Verfahren zur Vorbereitung von Metalloberflächen für das Emaillieren

A metal surface comprising iron is contacted with an aqueous phosphating solution comprising nickel ions and having a pH in the range 4.0 to 5.5, to form a coating comprising iron phosphate and nickel phosphate. An enamel frit is subsequently applied to the coated surface and is fired. The phosphati...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: LYONS, TERENCE JOHN, WHISTON, MERSEYSIDE, GB, CATTON, RONALD WILLIAM, PRINCESS RISBOROUGH, BUCKINGHAMSHIRE, GB
Format: Patent
Sprache:ger
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator LYONS, TERENCE JOHN, WHISTON, MERSEYSIDE, GB
CATTON, RONALD WILLIAM, PRINCESS RISBOROUGH, BUCKINGHAMSHIRE, GB
description A metal surface comprising iron is contacted with an aqueous phosphating solution comprising nickel ions and having a pH in the range 4.0 to 5.5, to form a coating comprising iron phosphate and nickel phosphate. An enamel frit is subsequently applied to the coated surface and is fired. The phosphating solution may contain an accelerator such as a fluoride in an amount up to 0.5 g/l and the nickel ions are preferably present in an amount 0.1-2.0 g/l and the phosphate ions in an amount 1-12 g/l. The enamel may be concentrated and is applied by conventional methods. A particular solid composition for use in forming the phosphating solution when dissolved in water comprises a mixture of an alkali metal or ammonium dihydrogen phosphate and a water-soluble inorganic nickel salt and optionally an alkali, a surfactant and/or an accelerator.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_DE3635896C2</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>DE3635896C2</sourcerecordid><originalsourceid>FETCH-epo_espacenet_DE3635896C23</originalsourceid><addsrcrecordid>eNrjZHALSy1KS8woSs1TqCotUgjLL0pKLUrNLCnNS1coy89T8E0tSczJyQcKpuUcXpKcAVSXdnhPkUJKYrGCa25iZk5OJlB9Hg8Da1piTnEqL5TmZlBwcw1x9tBNLciPTy0uSExOzUstiXdxNTYzNrWwNHM2MiZCCQCGmjTY</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Verfahren zur Vorbereitung von Metalloberflächen für das Emaillieren</title><source>esp@cenet</source><creator>LYONS, TERENCE JOHN, WHISTON, MERSEYSIDE, GB ; CATTON, RONALD WILLIAM, PRINCESS RISBOROUGH, BUCKINGHAMSHIRE, GB</creator><creatorcontrib>LYONS, TERENCE JOHN, WHISTON, MERSEYSIDE, GB ; CATTON, RONALD WILLIAM, PRINCESS RISBOROUGH, BUCKINGHAMSHIRE, GB</creatorcontrib><description>A metal surface comprising iron is contacted with an aqueous phosphating solution comprising nickel ions and having a pH in the range 4.0 to 5.5, to form a coating comprising iron phosphate and nickel phosphate. An enamel frit is subsequently applied to the coated surface and is fired. The phosphating solution may contain an accelerator such as a fluoride in an amount up to 0.5 g/l and the nickel ions are preferably present in an amount 0.1-2.0 g/l and the phosphate ions in an amount 1-12 g/l. The enamel may be concentrated and is applied by conventional methods. A particular solid composition for use in forming the phosphating solution when dissolved in water comprises a mixture of an alkali metal or ammonium dihydrogen phosphate and a water-soluble inorganic nickel salt and optionally an alkali, a surfactant and/or an accelerator.</description><edition>4</edition><language>ger</language><subject>CHEMICAL SURFACE TREATMENT ; CHEMISTRY ; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATIONOR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL ; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY IONIMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL ; COATING MATERIAL WITH METALLIC MATERIAL ; COATING METALLIC MATERIAL ; DIFFUSION TREATMENT OF METALLIC MATERIAL ; ENAMELLING OF, OR APPLYING A VITREOUS LAYER TO, METALS ; INHIBITING CORROSION OF METALLIC MATERIAL OR INCRUSTATION INGENERAL ; METALLURGY ; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THESURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION</subject><creationdate>1996</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19960222&amp;DB=EPODOC&amp;CC=DE&amp;NR=3635896C2$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19960222&amp;DB=EPODOC&amp;CC=DE&amp;NR=3635896C2$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>LYONS, TERENCE JOHN, WHISTON, MERSEYSIDE, GB</creatorcontrib><creatorcontrib>CATTON, RONALD WILLIAM, PRINCESS RISBOROUGH, BUCKINGHAMSHIRE, GB</creatorcontrib><title>Verfahren zur Vorbereitung von Metalloberflächen für das Emaillieren</title><description>A metal surface comprising iron is contacted with an aqueous phosphating solution comprising nickel ions and having a pH in the range 4.0 to 5.5, to form a coating comprising iron phosphate and nickel phosphate. An enamel frit is subsequently applied to the coated surface and is fired. The phosphating solution may contain an accelerator such as a fluoride in an amount up to 0.5 g/l and the nickel ions are preferably present in an amount 0.1-2.0 g/l and the phosphate ions in an amount 1-12 g/l. The enamel may be concentrated and is applied by conventional methods. A particular solid composition for use in forming the phosphating solution when dissolved in water comprises a mixture of an alkali metal or ammonium dihydrogen phosphate and a water-soluble inorganic nickel salt and optionally an alkali, a surfactant and/or an accelerator.</description><subject>CHEMICAL SURFACE TREATMENT</subject><subject>CHEMISTRY</subject><subject>COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATIONOR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL</subject><subject>COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY IONIMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL</subject><subject>COATING MATERIAL WITH METALLIC MATERIAL</subject><subject>COATING METALLIC MATERIAL</subject><subject>DIFFUSION TREATMENT OF METALLIC MATERIAL</subject><subject>ENAMELLING OF, OR APPLYING A VITREOUS LAYER TO, METALS</subject><subject>INHIBITING CORROSION OF METALLIC MATERIAL OR INCRUSTATION INGENERAL</subject><subject>METALLURGY</subject><subject>SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THESURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>1996</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZHALSy1KS8woSs1TqCotUgjLL0pKLUrNLCnNS1coy89T8E0tSczJyQcKpuUcXpKcAVSXdnhPkUJKYrGCa25iZk5OJlB9Hg8Da1piTnEqL5TmZlBwcw1x9tBNLciPTy0uSExOzUstiXdxNTYzNrWwNHM2MiZCCQCGmjTY</recordid><startdate>19960222</startdate><enddate>19960222</enddate><creator>LYONS, TERENCE JOHN, WHISTON, MERSEYSIDE, GB</creator><creator>CATTON, RONALD WILLIAM, PRINCESS RISBOROUGH, BUCKINGHAMSHIRE, GB</creator><scope>EVB</scope></search><sort><creationdate>19960222</creationdate><title>Verfahren zur Vorbereitung von Metalloberflächen für das Emaillieren</title><author>LYONS, TERENCE JOHN, WHISTON, MERSEYSIDE, GB ; CATTON, RONALD WILLIAM, PRINCESS RISBOROUGH, BUCKINGHAMSHIRE, GB</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_DE3635896C23</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>ger</language><creationdate>1996</creationdate><topic>CHEMICAL SURFACE TREATMENT</topic><topic>CHEMISTRY</topic><topic>COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATIONOR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL</topic><topic>COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY IONIMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL</topic><topic>COATING MATERIAL WITH METALLIC MATERIAL</topic><topic>COATING METALLIC MATERIAL</topic><topic>DIFFUSION TREATMENT OF METALLIC MATERIAL</topic><topic>ENAMELLING OF, OR APPLYING A VITREOUS LAYER TO, METALS</topic><topic>INHIBITING CORROSION OF METALLIC MATERIAL OR INCRUSTATION INGENERAL</topic><topic>METALLURGY</topic><topic>SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THESURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION</topic><toplevel>online_resources</toplevel><creatorcontrib>LYONS, TERENCE JOHN, WHISTON, MERSEYSIDE, GB</creatorcontrib><creatorcontrib>CATTON, RONALD WILLIAM, PRINCESS RISBOROUGH, BUCKINGHAMSHIRE, GB</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>LYONS, TERENCE JOHN, WHISTON, MERSEYSIDE, GB</au><au>CATTON, RONALD WILLIAM, PRINCESS RISBOROUGH, BUCKINGHAMSHIRE, GB</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Verfahren zur Vorbereitung von Metalloberflächen für das Emaillieren</title><date>1996-02-22</date><risdate>1996</risdate><abstract>A metal surface comprising iron is contacted with an aqueous phosphating solution comprising nickel ions and having a pH in the range 4.0 to 5.5, to form a coating comprising iron phosphate and nickel phosphate. An enamel frit is subsequently applied to the coated surface and is fired. The phosphating solution may contain an accelerator such as a fluoride in an amount up to 0.5 g/l and the nickel ions are preferably present in an amount 0.1-2.0 g/l and the phosphate ions in an amount 1-12 g/l. The enamel may be concentrated and is applied by conventional methods. A particular solid composition for use in forming the phosphating solution when dissolved in water comprises a mixture of an alkali metal or ammonium dihydrogen phosphate and a water-soluble inorganic nickel salt and optionally an alkali, a surfactant and/or an accelerator.</abstract><edition>4</edition><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language ger
recordid cdi_epo_espacenet_DE3635896C2
source esp@cenet
subjects CHEMICAL SURFACE TREATMENT
CHEMISTRY
COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATIONOR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL
COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY IONIMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL
COATING MATERIAL WITH METALLIC MATERIAL
COATING METALLIC MATERIAL
DIFFUSION TREATMENT OF METALLIC MATERIAL
ENAMELLING OF, OR APPLYING A VITREOUS LAYER TO, METALS
INHIBITING CORROSION OF METALLIC MATERIAL OR INCRUSTATION INGENERAL
METALLURGY
SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THESURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION
title Verfahren zur Vorbereitung von Metalloberflächen für das Emaillieren
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-03T05%3A00%3A57IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=LYONS,%20TERENCE%20JOHN,%20WHISTON,%20MERSEYSIDE,%20GB&rft.date=1996-02-22&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EDE3635896C2%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true