PROCESS FOR MANUFACTURING GRAPHITE POWDER FOR LITHIUM SECONDARY BATTERY NEGATIVE ELECTRODE MATERIAL

A method for producing a graphite powder for use as a lithium secondary battery negative electrode material easily produces a graphite powder for use as a lithium secondary battery negative electrode material that has a small specific surface area while reducing the energy consumption, and achieving...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: YAMAKI MOTOHIRO, KUROYANAGI AKIHIRO, KOMORIYA MAYURI, FUKUGAWA TOMOHITO, YAMAMOTO KAZUHIRO
Format: Patent
Sprache:eng ; fre ; ger
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator YAMAKI MOTOHIRO
KUROYANAGI AKIHIRO
KOMORIYA MAYURI
FUKUGAWA TOMOHITO
YAMAMOTO KAZUHIRO
description A method for producing a graphite powder for use as a lithium secondary battery negative electrode material easily produces a graphite powder for use as a lithium secondary battery negative electrode material that has a small specific surface area while reducing the energy consumption, and achieving a high graphitization efficiency. The method includes melt-mixing a coke powder and a carbon precursor binder so that an amount of fixed carbon included in the carbon precursor binder is 5 to 15 parts by mass based on 100 parts by mass of the coke powder, to prepare a mixture, and pressing the mixture to prepare a compact, the coke powder being obtained by heating a green coke powder at 600 to 1450°C in a non-oxidizing atmosphere, the green coke powder having a cumulative particle size at 50% in a volumetric cumulative particle size distribution of 5 to 50 µm; heating the compact in a non-oxidizing atmosphere to effect carbonization and graphitization to obtain a graphitized compact; and grinding the graphitized compact.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_EP2913873A4</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>EP2913873A4</sourcerecordid><originalsourceid>FETCH-epo_espacenet_EP2913873A43</originalsourceid><addsrcrecordid>eNqNjEEKwjAQAHvxIOof9gMeNIJ6XNNNG2iTsN1UPJVS4km0UP-PRXyApznMMMtsCOw1NQ0Yz1Cjiwa1RLaugIIxlFYIgr_mxN-islLaWEND2rsc-QYXFKGZjgoU2xJQRVrY5zTvZmOxWmeLe_-Y0ubHVQaGRJfbNL66NI39kJ7p3VHYn3fqdFR4UH8kH_TkNFg</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>PROCESS FOR MANUFACTURING GRAPHITE POWDER FOR LITHIUM SECONDARY BATTERY NEGATIVE ELECTRODE MATERIAL</title><source>esp@cenet</source><creator>YAMAKI MOTOHIRO ; KUROYANAGI AKIHIRO ; KOMORIYA MAYURI ; FUKUGAWA TOMOHITO ; YAMAMOTO KAZUHIRO</creator><creatorcontrib>YAMAKI MOTOHIRO ; KUROYANAGI AKIHIRO ; KOMORIYA MAYURI ; FUKUGAWA TOMOHITO ; YAMAMOTO KAZUHIRO</creatorcontrib><description>A method for producing a graphite powder for use as a lithium secondary battery negative electrode material easily produces a graphite powder for use as a lithium secondary battery negative electrode material that has a small specific surface area while reducing the energy consumption, and achieving a high graphitization efficiency. The method includes melt-mixing a coke powder and a carbon precursor binder so that an amount of fixed carbon included in the carbon precursor binder is 5 to 15 parts by mass based on 100 parts by mass of the coke powder, to prepare a mixture, and pressing the mixture to prepare a compact, the coke powder being obtained by heating a green coke powder at 600 to 1450°C in a non-oxidizing atmosphere, the green coke powder having a cumulative particle size at 50% in a volumetric cumulative particle size distribution of 5 to 50 µm; heating the compact in a non-oxidizing atmosphere to effect carbonization and graphitization to obtain a graphitized compact; and grinding the graphitized compact.</description><language>eng ; fre ; ger</language><subject>ARTIFICIAL STONE ; BASIC ELECTRIC ELEMENTS ; CEMENTS ; CERAMICS ; CHEMISTRY ; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS ; COMPOUNDS THEREOF ; CONCRETE ; ELECTRICITY ; INORGANIC CHEMISTRY ; LIME, MAGNESIA ; METALLURGY ; NON-METALLIC ELEMENTS ; PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY ; REFRACTORIES ; SLAG ; TREATMENT OF NATURAL STONE</subject><creationdate>2016</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20160629&amp;DB=EPODOC&amp;CC=EP&amp;NR=2913873A4$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20160629&amp;DB=EPODOC&amp;CC=EP&amp;NR=2913873A4$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>YAMAKI MOTOHIRO</creatorcontrib><creatorcontrib>KUROYANAGI AKIHIRO</creatorcontrib><creatorcontrib>KOMORIYA MAYURI</creatorcontrib><creatorcontrib>FUKUGAWA TOMOHITO</creatorcontrib><creatorcontrib>YAMAMOTO KAZUHIRO</creatorcontrib><title>PROCESS FOR MANUFACTURING GRAPHITE POWDER FOR LITHIUM SECONDARY BATTERY NEGATIVE ELECTRODE MATERIAL</title><description>A method for producing a graphite powder for use as a lithium secondary battery negative electrode material easily produces a graphite powder for use as a lithium secondary battery negative electrode material that has a small specific surface area while reducing the energy consumption, and achieving a high graphitization efficiency. The method includes melt-mixing a coke powder and a carbon precursor binder so that an amount of fixed carbon included in the carbon precursor binder is 5 to 15 parts by mass based on 100 parts by mass of the coke powder, to prepare a mixture, and pressing the mixture to prepare a compact, the coke powder being obtained by heating a green coke powder at 600 to 1450°C in a non-oxidizing atmosphere, the green coke powder having a cumulative particle size at 50% in a volumetric cumulative particle size distribution of 5 to 50 µm; heating the compact in a non-oxidizing atmosphere to effect carbonization and graphitization to obtain a graphitized compact; and grinding the graphitized compact.</description><subject>ARTIFICIAL STONE</subject><subject>BASIC ELECTRIC ELEMENTS</subject><subject>CEMENTS</subject><subject>CERAMICS</subject><subject>CHEMISTRY</subject><subject>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</subject><subject>COMPOUNDS THEREOF</subject><subject>CONCRETE</subject><subject>ELECTRICITY</subject><subject>INORGANIC CHEMISTRY</subject><subject>LIME, MAGNESIA</subject><subject>METALLURGY</subject><subject>NON-METALLIC ELEMENTS</subject><subject>PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY</subject><subject>REFRACTORIES</subject><subject>SLAG</subject><subject>TREATMENT OF NATURAL STONE</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2016</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNjEEKwjAQAHvxIOof9gMeNIJ6XNNNG2iTsN1UPJVS4km0UP-PRXyApznMMMtsCOw1NQ0Yz1Cjiwa1RLaugIIxlFYIgr_mxN-islLaWEND2rsc-QYXFKGZjgoU2xJQRVrY5zTvZmOxWmeLe_-Y0ubHVQaGRJfbNL66NI39kJ7p3VHYn3fqdFR4UH8kH_TkNFg</recordid><startdate>20160629</startdate><enddate>20160629</enddate><creator>YAMAKI MOTOHIRO</creator><creator>KUROYANAGI AKIHIRO</creator><creator>KOMORIYA MAYURI</creator><creator>FUKUGAWA TOMOHITO</creator><creator>YAMAMOTO KAZUHIRO</creator><scope>EVB</scope></search><sort><creationdate>20160629</creationdate><title>PROCESS FOR MANUFACTURING GRAPHITE POWDER FOR LITHIUM SECONDARY BATTERY NEGATIVE ELECTRODE MATERIAL</title><author>YAMAKI MOTOHIRO ; KUROYANAGI AKIHIRO ; KOMORIYA MAYURI ; FUKUGAWA TOMOHITO ; YAMAMOTO KAZUHIRO</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_EP2913873A43</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; fre ; ger</language><creationdate>2016</creationdate><topic>ARTIFICIAL STONE</topic><topic>BASIC ELECTRIC ELEMENTS</topic><topic>CEMENTS</topic><topic>CERAMICS</topic><topic>CHEMISTRY</topic><topic>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</topic><topic>COMPOUNDS THEREOF</topic><topic>CONCRETE</topic><topic>ELECTRICITY</topic><topic>INORGANIC CHEMISTRY</topic><topic>LIME, MAGNESIA</topic><topic>METALLURGY</topic><topic>NON-METALLIC ELEMENTS</topic><topic>PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY</topic><topic>REFRACTORIES</topic><topic>SLAG</topic><topic>TREATMENT OF NATURAL STONE</topic><toplevel>online_resources</toplevel><creatorcontrib>YAMAKI MOTOHIRO</creatorcontrib><creatorcontrib>KUROYANAGI AKIHIRO</creatorcontrib><creatorcontrib>KOMORIYA MAYURI</creatorcontrib><creatorcontrib>FUKUGAWA TOMOHITO</creatorcontrib><creatorcontrib>YAMAMOTO KAZUHIRO</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>YAMAKI MOTOHIRO</au><au>KUROYANAGI AKIHIRO</au><au>KOMORIYA MAYURI</au><au>FUKUGAWA TOMOHITO</au><au>YAMAMOTO KAZUHIRO</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>PROCESS FOR MANUFACTURING GRAPHITE POWDER FOR LITHIUM SECONDARY BATTERY NEGATIVE ELECTRODE MATERIAL</title><date>2016-06-29</date><risdate>2016</risdate><abstract>A method for producing a graphite powder for use as a lithium secondary battery negative electrode material easily produces a graphite powder for use as a lithium secondary battery negative electrode material that has a small specific surface area while reducing the energy consumption, and achieving a high graphitization efficiency. The method includes melt-mixing a coke powder and a carbon precursor binder so that an amount of fixed carbon included in the carbon precursor binder is 5 to 15 parts by mass based on 100 parts by mass of the coke powder, to prepare a mixture, and pressing the mixture to prepare a compact, the coke powder being obtained by heating a green coke powder at 600 to 1450°C in a non-oxidizing atmosphere, the green coke powder having a cumulative particle size at 50% in a volumetric cumulative particle size distribution of 5 to 50 µm; heating the compact in a non-oxidizing atmosphere to effect carbonization and graphitization to obtain a graphitized compact; and grinding the graphitized compact.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng ; fre ; ger
recordid cdi_epo_espacenet_EP2913873A4
source esp@cenet
subjects ARTIFICIAL STONE
BASIC ELECTRIC ELEMENTS
CEMENTS
CERAMICS
CHEMISTRY
COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS
COMPOUNDS THEREOF
CONCRETE
ELECTRICITY
INORGANIC CHEMISTRY
LIME, MAGNESIA
METALLURGY
NON-METALLIC ELEMENTS
PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY
REFRACTORIES
SLAG
TREATMENT OF NATURAL STONE
title PROCESS FOR MANUFACTURING GRAPHITE POWDER FOR LITHIUM SECONDARY BATTERY NEGATIVE ELECTRODE MATERIAL
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-06T02%3A24%3A57IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=YAMAKI%20MOTOHIRO&rft.date=2016-06-29&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EEP2913873A4%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true