Process for the preparation of monoclinic zirconium dioxide with high surface area

At least 80 wt.% monoclinic zirconium dioxide comprises a BET surface area of NOTLESS 100 m /g. Also claimed are: (a) at least 80 wt.% monoclinic sulphated dioxide with a sulphate content of 0.05-10 wt.%, calculated as SO4, and BET surface area of NOTLESS 100 m /g; (b) methods of preparing the dioxi...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: STICHERT, WOLFRAM, WULFF-DOERING, JOACHIM, SCHUETH, FERDI, DR
Format: Patent
Sprache:eng ; fre ; ger
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:At least 80 wt.% monoclinic zirconium dioxide comprises a BET surface area of NOTLESS 100 m /g. Also claimed are: (a) at least 80 wt.% monoclinic sulphated dioxide with a sulphate content of 0.05-10 wt.%, calculated as SO4, and BET surface area of NOTLESS 100 m /g; (b) methods of preparing the dioxides; (c) zirconium dioxide prepared by these methods; (d) mouldings containing zirconium dioxide of these types; (e) the production of mouldings by pressing the zirconium dioxide; and (f) a catalyst with a support of zirconium dioxide of these types, doped with 0.1-20 wt.% catalytically active metal(s).