Process for producing needle-shaped highly coercive gamma-iron(III) oxide

Acicular gamma-iron(III) oxide of high coercive force is produced by reducing acicular nonmagnetic iron(III) oxides or oxide hydroxides at between 250 and 700 DEG C with a superheated vapour mixture of an organic compound which is decomposable within this temperature range in the presence of iron ox...