OPTICAL ARTICLE COMPRISING AN EXTERNAL WATER- AND/OR OIL-REPELLENT COATING COATED WITH A TEMPORARY COATING

The optical article e.g. ophthalmic lens comprises an external water- and/or oil-repellent coating on one of its principle surfaces and a strippable coating directly deposited on the external water- and/or oil repellent coating. The external water- and/or oil repellent coating has a surface energy =...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: HABASSI, CHEFIK, LY, LEANG
Format: Patent
Sprache:eng ; fre ; ger
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator HABASSI, CHEFIK
LY, LEANG
description The optical article e.g. ophthalmic lens comprises an external water- and/or oil-repellent coating on one of its principle surfaces and a strippable coating directly deposited on the external water- and/or oil repellent coating. The external water- and/or oil repellent coating has a surface energy = 12 mJ/m 2>. The strippable coating has a surface energy >= 30 mJ/m 2>, and has a polar surface energy lower than 26 mJ/m 2>. A thickness and an elongation-to-break of the strippable coating is 15-20 mu m and = 150% respectively. The optical article e.g. ophthalmic lens comprises an external water- and/or oil-repellent coating on one of its principle surfaces and a strippable coating directly deposited on the external water- and/or oil repellent coating. The external water- and/or oil repellent coating has a surface energy = 12 mJ/m 2>. The strippable coating has a surface energy >= 30 mJ/m 2>, and has a polar surface energy lower than 26 mJ/m 2>. A thickness and an elongation-to-break of the strippable coating is 15-20 mu m and = 150% respectively. A solid content of polyurethane latex is 25-45 wt.% with respect to a total weight of the latex composition. The external water- and/or oil-repellent coating is deposited on a mono or multi-layer anti-reflection coating.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_EP2021836B1</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>EP2021836B1</sourcerecordid><originalsourceid>FETCH-epo_espacenet_EP2021836B13</originalsourceid><addsrcrecordid>eNqNi8EKwjAQRHvxIOo_7A8EbQvidU1XG0iTsC5UT6VIPIhoof4_pqB3T2-YNzPP7j6I0WgBOdESaN8ENifjjoAO6CzELukWU1CpqtaewRurmAJZS07SBWXaT6QKWiM1IAg1wTPy5eeX2ezWP8a4-nKRwYFE1yoOry6OQ3-Nz_juKBSbIt-V231e_jH5AAqvNY0</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>OPTICAL ARTICLE COMPRISING AN EXTERNAL WATER- AND/OR OIL-REPELLENT COATING COATED WITH A TEMPORARY COATING</title><source>esp@cenet</source><creator>HABASSI, CHEFIK ; LY, LEANG</creator><creatorcontrib>HABASSI, CHEFIK ; LY, LEANG</creatorcontrib><description>The optical article e.g. ophthalmic lens comprises an external water- and/or oil-repellent coating on one of its principle surfaces and a strippable coating directly deposited on the external water- and/or oil repellent coating. The external water- and/or oil repellent coating has a surface energy = 12 mJ/m 2&gt;. The strippable coating has a surface energy &gt;= 30 mJ/m 2&gt;, and has a polar surface energy lower than 26 mJ/m 2&gt;. A thickness and an elongation-to-break of the strippable coating is 15-20 mu m and = 150% respectively. The optical article e.g. ophthalmic lens comprises an external water- and/or oil-repellent coating on one of its principle surfaces and a strippable coating directly deposited on the external water- and/or oil repellent coating. The external water- and/or oil repellent coating has a surface energy = 12 mJ/m 2&gt;. The strippable coating has a surface energy &gt;= 30 mJ/m 2&gt;, and has a polar surface energy lower than 26 mJ/m 2&gt;. A thickness and an elongation-to-break of the strippable coating is 15-20 mu m and = 150% respectively. A solid content of polyurethane latex is 25-45 wt.% with respect to a total weight of the latex composition. The external water- and/or oil-repellent coating is deposited on a mono or multi-layer anti-reflection coating.</description><language>eng ; fre ; ger</language><subject>CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS ; CHEMISTRY ; GLASS ; JOINING GLASS TO GLASS OR OTHER MATERIALS ; METALLURGY ; MINERAL OR SLAG WOOL ; OPTICAL ELEMENTS, SYSTEMS, OR APPARATUS ; OPTICS ; PHYSICS ; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS ; SURFACE TREATMENT OF GLASS</subject><creationdate>2011</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20110629&amp;DB=EPODOC&amp;CC=EP&amp;NR=2021836B1$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20110629&amp;DB=EPODOC&amp;CC=EP&amp;NR=2021836B1$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>HABASSI, CHEFIK</creatorcontrib><creatorcontrib>LY, LEANG</creatorcontrib><title>OPTICAL ARTICLE COMPRISING AN EXTERNAL WATER- AND/OR OIL-REPELLENT COATING COATED WITH A TEMPORARY COATING</title><description>The optical article e.g. ophthalmic lens comprises an external water- and/or oil-repellent coating on one of its principle surfaces and a strippable coating directly deposited on the external water- and/or oil repellent coating. The external water- and/or oil repellent coating has a surface energy = 12 mJ/m 2&gt;. The strippable coating has a surface energy &gt;= 30 mJ/m 2&gt;, and has a polar surface energy lower than 26 mJ/m 2&gt;. A thickness and an elongation-to-break of the strippable coating is 15-20 mu m and = 150% respectively. The optical article e.g. ophthalmic lens comprises an external water- and/or oil-repellent coating on one of its principle surfaces and a strippable coating directly deposited on the external water- and/or oil repellent coating. The external water- and/or oil repellent coating has a surface energy = 12 mJ/m 2&gt;. The strippable coating has a surface energy &gt;= 30 mJ/m 2&gt;, and has a polar surface energy lower than 26 mJ/m 2&gt;. A thickness and an elongation-to-break of the strippable coating is 15-20 mu m and = 150% respectively. A solid content of polyurethane latex is 25-45 wt.% with respect to a total weight of the latex composition. The external water- and/or oil-repellent coating is deposited on a mono or multi-layer anti-reflection coating.</description><subject>CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS</subject><subject>CHEMISTRY</subject><subject>GLASS</subject><subject>JOINING GLASS TO GLASS OR OTHER MATERIALS</subject><subject>METALLURGY</subject><subject>MINERAL OR SLAG WOOL</subject><subject>OPTICAL ELEMENTS, SYSTEMS, OR APPARATUS</subject><subject>OPTICS</subject><subject>PHYSICS</subject><subject>SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS</subject><subject>SURFACE TREATMENT OF GLASS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2011</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNi8EKwjAQRHvxIOo_7A8EbQvidU1XG0iTsC5UT6VIPIhoof4_pqB3T2-YNzPP7j6I0WgBOdESaN8ENifjjoAO6CzELukWU1CpqtaewRurmAJZS07SBWXaT6QKWiM1IAg1wTPy5eeX2ezWP8a4-nKRwYFE1yoOry6OQ3-Nz_juKBSbIt-V231e_jH5AAqvNY0</recordid><startdate>20110629</startdate><enddate>20110629</enddate><creator>HABASSI, CHEFIK</creator><creator>LY, LEANG</creator><scope>EVB</scope></search><sort><creationdate>20110629</creationdate><title>OPTICAL ARTICLE COMPRISING AN EXTERNAL WATER- AND/OR OIL-REPELLENT COATING COATED WITH A TEMPORARY COATING</title><author>HABASSI, CHEFIK ; LY, LEANG</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_EP2021836B13</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; fre ; ger</language><creationdate>2011</creationdate><topic>CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS</topic><topic>CHEMISTRY</topic><topic>GLASS</topic><topic>JOINING GLASS TO GLASS OR OTHER MATERIALS</topic><topic>METALLURGY</topic><topic>MINERAL OR SLAG WOOL</topic><topic>OPTICAL ELEMENTS, SYSTEMS, OR APPARATUS</topic><topic>OPTICS</topic><topic>PHYSICS</topic><topic>SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS</topic><topic>SURFACE TREATMENT OF GLASS</topic><toplevel>online_resources</toplevel><creatorcontrib>HABASSI, CHEFIK</creatorcontrib><creatorcontrib>LY, LEANG</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>HABASSI, CHEFIK</au><au>LY, LEANG</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>OPTICAL ARTICLE COMPRISING AN EXTERNAL WATER- AND/OR OIL-REPELLENT COATING COATED WITH A TEMPORARY COATING</title><date>2011-06-29</date><risdate>2011</risdate><abstract>The optical article e.g. ophthalmic lens comprises an external water- and/or oil-repellent coating on one of its principle surfaces and a strippable coating directly deposited on the external water- and/or oil repellent coating. The external water- and/or oil repellent coating has a surface energy = 12 mJ/m 2&gt;. The strippable coating has a surface energy &gt;= 30 mJ/m 2&gt;, and has a polar surface energy lower than 26 mJ/m 2&gt;. A thickness and an elongation-to-break of the strippable coating is 15-20 mu m and = 150% respectively. The optical article e.g. ophthalmic lens comprises an external water- and/or oil-repellent coating on one of its principle surfaces and a strippable coating directly deposited on the external water- and/or oil repellent coating. The external water- and/or oil repellent coating has a surface energy = 12 mJ/m 2&gt;. The strippable coating has a surface energy &gt;= 30 mJ/m 2&gt;, and has a polar surface energy lower than 26 mJ/m 2&gt;. A thickness and an elongation-to-break of the strippable coating is 15-20 mu m and = 150% respectively. A solid content of polyurethane latex is 25-45 wt.% with respect to a total weight of the latex composition. The external water- and/or oil-repellent coating is deposited on a mono or multi-layer anti-reflection coating.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng ; fre ; ger
recordid cdi_epo_espacenet_EP2021836B1
source esp@cenet
subjects CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS
CHEMISTRY
GLASS
JOINING GLASS TO GLASS OR OTHER MATERIALS
METALLURGY
MINERAL OR SLAG WOOL
OPTICAL ELEMENTS, SYSTEMS, OR APPARATUS
OPTICS
PHYSICS
SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS
SURFACE TREATMENT OF GLASS
title OPTICAL ARTICLE COMPRISING AN EXTERNAL WATER- AND/OR OIL-REPELLENT COATING COATED WITH A TEMPORARY COATING
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-27T09%3A02%3A20IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=HABASSI,%20CHEFIK&rft.date=2011-06-29&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EEP2021836B1%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true