IMPROVEMENTS IN OR RELATING TO GLASS MELTING TANKS AND TO REFRACTORY MATERIALS FOR USE THEREIN
The glass melting tank for supplying a flat glass forming process has a melting zone (12) for melting solid batch material (20) and a refining zone (13) with reduced return flow of glass. The base of the refining zone (13) comprises a fusion cast refractory material (30) comprising alumina, silica a...
Gespeichert in:
1. Verfasser: | |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | LYTHGOE, STANLEY |
description | The glass melting tank for supplying a flat glass forming process has a melting zone (12) for melting solid batch material (20) and a refining zone (13) with reduced return flow of glass. The base of the refining zone (13) comprises a fusion cast refractory material (30) comprising alumina, silica and between 31 % and 43% by weight of zirconia. The refractory is conditioned by oxidation at at least 1450° C for 24 hours. |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_EP0186972A3</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>EP0186972A3</sourcerecordid><originalsourceid>FETCH-epo_espacenet_EP0186972A33</originalsourceid><addsrcrecordid>eNqNi0sKwkAQBbNxIeod-gKCGlCzbGJPMjif0N0KbgxBxpVoIN4fFT2AqwdV9cbZ2fqG45E8BRWwASIDk0O1oQKNUDkUAU_uCzDsBTDsPorJMJYa-QQeldiiEzDv_0EItCYmG6bZ6NrdhjT77SQDQ1rW89Q_2jT03SXd07OlZrHcrovNCvP8j-QFwx4ylA</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>IMPROVEMENTS IN OR RELATING TO GLASS MELTING TANKS AND TO REFRACTORY MATERIALS FOR USE THEREIN</title><source>esp@cenet</source><creator>LYTHGOE, STANLEY</creator><creatorcontrib>LYTHGOE, STANLEY</creatorcontrib><description>The glass melting tank for supplying a flat glass forming process has a melting zone (12) for melting solid batch material (20) and a refining zone (13) with reduced return flow of glass. The base of the refining zone (13) comprises a fusion cast refractory material (30) comprising alumina, silica and between 31 % and 43% by weight of zirconia. The refractory is conditioned by oxidation at at least 1450° C for 24 hours.</description><edition>4</edition><language>eng</language><subject>ARTIFICIAL STONE ; CEMENTS ; CERAMICS ; CHEMISTRY ; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS ; CONCRETE ; GLASS ; LIME, MAGNESIA ; MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES ; METALLURGY ; MINERAL OR SLAG WOOL ; REFRACTORIES ; SLAG ; TREATMENT OF NATURAL STONE</subject><creationdate>1986</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=19861008&DB=EPODOC&CC=EP&NR=0186972A3$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76289</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=19861008&DB=EPODOC&CC=EP&NR=0186972A3$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>LYTHGOE, STANLEY</creatorcontrib><title>IMPROVEMENTS IN OR RELATING TO GLASS MELTING TANKS AND TO REFRACTORY MATERIALS FOR USE THEREIN</title><description>The glass melting tank for supplying a flat glass forming process has a melting zone (12) for melting solid batch material (20) and a refining zone (13) with reduced return flow of glass. The base of the refining zone (13) comprises a fusion cast refractory material (30) comprising alumina, silica and between 31 % and 43% by weight of zirconia. The refractory is conditioned by oxidation at at least 1450° C for 24 hours.</description><subject>ARTIFICIAL STONE</subject><subject>CEMENTS</subject><subject>CERAMICS</subject><subject>CHEMISTRY</subject><subject>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</subject><subject>CONCRETE</subject><subject>GLASS</subject><subject>LIME, MAGNESIA</subject><subject>MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES</subject><subject>METALLURGY</subject><subject>MINERAL OR SLAG WOOL</subject><subject>REFRACTORIES</subject><subject>SLAG</subject><subject>TREATMENT OF NATURAL STONE</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>1986</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNi0sKwkAQBbNxIeod-gKCGlCzbGJPMjif0N0KbgxBxpVoIN4fFT2AqwdV9cbZ2fqG45E8BRWwASIDk0O1oQKNUDkUAU_uCzDsBTDsPorJMJYa-QQeldiiEzDv_0EItCYmG6bZ6NrdhjT77SQDQ1rW89Q_2jT03SXd07OlZrHcrovNCvP8j-QFwx4ylA</recordid><startdate>19861008</startdate><enddate>19861008</enddate><creator>LYTHGOE, STANLEY</creator><scope>EVB</scope></search><sort><creationdate>19861008</creationdate><title>IMPROVEMENTS IN OR RELATING TO GLASS MELTING TANKS AND TO REFRACTORY MATERIALS FOR USE THEREIN</title><author>LYTHGOE, STANLEY</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_EP0186972A33</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>1986</creationdate><topic>ARTIFICIAL STONE</topic><topic>CEMENTS</topic><topic>CERAMICS</topic><topic>CHEMISTRY</topic><topic>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</topic><topic>CONCRETE</topic><topic>GLASS</topic><topic>LIME, MAGNESIA</topic><topic>MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES</topic><topic>METALLURGY</topic><topic>MINERAL OR SLAG WOOL</topic><topic>REFRACTORIES</topic><topic>SLAG</topic><topic>TREATMENT OF NATURAL STONE</topic><toplevel>online_resources</toplevel><creatorcontrib>LYTHGOE, STANLEY</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>LYTHGOE, STANLEY</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>IMPROVEMENTS IN OR RELATING TO GLASS MELTING TANKS AND TO REFRACTORY MATERIALS FOR USE THEREIN</title><date>1986-10-08</date><risdate>1986</risdate><abstract>The glass melting tank for supplying a flat glass forming process has a melting zone (12) for melting solid batch material (20) and a refining zone (13) with reduced return flow of glass. The base of the refining zone (13) comprises a fusion cast refractory material (30) comprising alumina, silica and between 31 % and 43% by weight of zirconia. The refractory is conditioned by oxidation at at least 1450° C for 24 hours.</abstract><edition>4</edition><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | eng |
recordid | cdi_epo_espacenet_EP0186972A3 |
source | esp@cenet |
subjects | ARTIFICIAL STONE CEMENTS CERAMICS CHEMISTRY COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS CONCRETE GLASS LIME, MAGNESIA MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES METALLURGY MINERAL OR SLAG WOOL REFRACTORIES SLAG TREATMENT OF NATURAL STONE |
title | IMPROVEMENTS IN OR RELATING TO GLASS MELTING TANKS AND TO REFRACTORY MATERIALS FOR USE THEREIN |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-09T20%3A09%3A39IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=LYTHGOE,%20STANLEY&rft.date=1986-10-08&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EEP0186972A3%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |