METHOD OF PREPARING CARRIER MATERIALS FOR OPTICAL SENSORS
Bodies of borosilicate glass with a B2O3 content of less than 13 percent by weight are provided with a microporous layer of a thickness of 5 to 20 mu m, and are thus turned into carriers for optical sensors. This process is characterized by the following steps. Thermal decomposition for 5 to 10 days...