STEEL PIPE FOR AIR BAG INFLATOR AND METHOD FOR PRODUCTION THEREOF

A steel pipe for an airbag inflator having a high strength of at least 900 MPa and preferably at least 1000 MPa in tensile strength along with a high toughness and exhibiting good resistance to bursting such that it has no propagation of cracks in a burst test at -40°C or below is manufactured by qu...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: ARAI, YUJI, TAKANO, TAKASHI, HITOSHIO, KEISUKE, KONDO, KUNIO
Format: Patent
Sprache:eng ; fre ; ger
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator ARAI, YUJI
TAKANO, TAKASHI
HITOSHIO, KEISUKE
KONDO, KUNIO
description A steel pipe for an airbag inflator having a high strength of at least 900 MPa and preferably at least 1000 MPa in tensile strength along with a high toughness and exhibiting good resistance to bursting such that it has no propagation of cracks in a burst test at -40°C or below is manufactured by quenching a pipe of a steel comprising, in mass %, C: 0.05 - 0.20 %, Si: 0.1 - 1.0 %, P: at most 0.025 %, S: at most 0.010 %, Cr: 0.05 - 1.45 %, Al: at most 0.10 %, and one or both of Ti and Mn satisfying Ti ‰ 0.02% and 0.4% ‰ Mn + 40Ti ‰ 1.2% from a temperature of at least the Ac 1 transformation point of the steel, tempering the pipe at a temperature lower than the Ac 1 transformation point, applying cold working to it with a reduction of area of at most 65%, and subjecting it to stress relief annealing at a temperature lower than the Ac 1 transformation point. The ratio L/T of the X-ray integrated intensity ratio of the {110} plane measured for the cross section perpendicular to the axial direction L of the steel pipe to that measured for the cross section perpendicular to the circumferential direction T is at most 50.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_EP1816227B1</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>EP1816227B1</sourcerecordid><originalsourceid>FETCH-epo_espacenet_EP1816227B13</originalsourceid><addsrcrecordid>eNrjZHAMDnF19VEI8AxwVXDzD1Jw9AxScHJ0V_D0c_NxDAEJ-Lko-LqGePi7gOUDgvxdQp1DPP39FEI8XINc_d14GFjTEnOKU3mhNDeDgptriLOHbmpBfnxqcUFicmpeakm8a4ChhaGZkZG5k6ExEUoAUGMqLg</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>STEEL PIPE FOR AIR BAG INFLATOR AND METHOD FOR PRODUCTION THEREOF</title><source>esp@cenet</source><creator>ARAI, YUJI ; TAKANO, TAKASHI ; HITOSHIO, KEISUKE ; KONDO, KUNIO</creator><creatorcontrib>ARAI, YUJI ; TAKANO, TAKASHI ; HITOSHIO, KEISUKE ; KONDO, KUNIO</creatorcontrib><description>A steel pipe for an airbag inflator having a high strength of at least 900 MPa and preferably at least 1000 MPa in tensile strength along with a high toughness and exhibiting good resistance to bursting such that it has no propagation of cracks in a burst test at -40°C or below is manufactured by quenching a pipe of a steel comprising, in mass %, C: 0.05 - 0.20 %, Si: 0.1 - 1.0 %, P: at most 0.025 %, S: at most 0.010 %, Cr: 0.05 - 1.45 %, Al: at most 0.10 %, and one or both of Ti and Mn satisfying Ti ‰ 0.02% and 0.4% ‰ Mn + 40Ti ‰ 1.2% from a temperature of at least the Ac 1 transformation point of the steel, tempering the pipe at a temperature lower than the Ac 1 transformation point, applying cold working to it with a reduction of area of at most 65%, and subjecting it to stress relief annealing at a temperature lower than the Ac 1 transformation point. The ratio L/T of the X-ray integrated intensity ratio of the {110} plane measured for the cross section perpendicular to the axial direction L of the steel pipe to that measured for the cross section perpendicular to the circumferential direction T is at most 50.</description><language>eng ; fre ; ger</language><subject>ALLOYS ; CHEMISTRY ; FERROUS OR NON-FERROUS ALLOYS ; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS ; MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS ; METALLURGY ; METALLURGY OF IRON ; MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS ; PERFORMING OPERATIONS ; TRANSPORTING ; TREATMENT OF ALLOYS OR NON-FERROUS METALS ; VEHICLES IN GENERAL ; VEHICLES, VEHICLE FITTINGS, OR VEHICLE PARTS, NOT OTHERWISEPROVIDED FOR</subject><creationdate>2016</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20160309&amp;DB=EPODOC&amp;CC=EP&amp;NR=1816227B1$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25563,76418</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20160309&amp;DB=EPODOC&amp;CC=EP&amp;NR=1816227B1$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>ARAI, YUJI</creatorcontrib><creatorcontrib>TAKANO, TAKASHI</creatorcontrib><creatorcontrib>HITOSHIO, KEISUKE</creatorcontrib><creatorcontrib>KONDO, KUNIO</creatorcontrib><title>STEEL PIPE FOR AIR BAG INFLATOR AND METHOD FOR PRODUCTION THEREOF</title><description>A steel pipe for an airbag inflator having a high strength of at least 900 MPa and preferably at least 1000 MPa in tensile strength along with a high toughness and exhibiting good resistance to bursting such that it has no propagation of cracks in a burst test at -40°C or below is manufactured by quenching a pipe of a steel comprising, in mass %, C: 0.05 - 0.20 %, Si: 0.1 - 1.0 %, P: at most 0.025 %, S: at most 0.010 %, Cr: 0.05 - 1.45 %, Al: at most 0.10 %, and one or both of Ti and Mn satisfying Ti ‰ 0.02% and 0.4% ‰ Mn + 40Ti ‰ 1.2% from a temperature of at least the Ac 1 transformation point of the steel, tempering the pipe at a temperature lower than the Ac 1 transformation point, applying cold working to it with a reduction of area of at most 65%, and subjecting it to stress relief annealing at a temperature lower than the Ac 1 transformation point. The ratio L/T of the X-ray integrated intensity ratio of the {110} plane measured for the cross section perpendicular to the axial direction L of the steel pipe to that measured for the cross section perpendicular to the circumferential direction T is at most 50.</description><subject>ALLOYS</subject><subject>CHEMISTRY</subject><subject>FERROUS OR NON-FERROUS ALLOYS</subject><subject>GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS</subject><subject>MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS</subject><subject>METALLURGY</subject><subject>METALLURGY OF IRON</subject><subject>MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS</subject><subject>PERFORMING OPERATIONS</subject><subject>TRANSPORTING</subject><subject>TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><subject>VEHICLES IN GENERAL</subject><subject>VEHICLES, VEHICLE FITTINGS, OR VEHICLE PARTS, NOT OTHERWISEPROVIDED FOR</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2016</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZHAMDnF19VEI8AxwVXDzD1Jw9AxScHJ0V_D0c_NxDAEJ-Lko-LqGePi7gOUDgvxdQp1DPP39FEI8XINc_d14GFjTEnOKU3mhNDeDgptriLOHbmpBfnxqcUFicmpeakm8a4ChhaGZkZG5k6ExEUoAUGMqLg</recordid><startdate>20160309</startdate><enddate>20160309</enddate><creator>ARAI, YUJI</creator><creator>TAKANO, TAKASHI</creator><creator>HITOSHIO, KEISUKE</creator><creator>KONDO, KUNIO</creator><scope>EVB</scope></search><sort><creationdate>20160309</creationdate><title>STEEL PIPE FOR AIR BAG INFLATOR AND METHOD FOR PRODUCTION THEREOF</title><author>ARAI, YUJI ; TAKANO, TAKASHI ; HITOSHIO, KEISUKE ; KONDO, KUNIO</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_EP1816227B13</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; fre ; ger</language><creationdate>2016</creationdate><topic>ALLOYS</topic><topic>CHEMISTRY</topic><topic>FERROUS OR NON-FERROUS ALLOYS</topic><topic>GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS</topic><topic>MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS</topic><topic>METALLURGY</topic><topic>METALLURGY OF IRON</topic><topic>MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS</topic><topic>PERFORMING OPERATIONS</topic><topic>TRANSPORTING</topic><topic>TREATMENT OF ALLOYS OR NON-FERROUS METALS</topic><topic>VEHICLES IN GENERAL</topic><topic>VEHICLES, VEHICLE FITTINGS, OR VEHICLE PARTS, NOT OTHERWISEPROVIDED FOR</topic><toplevel>online_resources</toplevel><creatorcontrib>ARAI, YUJI</creatorcontrib><creatorcontrib>TAKANO, TAKASHI</creatorcontrib><creatorcontrib>HITOSHIO, KEISUKE</creatorcontrib><creatorcontrib>KONDO, KUNIO</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>ARAI, YUJI</au><au>TAKANO, TAKASHI</au><au>HITOSHIO, KEISUKE</au><au>KONDO, KUNIO</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>STEEL PIPE FOR AIR BAG INFLATOR AND METHOD FOR PRODUCTION THEREOF</title><date>2016-03-09</date><risdate>2016</risdate><abstract>A steel pipe for an airbag inflator having a high strength of at least 900 MPa and preferably at least 1000 MPa in tensile strength along with a high toughness and exhibiting good resistance to bursting such that it has no propagation of cracks in a burst test at -40°C or below is manufactured by quenching a pipe of a steel comprising, in mass %, C: 0.05 - 0.20 %, Si: 0.1 - 1.0 %, P: at most 0.025 %, S: at most 0.010 %, Cr: 0.05 - 1.45 %, Al: at most 0.10 %, and one or both of Ti and Mn satisfying Ti ‰ 0.02% and 0.4% ‰ Mn + 40Ti ‰ 1.2% from a temperature of at least the Ac 1 transformation point of the steel, tempering the pipe at a temperature lower than the Ac 1 transformation point, applying cold working to it with a reduction of area of at most 65%, and subjecting it to stress relief annealing at a temperature lower than the Ac 1 transformation point. The ratio L/T of the X-ray integrated intensity ratio of the {110} plane measured for the cross section perpendicular to the axial direction L of the steel pipe to that measured for the cross section perpendicular to the circumferential direction T is at most 50.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng ; fre ; ger
recordid cdi_epo_espacenet_EP1816227B1
source esp@cenet
subjects ALLOYS
CHEMISTRY
FERROUS OR NON-FERROUS ALLOYS
GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS
MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS
METALLURGY
METALLURGY OF IRON
MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS
PERFORMING OPERATIONS
TRANSPORTING
TREATMENT OF ALLOYS OR NON-FERROUS METALS
VEHICLES IN GENERAL
VEHICLES, VEHICLE FITTINGS, OR VEHICLE PARTS, NOT OTHERWISEPROVIDED FOR
title STEEL PIPE FOR AIR BAG INFLATOR AND METHOD FOR PRODUCTION THEREOF
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-08T18%3A29%3A55IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=ARAI,%20YUJI&rft.date=2016-03-09&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EEP1816227B1%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true