IMPROVED POLY(ARYLENE SULFIDE) AND METHOD OF MAKING, AND ARTICLE OF MANUFACTURE INCLUDING, THE SAME

An improved composite includes an improved polymer, specifically an improved poly(phenylene sulfide). The improved polymer is produced by an improved method including a polymerization phase, a recovery phase, a washing phase, and an optional air-curing phase. In the polymerization phase a low temper...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: YU, MICHAEL CHENU, JOHNSON, TIMOTHY WALTER, SOULES, DAVID ANDREW, GEIBEL, JON FREDERICK, SCOGGINS, LACEY EUGENE, STONE, MARK LEE, HAGENSON, RANDY LEE, REGISTER, DAVID FRANCIS
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator YU, MICHAEL CHENU
JOHNSON, TIMOTHY WALTER
SOULES, DAVID ANDREW
GEIBEL, JON FREDERICK
SCOGGINS, LACEY EUGENE
STONE, MARK LEE
HAGENSON, RANDY LEE
REGISTER, DAVID FRANCIS
description An improved composite includes an improved polymer, specifically an improved poly(phenylene sulfide). The improved polymer is produced by an improved method including a polymerization phase, a recovery phase, a washing phase, and an optional air-curing phase. In the polymerization phase a low temperature cycle and a high temperature cycle are used. In a preferred recovery phase, solidified polymer is quenched with N-methyl-2-pyrrolidone. In the washing phase, the recovered solidified polymer is washed with a hot acidic solution and then hot water. In a preferred embodiment, the method produces substantially linear poly(phenylene sulfide) having a melt flow within the range of about 50 to about 200 grams per 10 minutes and an ash content of not greater than about 0.1 weight percent and a melt crystallization temperature of not less than about 347 DEG F (175 DEG C).
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_EP0418455A3</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>EP0418455A3</sourcerecordid><originalsourceid>FETCH-epo_espacenet_EP0418455A33</originalsourceid><addsrcrecordid>eNqNjEsKwjAUALNxIeod3lJBQWkLbh_JiwnmU2IidFVKiSvRQr0_SvUArgaGYeas17YO_koCam-aNYbGkCO4JCO1oA2gE2ApKi_AS7B41u60nSyGqLmhr3ZJIo8pEGjHTRJTFdVnhJaWbHbr7mNe_bhgIClytcvDs83j0PX5kV8t1fvycCyrCovij-QNYZAzJg</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>IMPROVED POLY(ARYLENE SULFIDE) AND METHOD OF MAKING, AND ARTICLE OF MANUFACTURE INCLUDING, THE SAME</title><source>esp@cenet</source><creator>YU, MICHAEL CHENU ; JOHNSON, TIMOTHY WALTER ; SOULES, DAVID ANDREW ; GEIBEL, JON FREDERICK ; SCOGGINS, LACEY EUGENE ; STONE, MARK LEE ; HAGENSON, RANDY LEE ; REGISTER, DAVID FRANCIS</creator><creatorcontrib>YU, MICHAEL CHENU ; JOHNSON, TIMOTHY WALTER ; SOULES, DAVID ANDREW ; GEIBEL, JON FREDERICK ; SCOGGINS, LACEY EUGENE ; STONE, MARK LEE ; HAGENSON, RANDY LEE ; REGISTER, DAVID FRANCIS</creatorcontrib><description>An improved composite includes an improved polymer, specifically an improved poly(phenylene sulfide). The improved polymer is produced by an improved method including a polymerization phase, a recovery phase, a washing phase, and an optional air-curing phase. In the polymerization phase a low temperature cycle and a high temperature cycle are used. In a preferred recovery phase, solidified polymer is quenched with N-methyl-2-pyrrolidone. In the washing phase, the recovered solidified polymer is washed with a hot acidic solution and then hot water. In a preferred embodiment, the method produces substantially linear poly(phenylene sulfide) having a melt flow within the range of about 50 to about 200 grams per 10 minutes and an ash content of not greater than about 0.1 weight percent and a melt crystallization temperature of not less than about 347 DEG F (175 DEG C).</description><edition>5</edition><language>eng</language><subject>CHEMISTRY ; COMPOSITIONS BASED THEREON ; MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONSONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS ; METALLURGY ; ORGANIC MACROMOLECULAR COMPOUNDS ; THEIR PREPARATION OR CHEMICAL WORKING-UP</subject><creationdate>1991</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19911218&amp;DB=EPODOC&amp;CC=EP&amp;NR=0418455A3$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19911218&amp;DB=EPODOC&amp;CC=EP&amp;NR=0418455A3$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>YU, MICHAEL CHENU</creatorcontrib><creatorcontrib>JOHNSON, TIMOTHY WALTER</creatorcontrib><creatorcontrib>SOULES, DAVID ANDREW</creatorcontrib><creatorcontrib>GEIBEL, JON FREDERICK</creatorcontrib><creatorcontrib>SCOGGINS, LACEY EUGENE</creatorcontrib><creatorcontrib>STONE, MARK LEE</creatorcontrib><creatorcontrib>HAGENSON, RANDY LEE</creatorcontrib><creatorcontrib>REGISTER, DAVID FRANCIS</creatorcontrib><title>IMPROVED POLY(ARYLENE SULFIDE) AND METHOD OF MAKING, AND ARTICLE OF MANUFACTURE INCLUDING, THE SAME</title><description>An improved composite includes an improved polymer, specifically an improved poly(phenylene sulfide). The improved polymer is produced by an improved method including a polymerization phase, a recovery phase, a washing phase, and an optional air-curing phase. In the polymerization phase a low temperature cycle and a high temperature cycle are used. In a preferred recovery phase, solidified polymer is quenched with N-methyl-2-pyrrolidone. In the washing phase, the recovered solidified polymer is washed with a hot acidic solution and then hot water. In a preferred embodiment, the method produces substantially linear poly(phenylene sulfide) having a melt flow within the range of about 50 to about 200 grams per 10 minutes and an ash content of not greater than about 0.1 weight percent and a melt crystallization temperature of not less than about 347 DEG F (175 DEG C).</description><subject>CHEMISTRY</subject><subject>COMPOSITIONS BASED THEREON</subject><subject>MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONSONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS</subject><subject>METALLURGY</subject><subject>ORGANIC MACROMOLECULAR COMPOUNDS</subject><subject>THEIR PREPARATION OR CHEMICAL WORKING-UP</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>1991</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNjEsKwjAUALNxIeod3lJBQWkLbh_JiwnmU2IidFVKiSvRQr0_SvUArgaGYeas17YO_koCam-aNYbGkCO4JCO1oA2gE2ApKi_AS7B41u60nSyGqLmhr3ZJIo8pEGjHTRJTFdVnhJaWbHbr7mNe_bhgIClytcvDs83j0PX5kV8t1fvycCyrCovij-QNYZAzJg</recordid><startdate>19911218</startdate><enddate>19911218</enddate><creator>YU, MICHAEL CHENU</creator><creator>JOHNSON, TIMOTHY WALTER</creator><creator>SOULES, DAVID ANDREW</creator><creator>GEIBEL, JON FREDERICK</creator><creator>SCOGGINS, LACEY EUGENE</creator><creator>STONE, MARK LEE</creator><creator>HAGENSON, RANDY LEE</creator><creator>REGISTER, DAVID FRANCIS</creator><scope>EVB</scope></search><sort><creationdate>19911218</creationdate><title>IMPROVED POLY(ARYLENE SULFIDE) AND METHOD OF MAKING, AND ARTICLE OF MANUFACTURE INCLUDING, THE SAME</title><author>YU, MICHAEL CHENU ; JOHNSON, TIMOTHY WALTER ; SOULES, DAVID ANDREW ; GEIBEL, JON FREDERICK ; SCOGGINS, LACEY EUGENE ; STONE, MARK LEE ; HAGENSON, RANDY LEE ; REGISTER, DAVID FRANCIS</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_EP0418455A33</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>1991</creationdate><topic>CHEMISTRY</topic><topic>COMPOSITIONS BASED THEREON</topic><topic>MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONSONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS</topic><topic>METALLURGY</topic><topic>ORGANIC MACROMOLECULAR COMPOUNDS</topic><topic>THEIR PREPARATION OR CHEMICAL WORKING-UP</topic><toplevel>online_resources</toplevel><creatorcontrib>YU, MICHAEL CHENU</creatorcontrib><creatorcontrib>JOHNSON, TIMOTHY WALTER</creatorcontrib><creatorcontrib>SOULES, DAVID ANDREW</creatorcontrib><creatorcontrib>GEIBEL, JON FREDERICK</creatorcontrib><creatorcontrib>SCOGGINS, LACEY EUGENE</creatorcontrib><creatorcontrib>STONE, MARK LEE</creatorcontrib><creatorcontrib>HAGENSON, RANDY LEE</creatorcontrib><creatorcontrib>REGISTER, DAVID FRANCIS</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>YU, MICHAEL CHENU</au><au>JOHNSON, TIMOTHY WALTER</au><au>SOULES, DAVID ANDREW</au><au>GEIBEL, JON FREDERICK</au><au>SCOGGINS, LACEY EUGENE</au><au>STONE, MARK LEE</au><au>HAGENSON, RANDY LEE</au><au>REGISTER, DAVID FRANCIS</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>IMPROVED POLY(ARYLENE SULFIDE) AND METHOD OF MAKING, AND ARTICLE OF MANUFACTURE INCLUDING, THE SAME</title><date>1991-12-18</date><risdate>1991</risdate><abstract>An improved composite includes an improved polymer, specifically an improved poly(phenylene sulfide). The improved polymer is produced by an improved method including a polymerization phase, a recovery phase, a washing phase, and an optional air-curing phase. In the polymerization phase a low temperature cycle and a high temperature cycle are used. In a preferred recovery phase, solidified polymer is quenched with N-methyl-2-pyrrolidone. In the washing phase, the recovered solidified polymer is washed with a hot acidic solution and then hot water. In a preferred embodiment, the method produces substantially linear poly(phenylene sulfide) having a melt flow within the range of about 50 to about 200 grams per 10 minutes and an ash content of not greater than about 0.1 weight percent and a melt crystallization temperature of not less than about 347 DEG F (175 DEG C).</abstract><edition>5</edition><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_EP0418455A3
source esp@cenet
subjects CHEMISTRY
COMPOSITIONS BASED THEREON
MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONSONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
METALLURGY
ORGANIC MACROMOLECULAR COMPOUNDS
THEIR PREPARATION OR CHEMICAL WORKING-UP
title IMPROVED POLY(ARYLENE SULFIDE) AND METHOD OF MAKING, AND ARTICLE OF MANUFACTURE INCLUDING, THE SAME
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-26T14%3A21%3A36IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=YU,%20MICHAEL%20CHENU&rft.date=1991-12-18&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EEP0418455A3%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true