Fe-Mn Stahl mit guten Schwingungsdämpfungseigenschaften und Verfahren zu dessen Herstellung
An Fe-Mn vibration damping alloy steel having a mixture structure of epsilon , alpha ' and gamma . The alloy steel consists of iron, manganese from 10 to 24 % by weight and limited amounts of impurities. The alloy steel is manufactured by preparing an ingot at a temperature of 1000 DEG C to 130...
Gespeichert in:
Hauptverfasser: | , , , , , , |
---|---|
Format: | Patent |
Sprache: | ger |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | JUN, JOONG-HWAN, KANGNAM-KU, SEOUL, KR KO, YOUNG-SAM, DOBONG-KU, SEOUL, KR SON, YONGUL, SUNGNAM-SI, KYUNGKI-DO, KR KIM, JEONGOL, SEOUL, KR LEE, MAN-EOB, KWACHUN-SI, KYUNGKI-DO, KR BAEK, SEUNG-HAN, SUNGNAM-SI, KYUNGKI-DO, KR CHOI, CHONG-SOOL, MAPO-KU, SEOUL, KR |
description | An Fe-Mn vibration damping alloy steel having a mixture structure of epsilon , alpha ' and gamma . The alloy steel consists of iron, manganese from 10 to 24 % by weight and limited amounts of impurities. The alloy steel is manufactured by preparing an ingot at a temperature of 1000 DEG C to 1300 DEG C for 12 to 40 hours to homogenize the ingot and hot-rolling the homogenized ingot to produce a rolled alloy bar or plate, performing solid solution treatment on the alloy steel at 900 DEG C to 1100 DEG C for 30 to 60 minutes, cooling the alloy steel by air or water, and cold-rolling the alloy steel at a reduction rate of below 30 % at around room temperature. |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_DE69408773TT2</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>DE69408773TT2</sourcerecordid><originalsourceid>FETCH-epo_espacenet_DE69408773TT23</originalsourceid><addsrcrecordid>eNrjZIhxS9X1zVMILknMyFHIzSxRSC8tSQXykzPKM_PSS_PSi1MOL8ktSAOxUjPTU_OKkzMS00BKSvNSFMJSi9ISM4qAvKpShZTU4mIgyyO1qLgkNScHqIOHgTUtMac4lRdKczMoubmGOHvophbkx6cWFyQmp-allsS7uJpZmhhYmJsbh4QYGROlCAC23D3Q</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Fe-Mn Stahl mit guten Schwingungsdämpfungseigenschaften und Verfahren zu dessen Herstellung</title><source>esp@cenet</source><creator>JUN, JOONG-HWAN, KANGNAM-KU, SEOUL, KR ; KO, YOUNG-SAM, DOBONG-KU, SEOUL, KR ; SON, YONGUL, SUNGNAM-SI, KYUNGKI-DO, KR ; KIM, JEONGOL, SEOUL, KR ; LEE, MAN-EOB, KWACHUN-SI, KYUNGKI-DO, KR ; BAEK, SEUNG-HAN, SUNGNAM-SI, KYUNGKI-DO, KR ; CHOI, CHONG-SOOL, MAPO-KU, SEOUL, KR</creator><creatorcontrib>JUN, JOONG-HWAN, KANGNAM-KU, SEOUL, KR ; KO, YOUNG-SAM, DOBONG-KU, SEOUL, KR ; SON, YONGUL, SUNGNAM-SI, KYUNGKI-DO, KR ; KIM, JEONGOL, SEOUL, KR ; LEE, MAN-EOB, KWACHUN-SI, KYUNGKI-DO, KR ; BAEK, SEUNG-HAN, SUNGNAM-SI, KYUNGKI-DO, KR ; CHOI, CHONG-SOOL, MAPO-KU, SEOUL, KR</creatorcontrib><description>An Fe-Mn vibration damping alloy steel having a mixture structure of epsilon , alpha ' and gamma . The alloy steel consists of iron, manganese from 10 to 24 % by weight and limited amounts of impurities. The alloy steel is manufactured by preparing an ingot at a temperature of 1000 DEG C to 1300 DEG C for 12 to 40 hours to homogenize the ingot and hot-rolling the homogenized ingot to produce a rolled alloy bar or plate, performing solid solution treatment on the alloy steel at 900 DEG C to 1100 DEG C for 30 to 60 minutes, cooling the alloy steel by air or water, and cold-rolling the alloy steel at a reduction rate of below 30 % at around room temperature.</description><edition>6</edition><language>ger</language><subject>ALLOYS ; CHEMISTRY ; FERROUS OR NON-FERROUS ALLOYS ; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS ; MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS ; METALLURGY ; METALLURGY OF IRON ; MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS ; TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><creationdate>1998</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=19980813&DB=EPODOC&CC=DE&NR=69408773T2$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76516</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=19980813&DB=EPODOC&CC=DE&NR=69408773T2$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>JUN, JOONG-HWAN, KANGNAM-KU, SEOUL, KR</creatorcontrib><creatorcontrib>KO, YOUNG-SAM, DOBONG-KU, SEOUL, KR</creatorcontrib><creatorcontrib>SON, YONGUL, SUNGNAM-SI, KYUNGKI-DO, KR</creatorcontrib><creatorcontrib>KIM, JEONGOL, SEOUL, KR</creatorcontrib><creatorcontrib>LEE, MAN-EOB, KWACHUN-SI, KYUNGKI-DO, KR</creatorcontrib><creatorcontrib>BAEK, SEUNG-HAN, SUNGNAM-SI, KYUNGKI-DO, KR</creatorcontrib><creatorcontrib>CHOI, CHONG-SOOL, MAPO-KU, SEOUL, KR</creatorcontrib><title>Fe-Mn Stahl mit guten Schwingungsdämpfungseigenschaften und Verfahren zu dessen Herstellung</title><description>An Fe-Mn vibration damping alloy steel having a mixture structure of epsilon , alpha ' and gamma . The alloy steel consists of iron, manganese from 10 to 24 % by weight and limited amounts of impurities. The alloy steel is manufactured by preparing an ingot at a temperature of 1000 DEG C to 1300 DEG C for 12 to 40 hours to homogenize the ingot and hot-rolling the homogenized ingot to produce a rolled alloy bar or plate, performing solid solution treatment on the alloy steel at 900 DEG C to 1100 DEG C for 30 to 60 minutes, cooling the alloy steel by air or water, and cold-rolling the alloy steel at a reduction rate of below 30 % at around room temperature.</description><subject>ALLOYS</subject><subject>CHEMISTRY</subject><subject>FERROUS OR NON-FERROUS ALLOYS</subject><subject>GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS</subject><subject>MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS</subject><subject>METALLURGY</subject><subject>METALLURGY OF IRON</subject><subject>MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS</subject><subject>TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>1998</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZIhxS9X1zVMILknMyFHIzSxRSC8tSQXykzPKM_PSS_PSi1MOL8ktSAOxUjPTU_OKkzMS00BKSvNSFMJSi9ISM4qAvKpShZTU4mIgyyO1qLgkNScHqIOHgTUtMac4lRdKczMoubmGOHvophbkx6cWFyQmp-allsS7uJpZmhhYmJsbh4QYGROlCAC23D3Q</recordid><startdate>19980813</startdate><enddate>19980813</enddate><creator>JUN, JOONG-HWAN, KANGNAM-KU, SEOUL, KR</creator><creator>KO, YOUNG-SAM, DOBONG-KU, SEOUL, KR</creator><creator>SON, YONGUL, SUNGNAM-SI, KYUNGKI-DO, KR</creator><creator>KIM, JEONGOL, SEOUL, KR</creator><creator>LEE, MAN-EOB, KWACHUN-SI, KYUNGKI-DO, KR</creator><creator>BAEK, SEUNG-HAN, SUNGNAM-SI, KYUNGKI-DO, KR</creator><creator>CHOI, CHONG-SOOL, MAPO-KU, SEOUL, KR</creator><scope>EVB</scope></search><sort><creationdate>19980813</creationdate><title>Fe-Mn Stahl mit guten Schwingungsdämpfungseigenschaften und Verfahren zu dessen Herstellung</title><author>JUN, JOONG-HWAN, KANGNAM-KU, SEOUL, KR ; KO, YOUNG-SAM, DOBONG-KU, SEOUL, KR ; SON, YONGUL, SUNGNAM-SI, KYUNGKI-DO, KR ; KIM, JEONGOL, SEOUL, KR ; LEE, MAN-EOB, KWACHUN-SI, KYUNGKI-DO, KR ; BAEK, SEUNG-HAN, SUNGNAM-SI, KYUNGKI-DO, KR ; CHOI, CHONG-SOOL, MAPO-KU, SEOUL, KR</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_DE69408773TT23</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>ger</language><creationdate>1998</creationdate><topic>ALLOYS</topic><topic>CHEMISTRY</topic><topic>FERROUS OR NON-FERROUS ALLOYS</topic><topic>GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS</topic><topic>MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS</topic><topic>METALLURGY</topic><topic>METALLURGY OF IRON</topic><topic>MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS</topic><topic>TREATMENT OF ALLOYS OR NON-FERROUS METALS</topic><toplevel>online_resources</toplevel><creatorcontrib>JUN, JOONG-HWAN, KANGNAM-KU, SEOUL, KR</creatorcontrib><creatorcontrib>KO, YOUNG-SAM, DOBONG-KU, SEOUL, KR</creatorcontrib><creatorcontrib>SON, YONGUL, SUNGNAM-SI, KYUNGKI-DO, KR</creatorcontrib><creatorcontrib>KIM, JEONGOL, SEOUL, KR</creatorcontrib><creatorcontrib>LEE, MAN-EOB, KWACHUN-SI, KYUNGKI-DO, KR</creatorcontrib><creatorcontrib>BAEK, SEUNG-HAN, SUNGNAM-SI, KYUNGKI-DO, KR</creatorcontrib><creatorcontrib>CHOI, CHONG-SOOL, MAPO-KU, SEOUL, KR</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>JUN, JOONG-HWAN, KANGNAM-KU, SEOUL, KR</au><au>KO, YOUNG-SAM, DOBONG-KU, SEOUL, KR</au><au>SON, YONGUL, SUNGNAM-SI, KYUNGKI-DO, KR</au><au>KIM, JEONGOL, SEOUL, KR</au><au>LEE, MAN-EOB, KWACHUN-SI, KYUNGKI-DO, KR</au><au>BAEK, SEUNG-HAN, SUNGNAM-SI, KYUNGKI-DO, KR</au><au>CHOI, CHONG-SOOL, MAPO-KU, SEOUL, KR</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Fe-Mn Stahl mit guten Schwingungsdämpfungseigenschaften und Verfahren zu dessen Herstellung</title><date>1998-08-13</date><risdate>1998</risdate><abstract>An Fe-Mn vibration damping alloy steel having a mixture structure of epsilon , alpha ' and gamma . The alloy steel consists of iron, manganese from 10 to 24 % by weight and limited amounts of impurities. The alloy steel is manufactured by preparing an ingot at a temperature of 1000 DEG C to 1300 DEG C for 12 to 40 hours to homogenize the ingot and hot-rolling the homogenized ingot to produce a rolled alloy bar or plate, performing solid solution treatment on the alloy steel at 900 DEG C to 1100 DEG C for 30 to 60 minutes, cooling the alloy steel by air or water, and cold-rolling the alloy steel at a reduction rate of below 30 % at around room temperature.</abstract><edition>6</edition><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | ger |
recordid | cdi_epo_espacenet_DE69408773TT2 |
source | esp@cenet |
subjects | ALLOYS CHEMISTRY FERROUS OR NON-FERROUS ALLOYS GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS METALLURGY METALLURGY OF IRON MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS TREATMENT OF ALLOYS OR NON-FERROUS METALS |
title | Fe-Mn Stahl mit guten Schwingungsdämpfungseigenschaften und Verfahren zu dessen Herstellung |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-13T12%3A09%3A16IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=JUN,%20JOONG-HWAN,%20KANGNAM-KU,%20SEOUL,%20KR&rft.date=1998-08-13&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EDE69408773TT2%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |