METHOD FOR MANUFACTURING AN OPTICAL ARTICLE WITH ANTI-GLARE PROPERTIES

The present invention relates to a method for making an optical article with anti-reflection properties, comprising the steps of: a) forming on at least one main surface of a support, by applying a sol comprising at least one colloidal mineral oxide with a refractive index higher than or equal to 1....

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: KELLER, GERHARD, VANEECKHOUTTE, PHILIPPE, CRETIER, ANNETTE
Format: Patent
Sprache:eng ; fre ; ger
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator KELLER, GERHARD
VANEECKHOUTTE, PHILIPPE
CRETIER, ANNETTE
description The present invention relates to a method for making an optical article with anti-reflection properties, comprising the steps of: a) forming on at least one main surface of a support, by applying a sol comprising at least one colloidal mineral oxide with a refractive index higher than or equal to 1.80 having an initial porosity; b) optionally, forming on the first lower layer by applying a sol comprising at least one colloidal mineral oxide with a refractive index lower than 1.65 a second lower layer having an initial porosity at least equal to the initial porosity of said first layer; c) applying onto the one or more lower layer(s) an upper layer composition of an optically transparent polymer material with a refractive index lower than or equal to 1.50; d) filling the porosity of the one or more lower layer(s) through penetration into the one or more lower layer(s) of at least part of the material of the upper layer composition formed in step (c) and forming a cured upper layer which thickness is determined so that the upper layer and the one or more lower layer(s), once the initial porosity thereof has been filled, form a bilayered anti-reflection coating, within the range of from 400 to 700 nm, preferably of from 450 to 650 nm.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_EP2368146B1</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>EP2368146B1</sourcerecordid><originalsourceid>FETCH-epo_espacenet_EP2368146B13</originalsourceid><addsrcrecordid>eNrjZHDzdQ3x8HdRcPMPUvB19At1c3QOCQ3y9HNXcPRT8A8I8XR29FFwDALSPq4K4Z4hHkDxEE9ddx_HIFeFgCD_AFegnGswDwNrWmJOcSovlOZmUHBzDXH20E0tyI9PLS5ITE7NSy2Jdw0wMjazMDQxczI0JkIJAFsPK_s</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>METHOD FOR MANUFACTURING AN OPTICAL ARTICLE WITH ANTI-GLARE PROPERTIES</title><source>esp@cenet</source><creator>KELLER, GERHARD ; VANEECKHOUTTE, PHILIPPE ; CRETIER, ANNETTE</creator><creatorcontrib>KELLER, GERHARD ; VANEECKHOUTTE, PHILIPPE ; CRETIER, ANNETTE</creatorcontrib><description>The present invention relates to a method for making an optical article with anti-reflection properties, comprising the steps of: a) forming on at least one main surface of a support, by applying a sol comprising at least one colloidal mineral oxide with a refractive index higher than or equal to 1.80 having an initial porosity; b) optionally, forming on the first lower layer by applying a sol comprising at least one colloidal mineral oxide with a refractive index lower than 1.65 a second lower layer having an initial porosity at least equal to the initial porosity of said first layer; c) applying onto the one or more lower layer(s) an upper layer composition of an optically transparent polymer material with a refractive index lower than or equal to 1.50; d) filling the porosity of the one or more lower layer(s) through penetration into the one or more lower layer(s) of at least part of the material of the upper layer composition formed in step (c) and forming a cured upper layer which thickness is determined so that the upper layer and the one or more lower layer(s), once the initial porosity thereof has been filled, form a bilayered anti-reflection coating, within the range of from 400 to 700 nm, preferably of from 450 to 650 nm.</description><language>eng ; fre ; ger</language><subject>AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F,C08G ; CHEMISTRY ; COMPOSITIONS BASED THEREON ; CONTACT LENSES ; GENERAL PROCESSES OF COMPOUNDING ; METALLURGY ; OPTICAL ELEMENTS, SYSTEMS, OR APPARATUS ; OPTICS ; ORGANIC MACROMOLECULAR COMPOUNDS ; PHYSICS ; SPECTACLES ; SUNGLASSES OR GOGGLES INSOFAR AS THEY HAVE THE SAME FEATURESAS SPECTACLES ; THEIR PREPARATION OR CHEMICAL WORKING-UP ; WORKING-UP</subject><creationdate>2016</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20160810&amp;DB=EPODOC&amp;CC=EP&amp;NR=2368146B1$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76289</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20160810&amp;DB=EPODOC&amp;CC=EP&amp;NR=2368146B1$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>KELLER, GERHARD</creatorcontrib><creatorcontrib>VANEECKHOUTTE, PHILIPPE</creatorcontrib><creatorcontrib>CRETIER, ANNETTE</creatorcontrib><title>METHOD FOR MANUFACTURING AN OPTICAL ARTICLE WITH ANTI-GLARE PROPERTIES</title><description>The present invention relates to a method for making an optical article with anti-reflection properties, comprising the steps of: a) forming on at least one main surface of a support, by applying a sol comprising at least one colloidal mineral oxide with a refractive index higher than or equal to 1.80 having an initial porosity; b) optionally, forming on the first lower layer by applying a sol comprising at least one colloidal mineral oxide with a refractive index lower than 1.65 a second lower layer having an initial porosity at least equal to the initial porosity of said first layer; c) applying onto the one or more lower layer(s) an upper layer composition of an optically transparent polymer material with a refractive index lower than or equal to 1.50; d) filling the porosity of the one or more lower layer(s) through penetration into the one or more lower layer(s) of at least part of the material of the upper layer composition formed in step (c) and forming a cured upper layer which thickness is determined so that the upper layer and the one or more lower layer(s), once the initial porosity thereof has been filled, form a bilayered anti-reflection coating, within the range of from 400 to 700 nm, preferably of from 450 to 650 nm.</description><subject>AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F,C08G</subject><subject>CHEMISTRY</subject><subject>COMPOSITIONS BASED THEREON</subject><subject>CONTACT LENSES</subject><subject>GENERAL PROCESSES OF COMPOUNDING</subject><subject>METALLURGY</subject><subject>OPTICAL ELEMENTS, SYSTEMS, OR APPARATUS</subject><subject>OPTICS</subject><subject>ORGANIC MACROMOLECULAR COMPOUNDS</subject><subject>PHYSICS</subject><subject>SPECTACLES</subject><subject>SUNGLASSES OR GOGGLES INSOFAR AS THEY HAVE THE SAME FEATURESAS SPECTACLES</subject><subject>THEIR PREPARATION OR CHEMICAL WORKING-UP</subject><subject>WORKING-UP</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2016</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZHDzdQ3x8HdRcPMPUvB19At1c3QOCQ3y9HNXcPRT8A8I8XR29FFwDALSPq4K4Z4hHkDxEE9ddx_HIFeFgCD_AFegnGswDwNrWmJOcSovlOZmUHBzDXH20E0tyI9PLS5ITE7NSy2Jdw0wMjazMDQxczI0JkIJAFsPK_s</recordid><startdate>20160810</startdate><enddate>20160810</enddate><creator>KELLER, GERHARD</creator><creator>VANEECKHOUTTE, PHILIPPE</creator><creator>CRETIER, ANNETTE</creator><scope>EVB</scope></search><sort><creationdate>20160810</creationdate><title>METHOD FOR MANUFACTURING AN OPTICAL ARTICLE WITH ANTI-GLARE PROPERTIES</title><author>KELLER, GERHARD ; VANEECKHOUTTE, PHILIPPE ; CRETIER, ANNETTE</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_EP2368146B13</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; fre ; ger</language><creationdate>2016</creationdate><topic>AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F,C08G</topic><topic>CHEMISTRY</topic><topic>COMPOSITIONS BASED THEREON</topic><topic>CONTACT LENSES</topic><topic>GENERAL PROCESSES OF COMPOUNDING</topic><topic>METALLURGY</topic><topic>OPTICAL ELEMENTS, SYSTEMS, OR APPARATUS</topic><topic>OPTICS</topic><topic>ORGANIC MACROMOLECULAR COMPOUNDS</topic><topic>PHYSICS</topic><topic>SPECTACLES</topic><topic>SUNGLASSES OR GOGGLES INSOFAR AS THEY HAVE THE SAME FEATURESAS SPECTACLES</topic><topic>THEIR PREPARATION OR CHEMICAL WORKING-UP</topic><topic>WORKING-UP</topic><toplevel>online_resources</toplevel><creatorcontrib>KELLER, GERHARD</creatorcontrib><creatorcontrib>VANEECKHOUTTE, PHILIPPE</creatorcontrib><creatorcontrib>CRETIER, ANNETTE</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>KELLER, GERHARD</au><au>VANEECKHOUTTE, PHILIPPE</au><au>CRETIER, ANNETTE</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>METHOD FOR MANUFACTURING AN OPTICAL ARTICLE WITH ANTI-GLARE PROPERTIES</title><date>2016-08-10</date><risdate>2016</risdate><abstract>The present invention relates to a method for making an optical article with anti-reflection properties, comprising the steps of: a) forming on at least one main surface of a support, by applying a sol comprising at least one colloidal mineral oxide with a refractive index higher than or equal to 1.80 having an initial porosity; b) optionally, forming on the first lower layer by applying a sol comprising at least one colloidal mineral oxide with a refractive index lower than 1.65 a second lower layer having an initial porosity at least equal to the initial porosity of said first layer; c) applying onto the one or more lower layer(s) an upper layer composition of an optically transparent polymer material with a refractive index lower than or equal to 1.50; d) filling the porosity of the one or more lower layer(s) through penetration into the one or more lower layer(s) of at least part of the material of the upper layer composition formed in step (c) and forming a cured upper layer which thickness is determined so that the upper layer and the one or more lower layer(s), once the initial porosity thereof has been filled, form a bilayered anti-reflection coating, within the range of from 400 to 700 nm, preferably of from 450 to 650 nm.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng ; fre ; ger
recordid cdi_epo_espacenet_EP2368146B1
source esp@cenet
subjects AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F,C08G
CHEMISTRY
COMPOSITIONS BASED THEREON
CONTACT LENSES
GENERAL PROCESSES OF COMPOUNDING
METALLURGY
OPTICAL ELEMENTS, SYSTEMS, OR APPARATUS
OPTICS
ORGANIC MACROMOLECULAR COMPOUNDS
PHYSICS
SPECTACLES
SUNGLASSES OR GOGGLES INSOFAR AS THEY HAVE THE SAME FEATURESAS SPECTACLES
THEIR PREPARATION OR CHEMICAL WORKING-UP
WORKING-UP
title METHOD FOR MANUFACTURING AN OPTICAL ARTICLE WITH ANTI-GLARE PROPERTIES
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-11T16%3A03%3A20IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=KELLER,%20GERHARD&rft.date=2016-08-10&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EEP2368146B1%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true