A METHOD OF FORMING ALLOYS EXHIBITING SPINODAL GLASS MATRIX MICROCONSTITUENTS STRUCTURE AND DEFORMATION MECHANISMS

An alloy composition comprising iron present in the range of 49 atomic percent (at %) to 65 at %, nickel present in the range of 10.0 at % to 16.5 at %, cobalt optionally present in the range of 0.1 at % to 12 at %, boron present in the range of 12.5 at % to 16.5 at %, silicon optionally present in...