METHOD FOR HARDENING A DIE-CAST PART
Methods for hardening die-cast parts are known, in which firstly the die-cast part (16) is poured into a casting mould (2) having at least one fixed and one movable mould half (4, 6), then the casting mould (2) is opened by moving out the movable mould half (6), the die-cast part (16) in the movable...
Gespeichert in:
Hauptverfasser: | , , |
---|---|
Format: | Patent |
Sprache: | eng ; fre ; ger |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | REITER, ROLAND ZIEGLER, STEFFEN MÖDING, HERBERT |
description | Methods for hardening die-cast parts are known, in which firstly the die-cast part (16) is poured into a casting mould (2) having at least one fixed and one movable mould half (4, 6), then the casting mould (2) is opened by moving out the movable mould half (6), the die-cast part (16) in the movable mould half (6) is quenched, then the die-cast part (16) is ejected from the movable mould half (6) and finally, the die-cast part (16) is aged artificially. To increase the strength, according to the invention, spray tools (14) of a spraying device (8) are inserted between the mould halves (4, 6) immediately after or while the casting mould (2) is opened, with which spray tools a coolant is applied to the die-cast part (16) to quench same. |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_EP2741874A1</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>EP2741874A1</sourcerecordid><originalsourceid>FETCH-epo_espacenet_EP2741874A13</originalsourceid><addsrcrecordid>eNrjZFDxdQ3x8HdRcPMPUvBwDHJx9fP0c1dwVHDxdNV1dgwOUQhwDArhYWBNS8wpTuWF0twMCm6uIc4euqkF-fGpxQWJyal5qSXxrgFG5iaGFuYmjobGRCgBAAwQIi8</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>METHOD FOR HARDENING A DIE-CAST PART</title><source>esp@cenet</source><creator>REITER, ROLAND ; ZIEGLER, STEFFEN ; MÖDING, HERBERT</creator><creatorcontrib>REITER, ROLAND ; ZIEGLER, STEFFEN ; MÖDING, HERBERT</creatorcontrib><description>Methods for hardening die-cast parts are known, in which firstly the die-cast part (16) is poured into a casting mould (2) having at least one fixed and one movable mould half (4, 6), then the casting mould (2) is opened by moving out the movable mould half (6), the die-cast part (16) in the movable mould half (6) is quenched, then the die-cast part (16) is ejected from the movable mould half (6) and finally, the die-cast part (16) is aged artificially. To increase the strength, according to the invention, spray tools (14) of a spraying device (8) are inserted between the mould halves (4, 6) immediately after or while the casting mould (2) is opened, with which spray tools a coolant is applied to the die-cast part (16) to quench same.</description><language>eng ; fre ; ger</language><subject>CASTING ; CASTING OF METALS ; CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES ; CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS ANDNON-FERROUS ALLOYS ; CHEMISTRY ; FERROUS OR NON-FERROUS ALLOYS ; METALLURGY ; PERFORMING OPERATIONS ; POWDER METALLURGY ; TRANSPORTING ; TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><creationdate>2014</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20140618&DB=EPODOC&CC=EP&NR=2741874A1$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76289</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20140618&DB=EPODOC&CC=EP&NR=2741874A1$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>REITER, ROLAND</creatorcontrib><creatorcontrib>ZIEGLER, STEFFEN</creatorcontrib><creatorcontrib>MÖDING, HERBERT</creatorcontrib><title>METHOD FOR HARDENING A DIE-CAST PART</title><description>Methods for hardening die-cast parts are known, in which firstly the die-cast part (16) is poured into a casting mould (2) having at least one fixed and one movable mould half (4, 6), then the casting mould (2) is opened by moving out the movable mould half (6), the die-cast part (16) in the movable mould half (6) is quenched, then the die-cast part (16) is ejected from the movable mould half (6) and finally, the die-cast part (16) is aged artificially. To increase the strength, according to the invention, spray tools (14) of a spraying device (8) are inserted between the mould halves (4, 6) immediately after or while the casting mould (2) is opened, with which spray tools a coolant is applied to the die-cast part (16) to quench same.</description><subject>CASTING</subject><subject>CASTING OF METALS</subject><subject>CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES</subject><subject>CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS ANDNON-FERROUS ALLOYS</subject><subject>CHEMISTRY</subject><subject>FERROUS OR NON-FERROUS ALLOYS</subject><subject>METALLURGY</subject><subject>PERFORMING OPERATIONS</subject><subject>POWDER METALLURGY</subject><subject>TRANSPORTING</subject><subject>TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2014</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZFDxdQ3x8HdRcPMPUvBwDHJx9fP0c1dwVHDxdNV1dgwOUQhwDArhYWBNS8wpTuWF0twMCm6uIc4euqkF-fGpxQWJyal5qSXxrgFG5iaGFuYmjobGRCgBAAwQIi8</recordid><startdate>20140618</startdate><enddate>20140618</enddate><creator>REITER, ROLAND</creator><creator>ZIEGLER, STEFFEN</creator><creator>MÖDING, HERBERT</creator><scope>EVB</scope></search><sort><creationdate>20140618</creationdate><title>METHOD FOR HARDENING A DIE-CAST PART</title><author>REITER, ROLAND ; ZIEGLER, STEFFEN ; MÖDING, HERBERT</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_EP2741874A13</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; fre ; ger</language><creationdate>2014</creationdate><topic>CASTING</topic><topic>CASTING OF METALS</topic><topic>CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES</topic><topic>CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS ANDNON-FERROUS ALLOYS</topic><topic>CHEMISTRY</topic><topic>FERROUS OR NON-FERROUS ALLOYS</topic><topic>METALLURGY</topic><topic>PERFORMING OPERATIONS</topic><topic>POWDER METALLURGY</topic><topic>TRANSPORTING</topic><topic>TREATMENT OF ALLOYS OR NON-FERROUS METALS</topic><toplevel>online_resources</toplevel><creatorcontrib>REITER, ROLAND</creatorcontrib><creatorcontrib>ZIEGLER, STEFFEN</creatorcontrib><creatorcontrib>MÖDING, HERBERT</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>REITER, ROLAND</au><au>ZIEGLER, STEFFEN</au><au>MÖDING, HERBERT</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>METHOD FOR HARDENING A DIE-CAST PART</title><date>2014-06-18</date><risdate>2014</risdate><abstract>Methods for hardening die-cast parts are known, in which firstly the die-cast part (16) is poured into a casting mould (2) having at least one fixed and one movable mould half (4, 6), then the casting mould (2) is opened by moving out the movable mould half (6), the die-cast part (16) in the movable mould half (6) is quenched, then the die-cast part (16) is ejected from the movable mould half (6) and finally, the die-cast part (16) is aged artificially. To increase the strength, according to the invention, spray tools (14) of a spraying device (8) are inserted between the mould halves (4, 6) immediately after or while the casting mould (2) is opened, with which spray tools a coolant is applied to the die-cast part (16) to quench same.</abstract><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | eng ; fre ; ger |
recordid | cdi_epo_espacenet_EP2741874A1 |
source | esp@cenet |
subjects | CASTING CASTING OF METALS CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS ANDNON-FERROUS ALLOYS CHEMISTRY FERROUS OR NON-FERROUS ALLOYS METALLURGY PERFORMING OPERATIONS POWDER METALLURGY TRANSPORTING TREATMENT OF ALLOYS OR NON-FERROUS METALS |
title | METHOD FOR HARDENING A DIE-CAST PART |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-05T16%3A36%3A13IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=REITER,%20ROLAND&rft.date=2014-06-18&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EEP2741874A1%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |