenet_EP3083768A13</originalsourceid><addsrcrecordid>eNrjZLAJdvX1dPb3cwl1DvEMc1UI8PeJ9HUNUnD29w3wD_YM8fT3U3DzD1Jw9XF1DgnydAYqCAdJOzr5uAbzMLCmJeYUp_JCaW4GBTfXEGcP3dSC_PjU4oLE5NS81JJ41wBjAwtjczMLR0NjIpQAAOodKZg</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>SEMICONDUCTIVE POLYMER COMPOSITION FOR ELECTRIC POWER CABLES</title><source>esp@cenet</source><creator>WALTER, PETER ; JOHANSSON, MALIN ; NOYENS, KOENRAAD ; SVANBERG, CHRISTER ; SKOGMAN, FREDRIK ; JÄGER, KARL-MICHAEL ; UEMATSU, TAKASHI</creator><creatorcontrib>WALTER, PETER ; JOHANSSON, MALIN ; NOYENS, KOENRAAD ; SVANBERG, CHRISTER ; SKOGMAN, FREDRIK ; JÄGER, KARL-MICHAEL ; UEMATSU, TAKASHI</creatorcontrib><description>The invention provides a novel semiconductive polymer composition with improved smoothness and dispersibility of carbon black when compounding the polymer composition and feasible balance with other properties such as volume resistivity. The semiconductive polymer composition comprises (a) from 30 to 90 wt% of a polymer component, (b) from 10 to 70 wt% of carbon black and the carbon black (b) has a mass pellet strength (MPS) according to ASTM D1937-13 of from 50 to 250 N. The invention further relates to a process for preparing the semiconductive polymer composition comprising the steps of: i) introducing 30-90 wt% of a polymer component as defined above and 0-8 wt% additives in a mixer device and mixing the polymer component and additives at elevated temperature such that a polymer melt is obtained; ii) adding 10-70 wt% of a carbon black as defined above to the polymer melt and further mixing of the polymer melt.</description><language>eng ; fre ; ger</language><subject>AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F,C08G ; BASIC ELECTRIC ELEMENTS ; CABLES ; CHEMISTRY ; COMPOSITIONS BASED THEREON ; COMPOSITIONS OF MACROMOLECULAR COMPOUNDS ; CONDUCTORS ; ELECTRICITY ; GENERAL PROCESSES OF COMPOUNDING ; INSULATORS ; METALLURGY ; ORGANIC MACROMOLECULAR COMPOUNDS ; SELECTION OF MATERIALS FOR THEIR CONDUCTIVE, INSULATING ORDIELECTRIC PROPERTIES ; THEIR PREPARATION OR CHEMICAL WORKING-UP ; WORKING-UP</subject><creationdate>2016</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20161026&amp;DB=EPODOC&amp;CC=EP&amp;NR=3083768A1$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20161026&amp;DB=EPODOC&amp;CC=EP&amp;NR=3083768A1$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>WALTER, PETER</creatorcontrib><creatorcontrib>JOHANSSON, MALIN</creatorcontrib><creatorcontrib>NOYENS, KOENRAAD</creatorcontrib><creatorcontrib>SVANBERG, CHRISTER</creatorcontrib><creatorcontrib>SKOGMAN, FREDRIK</creatorcontrib><creatorcontrib>JÄGER, KARL-MICHAEL</creatorcontrib><creatorcontrib>UEMATSU, TAKASHI</creatorcontrib><title>SEMICONDUCTIVE POLYMER COMPOSITION FOR ELECTRIC POWER CABLES</title><description>The invention provides a novel semiconductive polymer composition with improved smoothness and dispersibility of carbon black when compounding the polymer composition and feasible balance with other properties such as volume resistivity. The semiconductive polymer composition comprises (a) from 30 to 90 wt% of a polymer component, (b) from 10 to 70 wt% of carbon black and the carbon black (b) has a mass pellet strength (MPS) according to ASTM D1937-13 of from 50 to 250 N. The invention further relates to a process for preparing the semiconductive polymer composition comprising the steps of: i) introducing 30-90 wt% of a polymer component as defined above and 0-8 wt% additives in a mixer device and mixing the polymer component and additives at elevated temperature such that a polymer melt is obtained; ii) adding 10-70 wt% of a carbon black as defined above to the polymer melt and further mixing of the polymer melt.</description><subject>AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F,C08G</subject><subject>BASIC ELECTRIC ELEMENTS</subject><subject>CABLES</subject><subject>CHEMISTRY</subject><subject>COMPOSITIONS BASED THEREON</subject><subject>COMPOSITIONS OF MACROMOLECULAR COMPOUNDS</subject><subject>CONDUCTORS</subject><subject>ELECTRICITY</subject><subject>GENERAL PROCESSES OF COMPOUNDING</subject><subject>INSULATORS</subject><subject>METALLURGY</subject><subject>ORGANIC MACROMOLECULAR COMPOUNDS</subject><subject>SELECTION OF MATERIALS FOR THEIR CONDUCTIVE, INSULATING ORDIELECTRIC PROPERTIES</subject><subject>THEIR PREPARATION OR CHEMICAL WORKING-UP</subject><subject>WORKING-UP</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2016</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZLAJdvX1dPb3cwl1DvEMc1UI8PeJ9HUNUnD29w3wD_YM8fT3U3DzD1Jw9XF1DgnydAYqCAdJOzr5uAbzMLCmJeYUp_JCaW4GBTfXEGcP3dSC_PjU4oLE5NS81JJ41wBjAwtjczMLR0NjIpQAAOodKZg</recordid><startdate>20161026</startdate><enddate>20161026</enddate><creator>WALTER, PETER</creator><creator>JOHANSSON, MALIN</creator><creator>NOYENS, KOENRAAD</creator><creator>SVANBERG, CHRISTER</creator><creator>SKOGMAN, FREDRIK</creator><creator>JÄGER, KARL-MICHAEL</creator><creator>UEMATSU, TAKASHI</creator><scope>EVB</scope></search><sort><creationdate>20161026</creationdate><title>SEMICONDUCTIVE POLYMER COMPOSITION FOR ELECTRIC POWER CABLES</title><author>WALTER, PETER ; JOHANSSON, MALIN ; NOYENS, KOENRAAD ; SVANBERG, CHRISTER ; SKOGMAN, FREDRIK ; JÄGER, KARL-MICHAEL ; UEMATSU, TAKASHI</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_EP3083768A13</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; fre ; ger</language><creationdate>2016</creationdate><topic>AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F,C08G</topic><topic>BASIC ELECTRIC ELEMENTS</topic><topic>CABLES</topic><topic>CHEMISTRY</topic><topic>COMPOSITIONS BASED THEREON</topic><topic>COMPOSITIONS OF MACROMOLECULAR COMPOUNDS</topic><topic>CONDUCTORS</topic><topic>ELECTRICITY</topic><topic>GENERAL PROCESSES OF COMPOUNDING</topic><topic>INSULATORS</topic><topic>METALLURGY</topic><topic>ORGANIC MACROMOLECULAR COMPOUNDS</topic><topic>SELECTION OF MATERIALS FOR THEIR CONDUCTIVE, INSULATING ORDIELECTRIC PROPERTIES</topic><topic>THEIR PREPARATION OR CHEMICAL WORKING-UP</topic><topic>WORKING-UP</topic><toplevel>online_resources</toplevel><creatorcontrib>WALTER, PETER</creatorcontrib><creatorcontrib>JOHANSSON, MALIN</creatorcontrib><creatorcontrib>NOYENS, KOENRAAD</creatorcontrib><creatorcontrib>SVANBERG, CHRISTER</creatorcontrib><creatorcontrib>SKOGMAN, FREDRIK</creatorcontrib><creatorcontrib>JÄGER, KARL-MICHAEL</creatorcontrib><creatorcontrib>UEMATSU, TAKASHI</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>WALTER, PETER</au><au>JOHANSSON, MALIN</au><au>NOYENS, KOENRAAD</au><au>SVANBERG, CHRISTER</au><au>SKOGMAN, FREDRIK</au><au>JÄGER, KARL-MICHAEL</au><au>UEMATSU, TAKASHI</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>SEMICONDUCTIVE POLYMER COMPOSITION FOR ELECTRIC POWER CABLES</title><date>2016-10-26</date><risdate>2016</risdate><abstract>The invention provides a novel semiconductive polymer composition with improved smoothness and dispersibility of carbon black when compounding the polymer composition and feasible balance with other properties such as volume resistivity. The semiconductive polymer composition comprises (a) from 30 to 90 wt% of a polymer component, (b) from 10 to 70 wt% of carbon black and the carbon black (b) has a mass pellet strength (MPS) according to ASTM D1937-13 of from 50 to 250 N. The invention further relates to a process for preparing the semiconductive polymer composition comprising the steps of: i) introducing 30-90 wt% of a polymer component as defined above and 0-8 wt% additives in a mixer device and mixing the polymer component and additives at elevated temperature such that a polymer melt is obtained; ii) adding 10-70 wt% of a carbon black as defined above to the polymer melt and further mixing of the polymer melt.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng ; fre ; ger
recordid cdi_epo_espacenet_EP3083768A1
source esp@cenet
subjects AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F,C08G
BASIC ELECTRIC ELEMENTS
CABLES
CHEMISTRY
COMPOSITIONS BASED THEREON
COMPOSITIONS OF MACROMOLECULAR COMPOUNDS
CONDUCTORS
ELECTRICITY
GENERAL PROCESSES OF COMPOUNDING
INSULATORS
METALLURGY
ORGANIC MACROMOLECULAR COMPOUNDS
SELECTION OF MATERIALS FOR THEIR CONDUCTIVE, INSULATING ORDIELECTRIC PROPERTIES
THEIR PREPARATION OR CHEMICAL WORKING-UP
WORKING-UP
title SEMICONDUCTIVE POLYMER COMPOSITION FOR ELECTRIC POWER CABLES
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-01T03%3A26%3A23IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=WALTER,%20PETER&rft.date=2016-10-26&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EEP3083768A1%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true