Self-adhesive air cushion film as protection for fresh varnishes during vehicle assembly and manufacturing method
The self-adhesive air cushion film (5) comprises a first carrier film (1), on whose first side an external film made of polypropylene, polypropylene-dominated polyolefin blends or propylene-dominated olefin copolymers is applied and on whose second side a second bubble-forming carrier film (2) is pr...
Gespeichert in:
1. Verfasser: | |
---|---|
Format: | Patent |
Sprache: | eng ; fre ; ger |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | BOEHM, NICOLAI |
description | The self-adhesive air cushion film (5) comprises a first carrier film (1), on whose first side an external film made of polypropylene, polypropylene-dominated polyolefin blends or propylene-dominated olefin copolymers is applied and on whose second side a second bubble-forming carrier film (2) is present, where the second side is opposite to the first side. The bubbles are filled with air. A polyethylene sheet (3a) is inseparably and partially applied to the bubbles. A self-adhesive layer is applied to the polyethylene sheet. The external film made of polypropylene has a sealing layer. The self-adhesive air cushion film (5) comprises a first carrier film (1), on whose first side an external film made of polypropylene, polypropylene-dominated polyolefin blends or propylene-dominated olefin copolymers is applied and on whose second side a second bubble-forming carrier film (2) is present, where the second side is opposite to the first side. The bubbles are filled with air. A polyethylene sheet (3a) is inseparably and partially applied to the bubbles. A self-adhesive layer is applied to the polyethylene sheet. The external film made of polypropylene has a sealing layer that is made of polyethylene or modified polyethylene towards the first carrier film. The external film made of polypropylene contains 50 wt.% of polypropylene if it consists of a blend of polyolefins, 50 mol.% of propylene if it is olefin copolymers, and 50 mol.% of propylene if it a blend of olefin copolymers or olefin copolymers and olefin-homopolymers. The external film and the sealing layer are produced by coextrusion. An adhesion promoter layer (3b) is present between the sheet and the self-adhesive layer. The external film, the first carrier film, the second carrier film and/or the sheet contain a light stabilizer in an amount of 0.15 wt.% and/or titanium dioxide in an amount of 5-15 wt.%. The first and/or second carrier film has a three-layer construction made of polyethylene sheet/barrier layer/polyethylene sheet. The self-adhesive compound is composed of polyethylene-vinyl acetate at a vinyl acetate content of 70 wt.%, and has a loss angle tan delta of 0.6-1.0 measured at a temperature of 60[deg] C and a frequency of 10 -> 2> Hz and tan delta of 0.4-0.7 measured at a temperature of 60[deg] C and a frequency of 10 Hz. The self-adhesive layer is mixed with additives such as tackifiers, plasticizers, organic or inorganic fillers, pigments, light stabilizers in the form of UV-absorbing st |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_EP2154218A3</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>EP2154218A3</sourcerecordid><originalsourceid>FETCH-epo_espacenet_EP2154218A33</originalsourceid><addsrcrecordid>eNqNjD0KwkAQRtNYiHqHuUCKJAq2IhFLQfsw7s66A_vnzibg7Q3qAawefLzvLavnlZypUVsSngiQM6hRLMcAhp0HFEg5FlLlM8UMJpNYmDAHlvkFeswcHjCRZeXmggj5u3sBBg0ew2hQla_iqdio19XCoBPa_Liq4NTfjueaUhxIEioKVIb-0ja7bdvsD133h_IGTL9DzQ</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Self-adhesive air cushion film as protection for fresh varnishes during vehicle assembly and manufacturing method</title><source>esp@cenet</source><creator>BOEHM, NICOLAI</creator><creatorcontrib>BOEHM, NICOLAI</creatorcontrib><description>The self-adhesive air cushion film (5) comprises a first carrier film (1), on whose first side an external film made of polypropylene, polypropylene-dominated polyolefin blends or propylene-dominated olefin copolymers is applied and on whose second side a second bubble-forming carrier film (2) is present, where the second side is opposite to the first side. The bubbles are filled with air. A polyethylene sheet (3a) is inseparably and partially applied to the bubbles. A self-adhesive layer is applied to the polyethylene sheet. The external film made of polypropylene has a sealing layer. The self-adhesive air cushion film (5) comprises a first carrier film (1), on whose first side an external film made of polypropylene, polypropylene-dominated polyolefin blends or propylene-dominated olefin copolymers is applied and on whose second side a second bubble-forming carrier film (2) is present, where the second side is opposite to the first side. The bubbles are filled with air. A polyethylene sheet (3a) is inseparably and partially applied to the bubbles. A self-adhesive layer is applied to the polyethylene sheet. The external film made of polypropylene has a sealing layer that is made of polyethylene or modified polyethylene towards the first carrier film. The external film made of polypropylene contains 50 wt.% of polypropylene if it consists of a blend of polyolefins, 50 mol.% of propylene if it is olefin copolymers, and 50 mol.% of propylene if it a blend of olefin copolymers or olefin copolymers and olefin-homopolymers. The external film and the sealing layer are produced by coextrusion. An adhesion promoter layer (3b) is present between the sheet and the self-adhesive layer. The external film, the first carrier film, the second carrier film and/or the sheet contain a light stabilizer in an amount of 0.15 wt.% and/or titanium dioxide in an amount of 5-15 wt.%. The first and/or second carrier film has a three-layer construction made of polyethylene sheet/barrier layer/polyethylene sheet. The self-adhesive compound is composed of polyethylene-vinyl acetate at a vinyl acetate content of 70 wt.%, and has a loss angle tan delta of 0.6-1.0 measured at a temperature of 60[deg] C and a frequency of 10 -> 2> Hz and tan delta of 0.4-0.7 measured at a temperature of 60[deg] C and a frequency of 10 Hz. The self-adhesive layer is mixed with additives such as tackifiers, plasticizers, organic or inorganic fillers, pigments, light stabilizers in the form of UV-absorbing sterically hindered amines (HALS), aging inhibitors in the form of lactones, primary and secondary antioxidants, cross-linking agents and/or cross-linking promoters. The self-adhesive air cushion film is perforated in uniform intervals transverse to the longitudinal direction. An independent claim is included for a process for producing a self-adhesive air cushion film.</description><language>eng ; fre ; ger</language><subject>ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE ; ADHESIVES ; CHEMISTRY ; DYES ; LAYERED PRODUCTS ; LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT ORNON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM ; METALLURGY ; MISCELLANEOUS APPLICATIONS OF MATERIALS ; MISCELLANEOUS COMPOSITIONS ; NATURAL RESINS ; NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL ; PAINTS ; PERFORMING OPERATIONS ; POLISHES ; TRANSPORTING ; USE OF MATERIALS AS ADHESIVES</subject><creationdate>2014</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20140312&DB=EPODOC&CC=EP&NR=2154218A3$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,309,781,886,25566,76549</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20140312&DB=EPODOC&CC=EP&NR=2154218A3$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>BOEHM, NICOLAI</creatorcontrib><title>Self-adhesive air cushion film as protection for fresh varnishes during vehicle assembly and manufacturing method</title><description>The self-adhesive air cushion film (5) comprises a first carrier film (1), on whose first side an external film made of polypropylene, polypropylene-dominated polyolefin blends or propylene-dominated olefin copolymers is applied and on whose second side a second bubble-forming carrier film (2) is present, where the second side is opposite to the first side. The bubbles are filled with air. A polyethylene sheet (3a) is inseparably and partially applied to the bubbles. A self-adhesive layer is applied to the polyethylene sheet. The external film made of polypropylene has a sealing layer. The self-adhesive air cushion film (5) comprises a first carrier film (1), on whose first side an external film made of polypropylene, polypropylene-dominated polyolefin blends or propylene-dominated olefin copolymers is applied and on whose second side a second bubble-forming carrier film (2) is present, where the second side is opposite to the first side. The bubbles are filled with air. A polyethylene sheet (3a) is inseparably and partially applied to the bubbles. A self-adhesive layer is applied to the polyethylene sheet. The external film made of polypropylene has a sealing layer that is made of polyethylene or modified polyethylene towards the first carrier film. The external film made of polypropylene contains 50 wt.% of polypropylene if it consists of a blend of polyolefins, 50 mol.% of propylene if it is olefin copolymers, and 50 mol.% of propylene if it a blend of olefin copolymers or olefin copolymers and olefin-homopolymers. The external film and the sealing layer are produced by coextrusion. An adhesion promoter layer (3b) is present between the sheet and the self-adhesive layer. The external film, the first carrier film, the second carrier film and/or the sheet contain a light stabilizer in an amount of 0.15 wt.% and/or titanium dioxide in an amount of 5-15 wt.%. The first and/or second carrier film has a three-layer construction made of polyethylene sheet/barrier layer/polyethylene sheet. The self-adhesive compound is composed of polyethylene-vinyl acetate at a vinyl acetate content of 70 wt.%, and has a loss angle tan delta of 0.6-1.0 measured at a temperature of 60[deg] C and a frequency of 10 -> 2> Hz and tan delta of 0.4-0.7 measured at a temperature of 60[deg] C and a frequency of 10 Hz. The self-adhesive layer is mixed with additives such as tackifiers, plasticizers, organic or inorganic fillers, pigments, light stabilizers in the form of UV-absorbing sterically hindered amines (HALS), aging inhibitors in the form of lactones, primary and secondary antioxidants, cross-linking agents and/or cross-linking promoters. The self-adhesive air cushion film is perforated in uniform intervals transverse to the longitudinal direction. An independent claim is included for a process for producing a self-adhesive air cushion film.</description><subject>ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE</subject><subject>ADHESIVES</subject><subject>CHEMISTRY</subject><subject>DYES</subject><subject>LAYERED PRODUCTS</subject><subject>LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT ORNON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM</subject><subject>METALLURGY</subject><subject>MISCELLANEOUS APPLICATIONS OF MATERIALS</subject><subject>MISCELLANEOUS COMPOSITIONS</subject><subject>NATURAL RESINS</subject><subject>NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL</subject><subject>PAINTS</subject><subject>PERFORMING OPERATIONS</subject><subject>POLISHES</subject><subject>TRANSPORTING</subject><subject>USE OF MATERIALS AS ADHESIVES</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2014</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNjD0KwkAQRtNYiHqHuUCKJAq2IhFLQfsw7s66A_vnzibg7Q3qAawefLzvLavnlZypUVsSngiQM6hRLMcAhp0HFEg5FlLlM8UMJpNYmDAHlvkFeswcHjCRZeXmggj5u3sBBg0ew2hQla_iqdio19XCoBPa_Liq4NTfjueaUhxIEioKVIb-0ja7bdvsD133h_IGTL9DzQ</recordid><startdate>20140312</startdate><enddate>20140312</enddate><creator>BOEHM, NICOLAI</creator><scope>EVB</scope></search><sort><creationdate>20140312</creationdate><title>Self-adhesive air cushion film as protection for fresh varnishes during vehicle assembly and manufacturing method</title><author>BOEHM, NICOLAI</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_EP2154218A33</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; fre ; ger</language><creationdate>2014</creationdate><topic>ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE</topic><topic>ADHESIVES</topic><topic>CHEMISTRY</topic><topic>DYES</topic><topic>LAYERED PRODUCTS</topic><topic>LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT ORNON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM</topic><topic>METALLURGY</topic><topic>MISCELLANEOUS APPLICATIONS OF MATERIALS</topic><topic>MISCELLANEOUS COMPOSITIONS</topic><topic>NATURAL RESINS</topic><topic>NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL</topic><topic>PAINTS</topic><topic>PERFORMING OPERATIONS</topic><topic>POLISHES</topic><topic>TRANSPORTING</topic><topic>USE OF MATERIALS AS ADHESIVES</topic><toplevel>online_resources</toplevel><creatorcontrib>BOEHM, NICOLAI</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>BOEHM, NICOLAI</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Self-adhesive air cushion film as protection for fresh varnishes during vehicle assembly and manufacturing method</title><date>2014-03-12</date><risdate>2014</risdate><abstract>The self-adhesive air cushion film (5) comprises a first carrier film (1), on whose first side an external film made of polypropylene, polypropylene-dominated polyolefin blends or propylene-dominated olefin copolymers is applied and on whose second side a second bubble-forming carrier film (2) is present, where the second side is opposite to the first side. The bubbles are filled with air. A polyethylene sheet (3a) is inseparably and partially applied to the bubbles. A self-adhesive layer is applied to the polyethylene sheet. The external film made of polypropylene has a sealing layer. The self-adhesive air cushion film (5) comprises a first carrier film (1), on whose first side an external film made of polypropylene, polypropylene-dominated polyolefin blends or propylene-dominated olefin copolymers is applied and on whose second side a second bubble-forming carrier film (2) is present, where the second side is opposite to the first side. The bubbles are filled with air. A polyethylene sheet (3a) is inseparably and partially applied to the bubbles. A self-adhesive layer is applied to the polyethylene sheet. The external film made of polypropylene has a sealing layer that is made of polyethylene or modified polyethylene towards the first carrier film. The external film made of polypropylene contains 50 wt.% of polypropylene if it consists of a blend of polyolefins, 50 mol.% of propylene if it is olefin copolymers, and 50 mol.% of propylene if it a blend of olefin copolymers or olefin copolymers and olefin-homopolymers. The external film and the sealing layer are produced by coextrusion. An adhesion promoter layer (3b) is present between the sheet and the self-adhesive layer. The external film, the first carrier film, the second carrier film and/or the sheet contain a light stabilizer in an amount of 0.15 wt.% and/or titanium dioxide in an amount of 5-15 wt.%. The first and/or second carrier film has a three-layer construction made of polyethylene sheet/barrier layer/polyethylene sheet. The self-adhesive compound is composed of polyethylene-vinyl acetate at a vinyl acetate content of 70 wt.%, and has a loss angle tan delta of 0.6-1.0 measured at a temperature of 60[deg] C and a frequency of 10 -> 2> Hz and tan delta of 0.4-0.7 measured at a temperature of 60[deg] C and a frequency of 10 Hz. The self-adhesive layer is mixed with additives such as tackifiers, plasticizers, organic or inorganic fillers, pigments, light stabilizers in the form of UV-absorbing sterically hindered amines (HALS), aging inhibitors in the form of lactones, primary and secondary antioxidants, cross-linking agents and/or cross-linking promoters. The self-adhesive air cushion film is perforated in uniform intervals transverse to the longitudinal direction. An independent claim is included for a process for producing a self-adhesive air cushion film.</abstract><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | eng ; fre ; ger |
recordid | cdi_epo_espacenet_EP2154218A3 |
source | esp@cenet |
subjects | ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE ADHESIVES CHEMISTRY DYES LAYERED PRODUCTS LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT ORNON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM METALLURGY MISCELLANEOUS APPLICATIONS OF MATERIALS MISCELLANEOUS COMPOSITIONS NATURAL RESINS NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL PAINTS PERFORMING OPERATIONS POLISHES TRANSPORTING USE OF MATERIALS AS ADHESIVES |
title | Self-adhesive air cushion film as protection for fresh varnishes during vehicle assembly and manufacturing method |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-18T10%3A23%3A11IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=BOEHM,%20NICOLAI&rft.date=2014-03-12&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EEP2154218A3%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |