Beschädigungstolerantes Aluminiumlegierungsprodukt und Verfahren zu seiner Herstellung
The invention relates to a Product comprising an aluminium base alloy consisting of (in weight %): Cu3.8-4.9, Mg 1.2-1.8, Mn 0.1-0.9, Fe max. 0.12, Si max. 0.10, Ti max. 0.15, Zn max. 0.20, Cr max. 0.10, impurities each max. 0.05, total max. 0.15, balance aluminium, said product having a minimum L-0...
Gespeichert in:
Hauptverfasser: | , |
---|---|
Format: | Patent |
Sprache: | ger |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | HEINZ, LUDWIG HASZLER, JOHANN |
description | The invention relates to a Product comprising an aluminium base alloy consisting of (in weight %): Cu3.8-4.9, Mg 1.2-1.8, Mn 0.1-0.9, Fe max. 0.12, Si max. 0.10, Ti max. 0.15, Zn max. 0.20, Cr max. 0.10, impurities each max. 0.05, total max. 0.15, balance aluminium, said product having a minimum L-0.2 % yield strength of 300 MPa or more, a minimum LT-0.2 % yield strength of 270 MPa, a minimum T-L fracture toughness KC(ao) of 100 MPa. 2ROOT m or more for a 700 mm wide CCT-panel, and having in both L/ST- and LT/ST-sections an average grain size of at least 6 according to ASTM E-112. Further the invention relates to a method for the manufacturing of such a product. |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_DE69915365TT2</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>DE69915365TT2</sourcerecordid><originalsourceid>FETCH-epo_espacenet_DE69915365TT23</originalsourceid><addsrcrecordid>eNqNyjEOgjAUh_EuDka9Q-PuoAQSRlQMB2h0JA38gcbyIO-1i-fxJl5MTTyA0zd8v6W6HSHN8Hq2ro_US5g82FKA6MLH0ZGLo0fvwN8789TGe9CRWn0Fd3ZgkH5ELXAE1hVYArz_2LVadNYLNr-u1PZSmlO1wzzVkNk2IIT6XGZ5vk-TLDXmkPyF3kQJPTE</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Beschädigungstolerantes Aluminiumlegierungsprodukt und Verfahren zu seiner Herstellung</title><source>esp@cenet</source><creator>HEINZ, LUDWIG ; HASZLER, JOHANN</creator><creatorcontrib>HEINZ, LUDWIG ; HASZLER, JOHANN</creatorcontrib><description>The invention relates to a Product comprising an aluminium base alloy consisting of (in weight %): Cu3.8-4.9, Mg 1.2-1.8, Mn 0.1-0.9, Fe max. 0.12, Si max. 0.10, Ti max. 0.15, Zn max. 0.20, Cr max. 0.10, impurities each max. 0.05, total max. 0.15, balance aluminium, said product having a minimum L-0.2 % yield strength of 300 MPa or more, a minimum LT-0.2 % yield strength of 270 MPa, a minimum T-L fracture toughness KC(ao) of 100 MPa. 2ROOT m or more for a 700 mm wide CCT-panel, and having in both L/ST- and LT/ST-sections an average grain size of at least 6 according to ASTM E-112. Further the invention relates to a method for the manufacturing of such a product.</description><edition>7</edition><language>ger</language><subject>ALLOYS ; CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS ANDNON-FERROUS ALLOYS ; CHEMISTRY ; FERROUS OR NON-FERROUS ALLOYS ; LAYERED PRODUCTS ; LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT ORNON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM ; MECHANICAL METAL-WORKING WITHOUT ESSENTIALLY REMOVINGMATERIAL ; METALLURGY ; PERFORMING OPERATIONS ; PUNCHING METAL ; ROLLING OF METAL ; TRANSPORTING ; TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><creationdate>2005</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20050217&DB=EPODOC&CC=DE&NR=69915365T2$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20050217&DB=EPODOC&CC=DE&NR=69915365T2$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>HEINZ, LUDWIG</creatorcontrib><creatorcontrib>HASZLER, JOHANN</creatorcontrib><title>Beschädigungstolerantes Aluminiumlegierungsprodukt und Verfahren zu seiner Herstellung</title><description>The invention relates to a Product comprising an aluminium base alloy consisting of (in weight %): Cu3.8-4.9, Mg 1.2-1.8, Mn 0.1-0.9, Fe max. 0.12, Si max. 0.10, Ti max. 0.15, Zn max. 0.20, Cr max. 0.10, impurities each max. 0.05, total max. 0.15, balance aluminium, said product having a minimum L-0.2 % yield strength of 300 MPa or more, a minimum LT-0.2 % yield strength of 270 MPa, a minimum T-L fracture toughness KC(ao) of 100 MPa. 2ROOT m or more for a 700 mm wide CCT-panel, and having in both L/ST- and LT/ST-sections an average grain size of at least 6 according to ASTM E-112. Further the invention relates to a method for the manufacturing of such a product.</description><subject>ALLOYS</subject><subject>CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS ANDNON-FERROUS ALLOYS</subject><subject>CHEMISTRY</subject><subject>FERROUS OR NON-FERROUS ALLOYS</subject><subject>LAYERED PRODUCTS</subject><subject>LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT ORNON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM</subject><subject>MECHANICAL METAL-WORKING WITHOUT ESSENTIALLY REMOVINGMATERIAL</subject><subject>METALLURGY</subject><subject>PERFORMING OPERATIONS</subject><subject>PUNCHING METAL</subject><subject>ROLLING OF METAL</subject><subject>TRANSPORTING</subject><subject>TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2005</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNyjEOgjAUh_EuDka9Q-PuoAQSRlQMB2h0JA38gcbyIO-1i-fxJl5MTTyA0zd8v6W6HSHN8Hq2ro_US5g82FKA6MLH0ZGLo0fvwN8789TGe9CRWn0Fd3ZgkH5ELXAE1hVYArz_2LVadNYLNr-u1PZSmlO1wzzVkNk2IIT6XGZ5vk-TLDXmkPyF3kQJPTE</recordid><startdate>20050217</startdate><enddate>20050217</enddate><creator>HEINZ, LUDWIG</creator><creator>HASZLER, JOHANN</creator><scope>EVB</scope></search><sort><creationdate>20050217</creationdate><title>Beschädigungstolerantes Aluminiumlegierungsprodukt und Verfahren zu seiner Herstellung</title><author>HEINZ, LUDWIG ; HASZLER, JOHANN</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_DE69915365TT23</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>ger</language><creationdate>2005</creationdate><topic>ALLOYS</topic><topic>CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS ANDNON-FERROUS ALLOYS</topic><topic>CHEMISTRY</topic><topic>FERROUS OR NON-FERROUS ALLOYS</topic><topic>LAYERED PRODUCTS</topic><topic>LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT ORNON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM</topic><topic>MECHANICAL METAL-WORKING WITHOUT ESSENTIALLY REMOVINGMATERIAL</topic><topic>METALLURGY</topic><topic>PERFORMING OPERATIONS</topic><topic>PUNCHING METAL</topic><topic>ROLLING OF METAL</topic><topic>TRANSPORTING</topic><topic>TREATMENT OF ALLOYS OR NON-FERROUS METALS</topic><toplevel>online_resources</toplevel><creatorcontrib>HEINZ, LUDWIG</creatorcontrib><creatorcontrib>HASZLER, JOHANN</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>HEINZ, LUDWIG</au><au>HASZLER, JOHANN</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Beschädigungstolerantes Aluminiumlegierungsprodukt und Verfahren zu seiner Herstellung</title><date>2005-02-17</date><risdate>2005</risdate><abstract>The invention relates to a Product comprising an aluminium base alloy consisting of (in weight %): Cu3.8-4.9, Mg 1.2-1.8, Mn 0.1-0.9, Fe max. 0.12, Si max. 0.10, Ti max. 0.15, Zn max. 0.20, Cr max. 0.10, impurities each max. 0.05, total max. 0.15, balance aluminium, said product having a minimum L-0.2 % yield strength of 300 MPa or more, a minimum LT-0.2 % yield strength of 270 MPa, a minimum T-L fracture toughness KC(ao) of 100 MPa. 2ROOT m or more for a 700 mm wide CCT-panel, and having in both L/ST- and LT/ST-sections an average grain size of at least 6 according to ASTM E-112. Further the invention relates to a method for the manufacturing of such a product.</abstract><edition>7</edition><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | ger |
recordid | cdi_epo_espacenet_DE69915365TT2 |
source | esp@cenet |
subjects | ALLOYS CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS ANDNON-FERROUS ALLOYS CHEMISTRY FERROUS OR NON-FERROUS ALLOYS LAYERED PRODUCTS LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT ORNON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM MECHANICAL METAL-WORKING WITHOUT ESSENTIALLY REMOVINGMATERIAL METALLURGY PERFORMING OPERATIONS PUNCHING METAL ROLLING OF METAL TRANSPORTING TREATMENT OF ALLOYS OR NON-FERROUS METALS |
title | Beschädigungstolerantes Aluminiumlegierungsprodukt und Verfahren zu seiner Herstellung |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-04T13%3A52%3A15IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=HEINZ,%20LUDWIG&rft.date=2005-02-17&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EDE69915365TT2%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |