DRIER FOR AUTO-OXIDISABLE COATING COMPOSITIONS

The invention relates to a drier for an air drying auto-oxidisable resin composition comprising a polymer comprising unsaturated fatty acid residues, the drier comprising a manganese triaza complex comprising the following structure: wherein R1=C1-C20alkyl optionally substituted with heteroatoms, or...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: FLAPPER, Jitte, MEIJER, Michel Daniel
Format: Patent
Sprache:eng ; fre ; ger
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:The invention relates to a drier for an air drying auto-oxidisable resin composition comprising a polymer comprising unsaturated fatty acid residues, the drier comprising a manganese triaza complex comprising the following structure: wherein R1=C1-C20alkyl optionally substituted with heteroatoms, or C6-C20aryl optionally substituted with heteroatoms; X and Y are independently selected from O and OC(R2)O, in which a=4 when X=O, and a=3 when X=OC(R2)O, and in which b=4 when Y=O, and b=3 when Y=OC(R2)O; Wherein R2=C1-C20alkyl optionally substituted with heteroatoms, C6-C20 aryl optionally substituted with heteroatoms, or a polymeric residue, and one or more anions, being chosen PF6-, SbF6-, AsF6-, BF4-, B(C6F5)4-, Cl-, Br-, I-, NO3-, or R3COO- or SO42−, and wherein R3 is C1-C20alkyl optionally substituted with heteroatoms, C6-C20aryl 1optionally substituted with heteroatoms, or a polymeric residue, and wherein the drier comprises an additional amount of, 4,7-trialkyl-1,4,7-triazacyclononane; wherein the 1,4,7-trialkyl-1,4,7-triazacyclononane (L) is present in an amount such that the molar ratio of L:Mn is at least 1.25:1 and preferably at least 1.5:1.