SELF-FLUXING PELLETS FOR USE IN A BLAST FURNACE AND PROCESS FOR THE PRODUCTION OF THE SAME

Provided are self-fluxing pellets for a blast furnace, characterized in that a CaO/SiO 2 weight ratio C/S is 0.8 or more and a MgO/SiO 2 weight ratio M/S is 0.4 or more; when the iron content (weight %) in the entire pellet is represented by %TFe, %TFe is 65% or less; and the temperature Ts (unit: °...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: HASEGAWA, NOBUHIRO, YASUDA, EISAKU, KITAYAMA, SHUJI, MATSUI, YOSHIYUKI
Format: Patent
Sprache:eng ; fre ; ger
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator HASEGAWA, NOBUHIRO
YASUDA, EISAKU
KITAYAMA, SHUJI
MATSUI, YOSHIYUKI
description Provided are self-fluxing pellets for a blast furnace, characterized in that a CaO/SiO 2 weight ratio C/S is 0.8 or more and a MgO/SiO 2 weight ratio M/S is 0.4 or more; when the iron content (weight %) in the entire pellet is represented by %TFe, %TFe is 65% or less; and the temperature Ts (unit: °C) at which the pressure loss starts to increase sharply in a loaded high-temperature reduction test, and which is calculated by the equation below, is 1290°C or higher: Equation : Ts = 110 × C / S + 100 × M / S + 25 × % TFe - 480
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_EP2239344A1</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>EP2239344A1</sourcerecordid><originalsourceid>FETCH-epo_espacenet_EP2239344A13</originalsourceid><addsrcrecordid>eNqNiksKwjAQQLtxIeod5gJd2HTjckxnbCAmIZOAuClF4kq0UO-P-DmAq8d7vGV1FrJcs80n4w4QyFpKAuwjZCEwDhD2FiUB5-hQE6DrIESvSb5b6untXdbJeAeeP0XwSOtqcR1vc9n8uKqAKem-LtNjKPM0Xsq9PAcKTaN2qm1xq_5YXqy_MM8</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>SELF-FLUXING PELLETS FOR USE IN A BLAST FURNACE AND PROCESS FOR THE PRODUCTION OF THE SAME</title><source>esp@cenet</source><creator>HASEGAWA, NOBUHIRO ; YASUDA, EISAKU ; KITAYAMA, SHUJI ; MATSUI, YOSHIYUKI</creator><creatorcontrib>HASEGAWA, NOBUHIRO ; YASUDA, EISAKU ; KITAYAMA, SHUJI ; MATSUI, YOSHIYUKI</creatorcontrib><description>Provided are self-fluxing pellets for a blast furnace, characterized in that a CaO/SiO 2 weight ratio C/S is 0.8 or more and a MgO/SiO 2 weight ratio M/S is 0.4 or more; when the iron content (weight %) in the entire pellet is represented by %TFe, %TFe is 65% or less; and the temperature Ts (unit: °C) at which the pressure loss starts to increase sharply in a loaded high-temperature reduction test, and which is calculated by the equation below, is 1290°C or higher: Equation : Ts = 110 × C / S + 100 × M / S + 25 × % TFe - 480</description><language>eng ; fre ; ger</language><subject>CHEMISTRY ; FERROUS OR NON-FERROUS ALLOYS ; MANUFACTURE OF IRON OR STEEL ; METALLURGY ; METALLURGY OF IRON ; PRETREATMENT OF RAW MATERIALS ; PRODUCTION AND REFINING OF METALS ; TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><creationdate>2010</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20101013&amp;DB=EPODOC&amp;CC=EP&amp;NR=2239344A1$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20101013&amp;DB=EPODOC&amp;CC=EP&amp;NR=2239344A1$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>HASEGAWA, NOBUHIRO</creatorcontrib><creatorcontrib>YASUDA, EISAKU</creatorcontrib><creatorcontrib>KITAYAMA, SHUJI</creatorcontrib><creatorcontrib>MATSUI, YOSHIYUKI</creatorcontrib><title>SELF-FLUXING PELLETS FOR USE IN A BLAST FURNACE AND PROCESS FOR THE PRODUCTION OF THE SAME</title><description>Provided are self-fluxing pellets for a blast furnace, characterized in that a CaO/SiO 2 weight ratio C/S is 0.8 or more and a MgO/SiO 2 weight ratio M/S is 0.4 or more; when the iron content (weight %) in the entire pellet is represented by %TFe, %TFe is 65% or less; and the temperature Ts (unit: °C) at which the pressure loss starts to increase sharply in a loaded high-temperature reduction test, and which is calculated by the equation below, is 1290°C or higher: Equation : Ts = 110 × C / S + 100 × M / S + 25 × % TFe - 480</description><subject>CHEMISTRY</subject><subject>FERROUS OR NON-FERROUS ALLOYS</subject><subject>MANUFACTURE OF IRON OR STEEL</subject><subject>METALLURGY</subject><subject>METALLURGY OF IRON</subject><subject>PRETREATMENT OF RAW MATERIALS</subject><subject>PRODUCTION AND REFINING OF METALS</subject><subject>TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2010</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNiksKwjAQQLtxIeod5gJd2HTjckxnbCAmIZOAuClF4kq0UO-P-DmAq8d7vGV1FrJcs80n4w4QyFpKAuwjZCEwDhD2FiUB5-hQE6DrIESvSb5b6untXdbJeAeeP0XwSOtqcR1vc9n8uKqAKem-LtNjKPM0Xsq9PAcKTaN2qm1xq_5YXqy_MM8</recordid><startdate>20101013</startdate><enddate>20101013</enddate><creator>HASEGAWA, NOBUHIRO</creator><creator>YASUDA, EISAKU</creator><creator>KITAYAMA, SHUJI</creator><creator>MATSUI, YOSHIYUKI</creator><scope>EVB</scope></search><sort><creationdate>20101013</creationdate><title>SELF-FLUXING PELLETS FOR USE IN A BLAST FURNACE AND PROCESS FOR THE PRODUCTION OF THE SAME</title><author>HASEGAWA, NOBUHIRO ; YASUDA, EISAKU ; KITAYAMA, SHUJI ; MATSUI, YOSHIYUKI</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_EP2239344A13</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; fre ; ger</language><creationdate>2010</creationdate><topic>CHEMISTRY</topic><topic>FERROUS OR NON-FERROUS ALLOYS</topic><topic>MANUFACTURE OF IRON OR STEEL</topic><topic>METALLURGY</topic><topic>METALLURGY OF IRON</topic><topic>PRETREATMENT OF RAW MATERIALS</topic><topic>PRODUCTION AND REFINING OF METALS</topic><topic>TREATMENT OF ALLOYS OR NON-FERROUS METALS</topic><toplevel>online_resources</toplevel><creatorcontrib>HASEGAWA, NOBUHIRO</creatorcontrib><creatorcontrib>YASUDA, EISAKU</creatorcontrib><creatorcontrib>KITAYAMA, SHUJI</creatorcontrib><creatorcontrib>MATSUI, YOSHIYUKI</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>HASEGAWA, NOBUHIRO</au><au>YASUDA, EISAKU</au><au>KITAYAMA, SHUJI</au><au>MATSUI, YOSHIYUKI</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>SELF-FLUXING PELLETS FOR USE IN A BLAST FURNACE AND PROCESS FOR THE PRODUCTION OF THE SAME</title><date>2010-10-13</date><risdate>2010</risdate><abstract>Provided are self-fluxing pellets for a blast furnace, characterized in that a CaO/SiO 2 weight ratio C/S is 0.8 or more and a MgO/SiO 2 weight ratio M/S is 0.4 or more; when the iron content (weight %) in the entire pellet is represented by %TFe, %TFe is 65% or less; and the temperature Ts (unit: °C) at which the pressure loss starts to increase sharply in a loaded high-temperature reduction test, and which is calculated by the equation below, is 1290°C or higher: Equation : Ts = 110 × C / S + 100 × M / S + 25 × % TFe - 480</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng ; fre ; ger
recordid cdi_epo_espacenet_EP2239344A1
source esp@cenet
subjects CHEMISTRY
FERROUS OR NON-FERROUS ALLOYS
MANUFACTURE OF IRON OR STEEL
METALLURGY
METALLURGY OF IRON
PRETREATMENT OF RAW MATERIALS
PRODUCTION AND REFINING OF METALS
TREATMENT OF ALLOYS OR NON-FERROUS METALS
title SELF-FLUXING PELLETS FOR USE IN A BLAST FURNACE AND PROCESS FOR THE PRODUCTION OF THE SAME
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-26T14%3A36%3A11IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=HASEGAWA,%20NOBUHIRO&rft.date=2010-10-13&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EEP2239344A1%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true