Process for the preparation of a temperature-stable TiO2/SiO2 mixed-oxide and its use as a catalyst carrier

Preparation of a titanium dioxide/silicone dioxide mixture, their hydrates and/or oxide hydrates comprises adding a titanium compound and/or their hydrolysis product with a silicic acid compound in an aqueous medium and hydrolyzing the titanium compound in presence or absence of the silicic acid com...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: DALLMANN, KAI, BRASCH, ANDREA, FREESE, UTE, SCHIMANSKI, JUERGEN, ROLFS, SOENKE, DOELLING, KAI
Format: Patent
Sprache:eng ; fre ; ger
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator DALLMANN, KAI
BRASCH, ANDREA
FREESE, UTE
SCHIMANSKI, JUERGEN
ROLFS, SOENKE
DOELLING, KAI
description Preparation of a titanium dioxide/silicone dioxide mixture, their hydrates and/or oxide hydrates comprises adding a titanium compound and/or their hydrolysis product with a silicic acid compound in an aqueous medium and hydrolyzing the titanium compound in presence or absence of the silicic acid compound comprising an aqueous silicic acid sol, where the titanium dioxide/silicone dioxide mixture comprises 0.5-95 wt.% of silicone and the titanium compound is a titanium alcoholate exhibiting at least 1-16C alcoholates. An independent claim is included for the titanium dioxide/silicone dioxide mixture comprising less than 25 wt.% of silicone dioxide and greater than 75, preferably 95 wt.% of the titanium dioxide that is present in titanium dioxide phase, where the titanium dioxide/silicone dioxide mixture exhibits pore volumes of greater than 0.35, preferably 0.50 ml/g and a rutile transformation temperature of greater than 850, preferably 1000[deg]C.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_EP1719737A1</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>EP1719737A1</sourcerecordid><originalsourceid>FETCH-epo_espacenet_EP1719737A13</originalsourceid><addsrcrecordid>eNqNi70KwkAQhNNYiPoO-wJBYopgKRKxM2D6sCYTPPJzx-4G4tt7hQ9gM_PxMbNNhkp8C1XqvZC9QUEQWNicn8n3xGSYAqJYBKkav0ZQ7R6n4zMGTW5Fl_rVdSCeO3KmtGhkjc-WjcePWgQRB9knm55HxeHXu4RuZX29pwi-gQZuMcOassqK7FzkxSXL_5h8AbeKP9E</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Process for the preparation of a temperature-stable TiO2/SiO2 mixed-oxide and its use as a catalyst carrier</title><source>esp@cenet</source><creator>DALLMANN, KAI ; BRASCH, ANDREA ; FREESE, UTE ; SCHIMANSKI, JUERGEN ; ROLFS, SOENKE ; DOELLING, KAI</creator><creatorcontrib>DALLMANN, KAI ; BRASCH, ANDREA ; FREESE, UTE ; SCHIMANSKI, JUERGEN ; ROLFS, SOENKE ; DOELLING, KAI</creatorcontrib><description>Preparation of a titanium dioxide/silicone dioxide mixture, their hydrates and/or oxide hydrates comprises adding a titanium compound and/or their hydrolysis product with a silicic acid compound in an aqueous medium and hydrolyzing the titanium compound in presence or absence of the silicic acid compound comprising an aqueous silicic acid sol, where the titanium dioxide/silicone dioxide mixture comprises 0.5-95 wt.% of silicone and the titanium compound is a titanium alcoholate exhibiting at least 1-16C alcoholates. An independent claim is included for the titanium dioxide/silicone dioxide mixture comprising less than 25 wt.% of silicone dioxide and greater than 75, preferably 95 wt.% of the titanium dioxide that is present in titanium dioxide phase, where the titanium dioxide/silicone dioxide mixture exhibits pore volumes of greater than 0.35, preferably 0.50 ml/g and a rutile transformation temperature of greater than 850, preferably 1000[deg]C.</description><language>eng ; fre ; ger</language><subject>CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOIDCHEMISTRY ; CHEMISTRY ; COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSESC01D OR C01F ; INORGANIC CHEMISTRY ; METALLURGY ; PERFORMING OPERATIONS ; PHYSICAL OR CHEMICAL PROCESSES OR APPARATUS IN GENERAL ; THEIR RELEVANT APPARATUS ; TRANSPORTING</subject><creationdate>2006</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20061108&amp;DB=EPODOC&amp;CC=EP&amp;NR=1719737A1$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20061108&amp;DB=EPODOC&amp;CC=EP&amp;NR=1719737A1$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>DALLMANN, KAI</creatorcontrib><creatorcontrib>BRASCH, ANDREA</creatorcontrib><creatorcontrib>FREESE, UTE</creatorcontrib><creatorcontrib>SCHIMANSKI, JUERGEN</creatorcontrib><creatorcontrib>ROLFS, SOENKE</creatorcontrib><creatorcontrib>DOELLING, KAI</creatorcontrib><title>Process for the preparation of a temperature-stable TiO2/SiO2 mixed-oxide and its use as a catalyst carrier</title><description>Preparation of a titanium dioxide/silicone dioxide mixture, their hydrates and/or oxide hydrates comprises adding a titanium compound and/or their hydrolysis product with a silicic acid compound in an aqueous medium and hydrolyzing the titanium compound in presence or absence of the silicic acid compound comprising an aqueous silicic acid sol, where the titanium dioxide/silicone dioxide mixture comprises 0.5-95 wt.% of silicone and the titanium compound is a titanium alcoholate exhibiting at least 1-16C alcoholates. An independent claim is included for the titanium dioxide/silicone dioxide mixture comprising less than 25 wt.% of silicone dioxide and greater than 75, preferably 95 wt.% of the titanium dioxide that is present in titanium dioxide phase, where the titanium dioxide/silicone dioxide mixture exhibits pore volumes of greater than 0.35, preferably 0.50 ml/g and a rutile transformation temperature of greater than 850, preferably 1000[deg]C.</description><subject>CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOIDCHEMISTRY</subject><subject>CHEMISTRY</subject><subject>COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSESC01D OR C01F</subject><subject>INORGANIC CHEMISTRY</subject><subject>METALLURGY</subject><subject>PERFORMING OPERATIONS</subject><subject>PHYSICAL OR CHEMICAL PROCESSES OR APPARATUS IN GENERAL</subject><subject>THEIR RELEVANT APPARATUS</subject><subject>TRANSPORTING</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2006</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNi70KwkAQhNNYiPoO-wJBYopgKRKxM2D6sCYTPPJzx-4G4tt7hQ9gM_PxMbNNhkp8C1XqvZC9QUEQWNicn8n3xGSYAqJYBKkav0ZQ7R6n4zMGTW5Fl_rVdSCeO3KmtGhkjc-WjcePWgQRB9knm55HxeHXu4RuZX29pwi-gQZuMcOassqK7FzkxSXL_5h8AbeKP9E</recordid><startdate>20061108</startdate><enddate>20061108</enddate><creator>DALLMANN, KAI</creator><creator>BRASCH, ANDREA</creator><creator>FREESE, UTE</creator><creator>SCHIMANSKI, JUERGEN</creator><creator>ROLFS, SOENKE</creator><creator>DOELLING, KAI</creator><scope>EVB</scope></search><sort><creationdate>20061108</creationdate><title>Process for the preparation of a temperature-stable TiO2/SiO2 mixed-oxide and its use as a catalyst carrier</title><author>DALLMANN, KAI ; BRASCH, ANDREA ; FREESE, UTE ; SCHIMANSKI, JUERGEN ; ROLFS, SOENKE ; DOELLING, KAI</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_EP1719737A13</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; fre ; ger</language><creationdate>2006</creationdate><topic>CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOIDCHEMISTRY</topic><topic>CHEMISTRY</topic><topic>COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSESC01D OR C01F</topic><topic>INORGANIC CHEMISTRY</topic><topic>METALLURGY</topic><topic>PERFORMING OPERATIONS</topic><topic>PHYSICAL OR CHEMICAL PROCESSES OR APPARATUS IN GENERAL</topic><topic>THEIR RELEVANT APPARATUS</topic><topic>TRANSPORTING</topic><toplevel>online_resources</toplevel><creatorcontrib>DALLMANN, KAI</creatorcontrib><creatorcontrib>BRASCH, ANDREA</creatorcontrib><creatorcontrib>FREESE, UTE</creatorcontrib><creatorcontrib>SCHIMANSKI, JUERGEN</creatorcontrib><creatorcontrib>ROLFS, SOENKE</creatorcontrib><creatorcontrib>DOELLING, KAI</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>DALLMANN, KAI</au><au>BRASCH, ANDREA</au><au>FREESE, UTE</au><au>SCHIMANSKI, JUERGEN</au><au>ROLFS, SOENKE</au><au>DOELLING, KAI</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Process for the preparation of a temperature-stable TiO2/SiO2 mixed-oxide and its use as a catalyst carrier</title><date>2006-11-08</date><risdate>2006</risdate><abstract>Preparation of a titanium dioxide/silicone dioxide mixture, their hydrates and/or oxide hydrates comprises adding a titanium compound and/or their hydrolysis product with a silicic acid compound in an aqueous medium and hydrolyzing the titanium compound in presence or absence of the silicic acid compound comprising an aqueous silicic acid sol, where the titanium dioxide/silicone dioxide mixture comprises 0.5-95 wt.% of silicone and the titanium compound is a titanium alcoholate exhibiting at least 1-16C alcoholates. An independent claim is included for the titanium dioxide/silicone dioxide mixture comprising less than 25 wt.% of silicone dioxide and greater than 75, preferably 95 wt.% of the titanium dioxide that is present in titanium dioxide phase, where the titanium dioxide/silicone dioxide mixture exhibits pore volumes of greater than 0.35, preferably 0.50 ml/g and a rutile transformation temperature of greater than 850, preferably 1000[deg]C.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng ; fre ; ger
recordid cdi_epo_espacenet_EP1719737A1
source esp@cenet
subjects CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOIDCHEMISTRY
CHEMISTRY
COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSESC01D OR C01F
INORGANIC CHEMISTRY
METALLURGY
PERFORMING OPERATIONS
PHYSICAL OR CHEMICAL PROCESSES OR APPARATUS IN GENERAL
THEIR RELEVANT APPARATUS
TRANSPORTING
title Process for the preparation of a temperature-stable TiO2/SiO2 mixed-oxide and its use as a catalyst carrier
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-04T00%3A04%3A08IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=DALLMANN,%20KAI&rft.date=2006-11-08&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EEP1719737A1%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true