Polyethylene and method of production thereof

Polyethylenes are prepared having a density in the range 900-980 kg/m3 and a weight average molecular weight >=375,000 characterized by a fracture toughness at -40° C. >20 kJ/m2 and a dynamic viscosity of

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: CLUTTON, EDWARD, QUENTIN, HOPE, PHILIP, STEPHEN
Format: Patent
Sprache:eng ; fre ; ger
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator CLUTTON, EDWARD, QUENTIN
HOPE, PHILIP, STEPHEN
description Polyethylenes are prepared having a density in the range 900-980 kg/m3 and a weight average molecular weight >=375,000 characterized by a fracture toughness at -40° C. >20 kJ/m2 and a dynamic viscosity of
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_EP1080121A1</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>EP1080121A1</sourcerecordid><originalsourceid>FETCH-epo_espacenet_EP1080121A13</originalsourceid><addsrcrecordid>eNrjZNANyM-pTC3JqMxJzUtVSMxLUcgF8vJTFPLTFAqK8lNKk0sy8_MUSjJSi1Lz03gYWNMSc4pTeaE0N4OCm2uIs4duakF-fGpxQWIy0JSSeNcAQwMLA0MjQ0dDYyKUAACUuyn1</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Polyethylene and method of production thereof</title><source>esp@cenet</source><creator>CLUTTON, EDWARD, QUENTIN ; HOPE, PHILIP, STEPHEN</creator><creatorcontrib>CLUTTON, EDWARD, QUENTIN ; HOPE, PHILIP, STEPHEN</creatorcontrib><description>Polyethylenes are prepared having a density in the range 900-980 kg/m3 and a weight average molecular weight &gt;=375,000 characterized by a fracture toughness at -40° C. &gt;20 kJ/m2 and a dynamic viscosity of &lt;3000 Pa.s at 100 rad/sec. The polymers also having a die swell of 10-80% and show a desirable combination of physical and processing properties. The polymers are prepared by the use of catalysts comprising a metallocene component and a Ziegler component.</description><edition>7</edition><language>eng ; fre ; ger</language><subject>AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F,C08G ; CHEMISTRY ; COMPOSITIONS BASED THEREON ; COMPOSITIONS OF MACROMOLECULAR COMPOUNDS ; GENERAL PROCESSES OF COMPOUNDING ; MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVINGCARBON-TO-CARBON UNSATURATED BONDS ; METALLURGY ; ORGANIC MACROMOLECULAR COMPOUNDS ; THEIR PREPARATION OR CHEMICAL WORKING-UP ; WORKING-UP</subject><creationdate>2001</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20010307&amp;DB=EPODOC&amp;CC=EP&amp;NR=1080121A1$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76290</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20010307&amp;DB=EPODOC&amp;CC=EP&amp;NR=1080121A1$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>CLUTTON, EDWARD, QUENTIN</creatorcontrib><creatorcontrib>HOPE, PHILIP, STEPHEN</creatorcontrib><title>Polyethylene and method of production thereof</title><description>Polyethylenes are prepared having a density in the range 900-980 kg/m3 and a weight average molecular weight &gt;=375,000 characterized by a fracture toughness at -40° C. &gt;20 kJ/m2 and a dynamic viscosity of &lt;3000 Pa.s at 100 rad/sec. The polymers also having a die swell of 10-80% and show a desirable combination of physical and processing properties. The polymers are prepared by the use of catalysts comprising a metallocene component and a Ziegler component.</description><subject>AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F,C08G</subject><subject>CHEMISTRY</subject><subject>COMPOSITIONS BASED THEREON</subject><subject>COMPOSITIONS OF MACROMOLECULAR COMPOUNDS</subject><subject>GENERAL PROCESSES OF COMPOUNDING</subject><subject>MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVINGCARBON-TO-CARBON UNSATURATED BONDS</subject><subject>METALLURGY</subject><subject>ORGANIC MACROMOLECULAR COMPOUNDS</subject><subject>THEIR PREPARATION OR CHEMICAL WORKING-UP</subject><subject>WORKING-UP</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2001</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZNANyM-pTC3JqMxJzUtVSMxLUcgF8vJTFPLTFAqK8lNKk0sy8_MUSjJSi1Lz03gYWNMSc4pTeaE0N4OCm2uIs4duakF-fGpxQWIy0JSSeNcAQwMLA0MjQ0dDYyKUAACUuyn1</recordid><startdate>20010307</startdate><enddate>20010307</enddate><creator>CLUTTON, EDWARD, QUENTIN</creator><creator>HOPE, PHILIP, STEPHEN</creator><scope>EVB</scope></search><sort><creationdate>20010307</creationdate><title>Polyethylene and method of production thereof</title><author>CLUTTON, EDWARD, QUENTIN ; HOPE, PHILIP, STEPHEN</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_EP1080121A13</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; fre ; ger</language><creationdate>2001</creationdate><topic>AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F,C08G</topic><topic>CHEMISTRY</topic><topic>COMPOSITIONS BASED THEREON</topic><topic>COMPOSITIONS OF MACROMOLECULAR COMPOUNDS</topic><topic>GENERAL PROCESSES OF COMPOUNDING</topic><topic>MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVINGCARBON-TO-CARBON UNSATURATED BONDS</topic><topic>METALLURGY</topic><topic>ORGANIC MACROMOLECULAR COMPOUNDS</topic><topic>THEIR PREPARATION OR CHEMICAL WORKING-UP</topic><topic>WORKING-UP</topic><toplevel>online_resources</toplevel><creatorcontrib>CLUTTON, EDWARD, QUENTIN</creatorcontrib><creatorcontrib>HOPE, PHILIP, STEPHEN</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>CLUTTON, EDWARD, QUENTIN</au><au>HOPE, PHILIP, STEPHEN</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Polyethylene and method of production thereof</title><date>2001-03-07</date><risdate>2001</risdate><abstract>Polyethylenes are prepared having a density in the range 900-980 kg/m3 and a weight average molecular weight &gt;=375,000 characterized by a fracture toughness at -40° C. &gt;20 kJ/m2 and a dynamic viscosity of &lt;3000 Pa.s at 100 rad/sec. The polymers also having a die swell of 10-80% and show a desirable combination of physical and processing properties. The polymers are prepared by the use of catalysts comprising a metallocene component and a Ziegler component.</abstract><edition>7</edition><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng ; fre ; ger
recordid cdi_epo_espacenet_EP1080121A1
source esp@cenet
subjects AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F,C08G
CHEMISTRY
COMPOSITIONS BASED THEREON
COMPOSITIONS OF MACROMOLECULAR COMPOUNDS
GENERAL PROCESSES OF COMPOUNDING
MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVINGCARBON-TO-CARBON UNSATURATED BONDS
METALLURGY
ORGANIC MACROMOLECULAR COMPOUNDS
THEIR PREPARATION OR CHEMICAL WORKING-UP
WORKING-UP
title Polyethylene and method of production thereof
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-30T16%3A27%3A59IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=CLUTTON,%20EDWARD,%20QUENTIN&rft.date=2001-03-07&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EEP1080121A1%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true