Method for reducing the hydrogen sensitivity of optical fibers at 1380nm-1410nm
A method for reducing the hydrogen aging loss of silica optical fibers by irreversible reaction of the peroxide defects with deuterium is described. This method comprises the step of contacting the optical fiber with deuterium by exposure to a gas mixture containing deuterium at a temperature compat...
Gespeichert in:
Hauptverfasser: | , , , , , |
---|---|
Format: | Patent |
Sprache: | eng ; fre ; ger |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | DECAUX, ISABELLE VOOTS, TERRY CAMPION, JEAN-FLORENT CHARLTON, ROGER DUPONT, PHILIPPE PIFFARETTI, JOSE |
description | A method for reducing the hydrogen aging loss of silica optical fibers by irreversible reaction of the peroxide defects with deuterium is described. This method comprises the step of contacting the optical fiber with deuterium by exposure to a gas mixture containing deuterium at a temperature compatible with the fiber without exposing the fiber to any further activation, and subsequently the step of degassing the fiber in a neutral atmosphere. The invention relates further a process of producing optical fibers with low hydrogen aging loss wherein an optical fiber is treated using the method for reducing the hydrogen aging loss. Finally, the invention relates to optical fibers with low hydrogen aging loss obtainable by this process and telecommunication cables produced using these optical fibers. Using the new method, an activation step using intense light and/or elevated temperature is not necessary to achieve the reaction of peroxide defects in silica with deuterium. The process according to the invention allows reaction at temperatures such as the ambient temperature without any further activation. |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_EP1182176B1</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>EP1182176B1</sourcerecordid><originalsourceid>FETCH-epo_espacenet_EP1182176B13</originalsourceid><addsrcrecordid>eNqNyrEKwjAQANAsDqL-w_1AwbOinZWKi-jgXmJ6aQ5qLiSn0L_XwQ9wesubm-uFNEgPXjJk6l-O4wAaCMLUZxkoQqFYWPnNOoF4kKTs7AieH5QLWAWsm3V8VrjFL0sz83YstPq5MHBq78dzRUk6Ksk6iqRde0NsNrjfHbD-o3wAYNg0_w</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Method for reducing the hydrogen sensitivity of optical fibers at 1380nm-1410nm</title><source>esp@cenet</source><creator>DECAUX, ISABELLE ; VOOTS, TERRY ; CAMPION, JEAN-FLORENT ; CHARLTON, ROGER ; DUPONT, PHILIPPE ; PIFFARETTI, JOSE</creator><creatorcontrib>DECAUX, ISABELLE ; VOOTS, TERRY ; CAMPION, JEAN-FLORENT ; CHARLTON, ROGER ; DUPONT, PHILIPPE ; PIFFARETTI, JOSE</creatorcontrib><description>A method for reducing the hydrogen aging loss of silica optical fibers by irreversible reaction of the peroxide defects with deuterium is described. This method comprises the step of contacting the optical fiber with deuterium by exposure to a gas mixture containing deuterium at a temperature compatible with the fiber without exposing the fiber to any further activation, and subsequently the step of degassing the fiber in a neutral atmosphere. The invention relates further a process of producing optical fibers with low hydrogen aging loss wherein an optical fiber is treated using the method for reducing the hydrogen aging loss. Finally, the invention relates to optical fibers with low hydrogen aging loss obtainable by this process and telecommunication cables produced using these optical fibers. Using the new method, an activation step using intense light and/or elevated temperature is not necessary to achieve the reaction of peroxide defects in silica with deuterium. The process according to the invention allows reaction at temperatures such as the ambient temperature without any further activation.</description><language>eng ; fre ; ger</language><subject>CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS ; CHEMISTRY ; GLASS ; JOINING GLASS TO GLASS OR OTHER MATERIALS ; METALLURGY ; MINERAL OR SLAG WOOL ; OPTICAL ELEMENTS, SYSTEMS, OR APPARATUS ; OPTICS ; PHYSICS ; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS ; SURFACE TREATMENT OF GLASS</subject><creationdate>2008</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20080723&DB=EPODOC&CC=EP&NR=1182176B1$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25543,76293</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20080723&DB=EPODOC&CC=EP&NR=1182176B1$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>DECAUX, ISABELLE</creatorcontrib><creatorcontrib>VOOTS, TERRY</creatorcontrib><creatorcontrib>CAMPION, JEAN-FLORENT</creatorcontrib><creatorcontrib>CHARLTON, ROGER</creatorcontrib><creatorcontrib>DUPONT, PHILIPPE</creatorcontrib><creatorcontrib>PIFFARETTI, JOSE</creatorcontrib><title>Method for reducing the hydrogen sensitivity of optical fibers at 1380nm-1410nm</title><description>A method for reducing the hydrogen aging loss of silica optical fibers by irreversible reaction of the peroxide defects with deuterium is described. This method comprises the step of contacting the optical fiber with deuterium by exposure to a gas mixture containing deuterium at a temperature compatible with the fiber without exposing the fiber to any further activation, and subsequently the step of degassing the fiber in a neutral atmosphere. The invention relates further a process of producing optical fibers with low hydrogen aging loss wherein an optical fiber is treated using the method for reducing the hydrogen aging loss. Finally, the invention relates to optical fibers with low hydrogen aging loss obtainable by this process and telecommunication cables produced using these optical fibers. Using the new method, an activation step using intense light and/or elevated temperature is not necessary to achieve the reaction of peroxide defects in silica with deuterium. The process according to the invention allows reaction at temperatures such as the ambient temperature without any further activation.</description><subject>CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS</subject><subject>CHEMISTRY</subject><subject>GLASS</subject><subject>JOINING GLASS TO GLASS OR OTHER MATERIALS</subject><subject>METALLURGY</subject><subject>MINERAL OR SLAG WOOL</subject><subject>OPTICAL ELEMENTS, SYSTEMS, OR APPARATUS</subject><subject>OPTICS</subject><subject>PHYSICS</subject><subject>SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS</subject><subject>SURFACE TREATMENT OF GLASS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2008</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNyrEKwjAQANAsDqL-w_1AwbOinZWKi-jgXmJ6aQ5qLiSn0L_XwQ9wesubm-uFNEgPXjJk6l-O4wAaCMLUZxkoQqFYWPnNOoF4kKTs7AieH5QLWAWsm3V8VrjFL0sz83YstPq5MHBq78dzRUk6Ksk6iqRde0NsNrjfHbD-o3wAYNg0_w</recordid><startdate>20080723</startdate><enddate>20080723</enddate><creator>DECAUX, ISABELLE</creator><creator>VOOTS, TERRY</creator><creator>CAMPION, JEAN-FLORENT</creator><creator>CHARLTON, ROGER</creator><creator>DUPONT, PHILIPPE</creator><creator>PIFFARETTI, JOSE</creator><scope>EVB</scope></search><sort><creationdate>20080723</creationdate><title>Method for reducing the hydrogen sensitivity of optical fibers at 1380nm-1410nm</title><author>DECAUX, ISABELLE ; VOOTS, TERRY ; CAMPION, JEAN-FLORENT ; CHARLTON, ROGER ; DUPONT, PHILIPPE ; PIFFARETTI, JOSE</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_EP1182176B13</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; fre ; ger</language><creationdate>2008</creationdate><topic>CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS</topic><topic>CHEMISTRY</topic><topic>GLASS</topic><topic>JOINING GLASS TO GLASS OR OTHER MATERIALS</topic><topic>METALLURGY</topic><topic>MINERAL OR SLAG WOOL</topic><topic>OPTICAL ELEMENTS, SYSTEMS, OR APPARATUS</topic><topic>OPTICS</topic><topic>PHYSICS</topic><topic>SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS</topic><topic>SURFACE TREATMENT OF GLASS</topic><toplevel>online_resources</toplevel><creatorcontrib>DECAUX, ISABELLE</creatorcontrib><creatorcontrib>VOOTS, TERRY</creatorcontrib><creatorcontrib>CAMPION, JEAN-FLORENT</creatorcontrib><creatorcontrib>CHARLTON, ROGER</creatorcontrib><creatorcontrib>DUPONT, PHILIPPE</creatorcontrib><creatorcontrib>PIFFARETTI, JOSE</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>DECAUX, ISABELLE</au><au>VOOTS, TERRY</au><au>CAMPION, JEAN-FLORENT</au><au>CHARLTON, ROGER</au><au>DUPONT, PHILIPPE</au><au>PIFFARETTI, JOSE</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Method for reducing the hydrogen sensitivity of optical fibers at 1380nm-1410nm</title><date>2008-07-23</date><risdate>2008</risdate><abstract>A method for reducing the hydrogen aging loss of silica optical fibers by irreversible reaction of the peroxide defects with deuterium is described. This method comprises the step of contacting the optical fiber with deuterium by exposure to a gas mixture containing deuterium at a temperature compatible with the fiber without exposing the fiber to any further activation, and subsequently the step of degassing the fiber in a neutral atmosphere. The invention relates further a process of producing optical fibers with low hydrogen aging loss wherein an optical fiber is treated using the method for reducing the hydrogen aging loss. Finally, the invention relates to optical fibers with low hydrogen aging loss obtainable by this process and telecommunication cables produced using these optical fibers. Using the new method, an activation step using intense light and/or elevated temperature is not necessary to achieve the reaction of peroxide defects in silica with deuterium. The process according to the invention allows reaction at temperatures such as the ambient temperature without any further activation.</abstract><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | eng ; fre ; ger |
recordid | cdi_epo_espacenet_EP1182176B1 |
source | esp@cenet |
subjects | CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS CHEMISTRY GLASS JOINING GLASS TO GLASS OR OTHER MATERIALS METALLURGY MINERAL OR SLAG WOOL OPTICAL ELEMENTS, SYSTEMS, OR APPARATUS OPTICS PHYSICS SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS SURFACE TREATMENT OF GLASS |
title | Method for reducing the hydrogen sensitivity of optical fibers at 1380nm-1410nm |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-23T17%3A59%3A55IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=DECAUX,%20ISABELLE&rft.date=2008-07-23&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EEP1182176B1%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |