METHOD FOR PRODUCING A COATED QUARTZ GLASS COMPONENT

In a known method, a SiO2 slip layer is applied to a basic quartz glass body by means of spraying on an SiO2 slip, the slip layer is dried and sintered to form an SiO2-containing functional layer. In order to permit the reproducible production of a functional quartz glass layer, even in the case of...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: WERDECKER, Waltraud, SCHENK, Christian, SCHEICH, Gerrit
Format: Patent
Sprache:eng ; fre ; ger
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator WERDECKER, Waltraud
SCHENK, Christian
SCHEICH, Gerrit
description In a known method, a SiO2 slip layer is applied to a basic quartz glass body by means of spraying on an SiO2 slip, the slip layer is dried and sintered to form an SiO2-containing functional layer. In order to permit the reproducible production of a functional quartz glass layer, even in the case of surfaces that are curved or inclined with respect to the vertical, having high layer thicknesses which satisfy high requirements on the layer homogeneity, the invention proposes that the slip contain the following components in a dispersion liquid: splintery, amorphous SiO2 granules having a gain size distribution having a D50 value in the range of 3 μm to 30 μm and having a proportion by weight of at least 10% by weight, based on the total solids content; spherical, amorphous SiO2 particles having a particle size distribution having a D50 value in the range of 1 μm to 50 μm and having a proportion by weight of at least 30% by weight, based on the total solids content; SiO2 nano particles having particle sizes of less than 100 nm and having a proportion by weight between 0.2% and 10% by weight, based on the total solids content; and a non-ionic, alkali-free surfactant having a proportion in the range of 0.005 to 0.5%, based on the volume of the dispersion liquid.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_EP2485988B1</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>EP2485988B1</sourcerecordid><originalsourceid>FETCH-epo_espacenet_EP2485988B13</originalsourceid><addsrcrecordid>eNrjZDDxdQ3x8HdRcPMPUggI8ncJdfb0c1dwVHD2dwxxdVEIDHUMColScPdxDA4GivkG-Pu5-oXwMLCmJeYUp_JCaW4GBTfXEGcP3dSC_PjU4oLE5NS81JJ41wAjEwtTSwsLJ0NjIpQAAHXoJxU</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>METHOD FOR PRODUCING A COATED QUARTZ GLASS COMPONENT</title><source>esp@cenet</source><creator>WERDECKER, Waltraud ; SCHENK, Christian ; SCHEICH, Gerrit</creator><creatorcontrib>WERDECKER, Waltraud ; SCHENK, Christian ; SCHEICH, Gerrit</creatorcontrib><description>In a known method, a SiO2 slip layer is applied to a basic quartz glass body by means of spraying on an SiO2 slip, the slip layer is dried and sintered to form an SiO2-containing functional layer. In order to permit the reproducible production of a functional quartz glass layer, even in the case of surfaces that are curved or inclined with respect to the vertical, having high layer thicknesses which satisfy high requirements on the layer homogeneity, the invention proposes that the slip contain the following components in a dispersion liquid: splintery, amorphous SiO2 granules having a gain size distribution having a D50 value in the range of 3 μm to 30 μm and having a proportion by weight of at least 10% by weight, based on the total solids content; spherical, amorphous SiO2 particles having a particle size distribution having a D50 value in the range of 1 μm to 50 μm and having a proportion by weight of at least 30% by weight, based on the total solids content; SiO2 nano particles having particle sizes of less than 100 nm and having a proportion by weight between 0.2% and 10% by weight, based on the total solids content; and a non-ionic, alkali-free surfactant having a proportion in the range of 0.005 to 0.5%, based on the volume of the dispersion liquid.</description><language>eng ; fre ; ger</language><subject>CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS ; CHEMISTRY ; GLASS ; JOINING GLASS TO GLASS OR OTHER MATERIALS ; MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES ; METALLURGY ; MINERAL OR SLAG WOOL ; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS ; SURFACE TREATMENT OF GLASS</subject><creationdate>2017</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20170809&amp;DB=EPODOC&amp;CC=EP&amp;NR=2485988B1$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20170809&amp;DB=EPODOC&amp;CC=EP&amp;NR=2485988B1$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>WERDECKER, Waltraud</creatorcontrib><creatorcontrib>SCHENK, Christian</creatorcontrib><creatorcontrib>SCHEICH, Gerrit</creatorcontrib><title>METHOD FOR PRODUCING A COATED QUARTZ GLASS COMPONENT</title><description>In a known method, a SiO2 slip layer is applied to a basic quartz glass body by means of spraying on an SiO2 slip, the slip layer is dried and sintered to form an SiO2-containing functional layer. In order to permit the reproducible production of a functional quartz glass layer, even in the case of surfaces that are curved or inclined with respect to the vertical, having high layer thicknesses which satisfy high requirements on the layer homogeneity, the invention proposes that the slip contain the following components in a dispersion liquid: splintery, amorphous SiO2 granules having a gain size distribution having a D50 value in the range of 3 μm to 30 μm and having a proportion by weight of at least 10% by weight, based on the total solids content; spherical, amorphous SiO2 particles having a particle size distribution having a D50 value in the range of 1 μm to 50 μm and having a proportion by weight of at least 30% by weight, based on the total solids content; SiO2 nano particles having particle sizes of less than 100 nm and having a proportion by weight between 0.2% and 10% by weight, based on the total solids content; and a non-ionic, alkali-free surfactant having a proportion in the range of 0.005 to 0.5%, based on the volume of the dispersion liquid.</description><subject>CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS</subject><subject>CHEMISTRY</subject><subject>GLASS</subject><subject>JOINING GLASS TO GLASS OR OTHER MATERIALS</subject><subject>MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES</subject><subject>METALLURGY</subject><subject>MINERAL OR SLAG WOOL</subject><subject>SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS</subject><subject>SURFACE TREATMENT OF GLASS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2017</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZDDxdQ3x8HdRcPMPUggI8ncJdfb0c1dwVHD2dwxxdVEIDHUMColScPdxDA4GivkG-Pu5-oXwMLCmJeYUp_JCaW4GBTfXEGcP3dSC_PjU4oLE5NS81JJ41wAjEwtTSwsLJ0NjIpQAAHXoJxU</recordid><startdate>20170809</startdate><enddate>20170809</enddate><creator>WERDECKER, Waltraud</creator><creator>SCHENK, Christian</creator><creator>SCHEICH, Gerrit</creator><scope>EVB</scope></search><sort><creationdate>20170809</creationdate><title>METHOD FOR PRODUCING A COATED QUARTZ GLASS COMPONENT</title><author>WERDECKER, Waltraud ; SCHENK, Christian ; SCHEICH, Gerrit</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_EP2485988B13</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; fre ; ger</language><creationdate>2017</creationdate><topic>CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS</topic><topic>CHEMISTRY</topic><topic>GLASS</topic><topic>JOINING GLASS TO GLASS OR OTHER MATERIALS</topic><topic>MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES</topic><topic>METALLURGY</topic><topic>MINERAL OR SLAG WOOL</topic><topic>SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS</topic><topic>SURFACE TREATMENT OF GLASS</topic><toplevel>online_resources</toplevel><creatorcontrib>WERDECKER, Waltraud</creatorcontrib><creatorcontrib>SCHENK, Christian</creatorcontrib><creatorcontrib>SCHEICH, Gerrit</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>WERDECKER, Waltraud</au><au>SCHENK, Christian</au><au>SCHEICH, Gerrit</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>METHOD FOR PRODUCING A COATED QUARTZ GLASS COMPONENT</title><date>2017-08-09</date><risdate>2017</risdate><abstract>In a known method, a SiO2 slip layer is applied to a basic quartz glass body by means of spraying on an SiO2 slip, the slip layer is dried and sintered to form an SiO2-containing functional layer. In order to permit the reproducible production of a functional quartz glass layer, even in the case of surfaces that are curved or inclined with respect to the vertical, having high layer thicknesses which satisfy high requirements on the layer homogeneity, the invention proposes that the slip contain the following components in a dispersion liquid: splintery, amorphous SiO2 granules having a gain size distribution having a D50 value in the range of 3 μm to 30 μm and having a proportion by weight of at least 10% by weight, based on the total solids content; spherical, amorphous SiO2 particles having a particle size distribution having a D50 value in the range of 1 μm to 50 μm and having a proportion by weight of at least 30% by weight, based on the total solids content; SiO2 nano particles having particle sizes of less than 100 nm and having a proportion by weight between 0.2% and 10% by weight, based on the total solids content; and a non-ionic, alkali-free surfactant having a proportion in the range of 0.005 to 0.5%, based on the volume of the dispersion liquid.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng ; fre ; ger
recordid cdi_epo_espacenet_EP2485988B1
source esp@cenet
subjects CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS
CHEMISTRY
GLASS
JOINING GLASS TO GLASS OR OTHER MATERIALS
MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES
METALLURGY
MINERAL OR SLAG WOOL
SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS
SURFACE TREATMENT OF GLASS
title METHOD FOR PRODUCING A COATED QUARTZ GLASS COMPONENT
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-03T19%3A38%3A58IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=WERDECKER,%20Waltraud&rft.date=2017-08-09&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EEP2485988B1%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true