METHOD FOR MAKING REDUCED STRIAE LOW EXPANSION GLASS

The invention is directed to a low expansion glass with reduced striae, the glass have a point-to-point variation in titania content is 0.1 wt % or less through its thickness and a CTE of 0±3 ppb/° C. in the temperature range 5-35° C. The invention is further directed to a method for producing the l...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: MAXON, JOHN E, ROSCH, WILLIAM R
Format: Patent
Sprache:eng ; fre ; ger
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator MAXON, JOHN E
ROSCH, WILLIAM R
description The invention is directed to a low expansion glass with reduced striae, the glass have a point-to-point variation in titania content is 0.1 wt % or less through its thickness and a CTE of 0±3 ppb/° C. in the temperature range 5-35° C. The invention is further directed to a method for producing the low expansion glass by using a method in which the time for repetition of the oscillation patterns used in the process are 10 minutes or less. In addition, the low expansion glass of the invention can have striae further reduced by heat-treating the glass at temperatures above 1600° C. for a time in the range of 48-160 hours.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_EP2038230A2</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>EP2038230A2</sourcerecordid><originalsourceid>FETCH-epo_espacenet_EP2038230A23</originalsourceid><addsrcrecordid>eNrjZDDxdQ3x8HdRcPMPUvB19Pb0c1cIcnUJdXZ1UQgOCfJ0dFXw8Q9XcI0IcPQL9vT3U3D3cQwO5mFgTUvMKU7lhdLcDApuriHOHrqpBfnxqcUFicmpeakl8a4BRgbGFkbGBo5GxkQoAQBpcybN</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>METHOD FOR MAKING REDUCED STRIAE LOW EXPANSION GLASS</title><source>esp@cenet</source><creator>MAXON, JOHN E ; ROSCH, WILLIAM R</creator><creatorcontrib>MAXON, JOHN E ; ROSCH, WILLIAM R</creatorcontrib><description>The invention is directed to a low expansion glass with reduced striae, the glass have a point-to-point variation in titania content is 0.1 wt % or less through its thickness and a CTE of 0±3 ppb/° C. in the temperature range 5-35° C. The invention is further directed to a method for producing the low expansion glass by using a method in which the time for repetition of the oscillation patterns used in the process are 10 minutes or less. In addition, the low expansion glass of the invention can have striae further reduced by heat-treating the glass at temperatures above 1600° C. for a time in the range of 48-160 hours.</description><language>eng ; fre ; ger</language><subject>CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS ; CHEMISTRY ; GLASS ; JOINING GLASS TO GLASS OR OTHER MATERIALS ; MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES ; METALLURGY ; MINERAL OR SLAG WOOL ; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS ; SURFACE TREATMENT OF GLASS</subject><creationdate>2009</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20090325&amp;DB=EPODOC&amp;CC=EP&amp;NR=2038230A2$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20090325&amp;DB=EPODOC&amp;CC=EP&amp;NR=2038230A2$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>MAXON, JOHN E</creatorcontrib><creatorcontrib>ROSCH, WILLIAM R</creatorcontrib><title>METHOD FOR MAKING REDUCED STRIAE LOW EXPANSION GLASS</title><description>The invention is directed to a low expansion glass with reduced striae, the glass have a point-to-point variation in titania content is 0.1 wt % or less through its thickness and a CTE of 0±3 ppb/° C. in the temperature range 5-35° C. The invention is further directed to a method for producing the low expansion glass by using a method in which the time for repetition of the oscillation patterns used in the process are 10 minutes or less. In addition, the low expansion glass of the invention can have striae further reduced by heat-treating the glass at temperatures above 1600° C. for a time in the range of 48-160 hours.</description><subject>CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS</subject><subject>CHEMISTRY</subject><subject>GLASS</subject><subject>JOINING GLASS TO GLASS OR OTHER MATERIALS</subject><subject>MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES</subject><subject>METALLURGY</subject><subject>MINERAL OR SLAG WOOL</subject><subject>SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS</subject><subject>SURFACE TREATMENT OF GLASS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2009</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZDDxdQ3x8HdRcPMPUvB19Pb0c1cIcnUJdXZ1UQgOCfJ0dFXw8Q9XcI0IcPQL9vT3U3D3cQwO5mFgTUvMKU7lhdLcDApuriHOHrqpBfnxqcUFicmpeakl8a4BRgbGFkbGBo5GxkQoAQBpcybN</recordid><startdate>20090325</startdate><enddate>20090325</enddate><creator>MAXON, JOHN E</creator><creator>ROSCH, WILLIAM R</creator><scope>EVB</scope></search><sort><creationdate>20090325</creationdate><title>METHOD FOR MAKING REDUCED STRIAE LOW EXPANSION GLASS</title><author>MAXON, JOHN E ; ROSCH, WILLIAM R</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_EP2038230A23</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; fre ; ger</language><creationdate>2009</creationdate><topic>CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS</topic><topic>CHEMISTRY</topic><topic>GLASS</topic><topic>JOINING GLASS TO GLASS OR OTHER MATERIALS</topic><topic>MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES</topic><topic>METALLURGY</topic><topic>MINERAL OR SLAG WOOL</topic><topic>SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS</topic><topic>SURFACE TREATMENT OF GLASS</topic><toplevel>online_resources</toplevel><creatorcontrib>MAXON, JOHN E</creatorcontrib><creatorcontrib>ROSCH, WILLIAM R</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>MAXON, JOHN E</au><au>ROSCH, WILLIAM R</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>METHOD FOR MAKING REDUCED STRIAE LOW EXPANSION GLASS</title><date>2009-03-25</date><risdate>2009</risdate><abstract>The invention is directed to a low expansion glass with reduced striae, the glass have a point-to-point variation in titania content is 0.1 wt % or less through its thickness and a CTE of 0±3 ppb/° C. in the temperature range 5-35° C. The invention is further directed to a method for producing the low expansion glass by using a method in which the time for repetition of the oscillation patterns used in the process are 10 minutes or less. In addition, the low expansion glass of the invention can have striae further reduced by heat-treating the glass at temperatures above 1600° C. for a time in the range of 48-160 hours.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng ; fre ; ger
recordid cdi_epo_espacenet_EP2038230A2
source esp@cenet
subjects CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS
CHEMISTRY
GLASS
JOINING GLASS TO GLASS OR OTHER MATERIALS
MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES
METALLURGY
MINERAL OR SLAG WOOL
SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS
SURFACE TREATMENT OF GLASS
title METHOD FOR MAKING REDUCED STRIAE LOW EXPANSION GLASS
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-26T01%3A37%3A03IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=MAXON,%20JOHN%20E&rft.date=2009-03-25&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EEP2038230A2%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true