METHOD FOR TREATMENT OF CHROMIUM-CONTAINING HOT METAL AND SLAG

[Problem] To provide a means for reducing and collecting chrome from slag with simultaneously promoting desulfurization of molten iron, as directed to chrome-containing molten iron and slag to be obtained in electric furnace operation using CaF 2 -free slag. [Means for Resolution] In mechanically st...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: MORI Masakazu, YOSHINO Takahiro
Format: Patent
Sprache:eng ; fre ; ger
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator MORI Masakazu
YOSHINO Takahiro
description [Problem] To provide a means for reducing and collecting chrome from slag with simultaneously promoting desulfurization of molten iron, as directed to chrome-containing molten iron and slag to be obtained in electric furnace operation using CaF 2 -free slag. [Means for Resolution] In mechanically stirring a chrome-containing molten iron produced in an electric furnace and having a Cr content of from 8.0 to 35.0% by mass, and a CaF 2 -free electric furnace slag formed during the molten iron production, including Cr 2 O 3 , SiO 2 and CaO as the constituent components and having a basicity CaO/SiO 2 of from 0.7 to 1.7, with an impeller in a refining vessel, a metal Al-containing substance and CaO are put into the vessel before the end of stirring to thereby control the basicity of the slag after the end of stirring to at least 1.9.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_EP2554684B1</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>EP2554684B1</sourcerecordid><originalsourceid>FETCH-epo_espacenet_EP2554684B13</originalsourceid><addsrcrecordid>eNrjZLDzdQ3x8HdRcPMPUggJcnUM8XX1C1Hwd1Nw9gjy9_UM9dV19vcLcfT08_RzV_DwD1EAqnf0UXD0c1EI9nF052FgTUvMKU7lhdLcDApuriHOHrqpBfnxqcUFicmpeakl8a4BRqamJmYWJk6GxkQoAQD5HSmX</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>METHOD FOR TREATMENT OF CHROMIUM-CONTAINING HOT METAL AND SLAG</title><source>esp@cenet</source><creator>MORI Masakazu ; YOSHINO Takahiro</creator><creatorcontrib>MORI Masakazu ; YOSHINO Takahiro</creatorcontrib><description>[Problem] To provide a means for reducing and collecting chrome from slag with simultaneously promoting desulfurization of molten iron, as directed to chrome-containing molten iron and slag to be obtained in electric furnace operation using CaF 2 -free slag. [Means for Resolution] In mechanically stirring a chrome-containing molten iron produced in an electric furnace and having a Cr content of from 8.0 to 35.0% by mass, and a CaF 2 -free electric furnace slag formed during the molten iron production, including Cr 2 O 3 , SiO 2 and CaO as the constituent components and having a basicity CaO/SiO 2 of from 0.7 to 1.7, with an impeller in a refining vessel, a metal Al-containing substance and CaO are put into the vessel before the end of stirring to thereby control the basicity of the slag after the end of stirring to at least 1.9.</description><language>eng ; fre ; ger</language><subject>BLASTING ; CHEMISTRY ; DETAILS OR ACCESSORIES OF FURNACES, KILNS, OVENS, OR RETORTS,IN SO FAR AS THEY ARE OF KINDS OCCURRING IN MORE THAN ONE KINDOF FURNACE ; FURNACES ; HEATING ; KILNS ; LIGHTING ; MECHANICAL ENGINEERING ; METALLURGY ; METALLURGY OF IRON ; OVENS ; PROCESSING OF PIG-IRON, e.g. REFINING, MANUFACTURE OFWROUGHT-IRON OR STEEL ; RETORTS ; TREATMENT IN MOLTEN STATE OF FERROUS ALLOYS ; WEAPONS</subject><creationdate>2018</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20180620&amp;DB=EPODOC&amp;CC=EP&amp;NR=2554684B1$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25543,76293</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20180620&amp;DB=EPODOC&amp;CC=EP&amp;NR=2554684B1$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>MORI Masakazu</creatorcontrib><creatorcontrib>YOSHINO Takahiro</creatorcontrib><title>METHOD FOR TREATMENT OF CHROMIUM-CONTAINING HOT METAL AND SLAG</title><description>[Problem] To provide a means for reducing and collecting chrome from slag with simultaneously promoting desulfurization of molten iron, as directed to chrome-containing molten iron and slag to be obtained in electric furnace operation using CaF 2 -free slag. [Means for Resolution] In mechanically stirring a chrome-containing molten iron produced in an electric furnace and having a Cr content of from 8.0 to 35.0% by mass, and a CaF 2 -free electric furnace slag formed during the molten iron production, including Cr 2 O 3 , SiO 2 and CaO as the constituent components and having a basicity CaO/SiO 2 of from 0.7 to 1.7, with an impeller in a refining vessel, a metal Al-containing substance and CaO are put into the vessel before the end of stirring to thereby control the basicity of the slag after the end of stirring to at least 1.9.</description><subject>BLASTING</subject><subject>CHEMISTRY</subject><subject>DETAILS OR ACCESSORIES OF FURNACES, KILNS, OVENS, OR RETORTS,IN SO FAR AS THEY ARE OF KINDS OCCURRING IN MORE THAN ONE KINDOF FURNACE</subject><subject>FURNACES</subject><subject>HEATING</subject><subject>KILNS</subject><subject>LIGHTING</subject><subject>MECHANICAL ENGINEERING</subject><subject>METALLURGY</subject><subject>METALLURGY OF IRON</subject><subject>OVENS</subject><subject>PROCESSING OF PIG-IRON, e.g. REFINING, MANUFACTURE OFWROUGHT-IRON OR STEEL</subject><subject>RETORTS</subject><subject>TREATMENT IN MOLTEN STATE OF FERROUS ALLOYS</subject><subject>WEAPONS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2018</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZLDzdQ3x8HdRcPMPUggJcnUM8XX1C1Hwd1Nw9gjy9_UM9dV19vcLcfT08_RzV_DwD1EAqnf0UXD0c1EI9nF052FgTUvMKU7lhdLcDApuriHOHrqpBfnxqcUFicmpeakl8a4BRqamJmYWJk6GxkQoAQD5HSmX</recordid><startdate>20180620</startdate><enddate>20180620</enddate><creator>MORI Masakazu</creator><creator>YOSHINO Takahiro</creator><scope>EVB</scope></search><sort><creationdate>20180620</creationdate><title>METHOD FOR TREATMENT OF CHROMIUM-CONTAINING HOT METAL AND SLAG</title><author>MORI Masakazu ; YOSHINO Takahiro</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_EP2554684B13</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; fre ; ger</language><creationdate>2018</creationdate><topic>BLASTING</topic><topic>CHEMISTRY</topic><topic>DETAILS OR ACCESSORIES OF FURNACES, KILNS, OVENS, OR RETORTS,IN SO FAR AS THEY ARE OF KINDS OCCURRING IN MORE THAN ONE KINDOF FURNACE</topic><topic>FURNACES</topic><topic>HEATING</topic><topic>KILNS</topic><topic>LIGHTING</topic><topic>MECHANICAL ENGINEERING</topic><topic>METALLURGY</topic><topic>METALLURGY OF IRON</topic><topic>OVENS</topic><topic>PROCESSING OF PIG-IRON, e.g. REFINING, MANUFACTURE OFWROUGHT-IRON OR STEEL</topic><topic>RETORTS</topic><topic>TREATMENT IN MOLTEN STATE OF FERROUS ALLOYS</topic><topic>WEAPONS</topic><toplevel>online_resources</toplevel><creatorcontrib>MORI Masakazu</creatorcontrib><creatorcontrib>YOSHINO Takahiro</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>MORI Masakazu</au><au>YOSHINO Takahiro</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>METHOD FOR TREATMENT OF CHROMIUM-CONTAINING HOT METAL AND SLAG</title><date>2018-06-20</date><risdate>2018</risdate><abstract>[Problem] To provide a means for reducing and collecting chrome from slag with simultaneously promoting desulfurization of molten iron, as directed to chrome-containing molten iron and slag to be obtained in electric furnace operation using CaF 2 -free slag. [Means for Resolution] In mechanically stirring a chrome-containing molten iron produced in an electric furnace and having a Cr content of from 8.0 to 35.0% by mass, and a CaF 2 -free electric furnace slag formed during the molten iron production, including Cr 2 O 3 , SiO 2 and CaO as the constituent components and having a basicity CaO/SiO 2 of from 0.7 to 1.7, with an impeller in a refining vessel, a metal Al-containing substance and CaO are put into the vessel before the end of stirring to thereby control the basicity of the slag after the end of stirring to at least 1.9.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng ; fre ; ger
recordid cdi_epo_espacenet_EP2554684B1
source esp@cenet
subjects BLASTING
CHEMISTRY
DETAILS OR ACCESSORIES OF FURNACES, KILNS, OVENS, OR RETORTS,IN SO FAR AS THEY ARE OF KINDS OCCURRING IN MORE THAN ONE KINDOF FURNACE
FURNACES
HEATING
KILNS
LIGHTING
MECHANICAL ENGINEERING
METALLURGY
METALLURGY OF IRON
OVENS
PROCESSING OF PIG-IRON, e.g. REFINING, MANUFACTURE OFWROUGHT-IRON OR STEEL
RETORTS
TREATMENT IN MOLTEN STATE OF FERROUS ALLOYS
WEAPONS
title METHOD FOR TREATMENT OF CHROMIUM-CONTAINING HOT METAL AND SLAG
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-24T09%3A39%3A25IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=MORI%20Masakazu&rft.date=2018-06-20&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EEP2554684B1%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true