KUNSTHARZ-FORMKOERPER UND VERFAHREN ZU IHRER HERSTELLUNG

Novel resin products produced by reacting unique polycyclic, aromatic, polycarboxylic acid products with low molecular weight polyols display satisfactory toughness properties and good Barcol hardness values. The process for preparing these novel resin products first involves preparing an intimate,...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: G. SCHULZ,JOHANN, P. BARIE,JR,WALTER, T. EURICH,JAMES
Format: Patent
Sprache:ger
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator G. SCHULZ,JOHANN
P. BARIE,JR,WALTER
T. EURICH,JAMES
description Novel resin products produced by reacting unique polycyclic, aromatic, polycarboxylic acid products with low molecular weight polyols display satisfactory toughness properties and good Barcol hardness values. The process for preparing these novel resin products first involves preparing an intimate, finely divided mixture comprising the acid product derived from the nitric acid oxidation of naturally occurring solid carbonaceous material, a roughly equivalent amount of a liquid polyol, and a suitable acid catalyst. The mixture is then subjected to a precure step which involves heating at temperatures between 80 DEG and 150 DEG C. for from about fifteen minutes to about four hours. The precured mixture may thereafter be subjected to suitable molding conditions at a temperature below about 220 DEG C.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_DE3309894A1</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>DE3309894A1</sourcerecordid><originalsourceid>FETCH-epo_espacenet_DE3309894A13</originalsourceid><addsrcrecordid>eNrjZLDwDvULDvFwDIrSdfMP8vX2dw0KcA1SCPVzUQhzDXJz9Ahy9VOIClXwBDKCFDxcg4JDXH18Qv3ceRhY0xJzilN5oTQ3g4Kba4izh25qQX58anFBYnJqXmpJvIursbGBpYWliaOhMRFKAFe4KJg</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>KUNSTHARZ-FORMKOERPER UND VERFAHREN ZU IHRER HERSTELLUNG</title><source>esp@cenet</source><creator>G. SCHULZ,JOHANN ; P. BARIE,JR,WALTER ; T. EURICH,JAMES</creator><creatorcontrib>G. SCHULZ,JOHANN ; P. BARIE,JR,WALTER ; T. EURICH,JAMES</creatorcontrib><description>Novel resin products produced by reacting unique polycyclic, aromatic, polycarboxylic acid products with low molecular weight polyols display satisfactory toughness properties and good Barcol hardness values. The process for preparing these novel resin products first involves preparing an intimate, finely divided mixture comprising the acid product derived from the nitric acid oxidation of naturally occurring solid carbonaceous material, a roughly equivalent amount of a liquid polyol, and a suitable acid catalyst. The mixture is then subjected to a precure step which involves heating at temperatures between 80 DEG and 150 DEG C. for from about fifteen minutes to about four hours. The precured mixture may thereafter be subjected to suitable molding conditions at a temperature below about 220 DEG C.</description><language>ger</language><subject>CHEMISTRY ; COMPOSITIONS BASED THEREON ; MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONSONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS ; METALLURGY ; ORGANIC MACROMOLECULAR COMPOUNDS ; THEIR PREPARATION OR CHEMICAL WORKING-UP</subject><creationdate>1984</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19840920&amp;DB=EPODOC&amp;CC=DE&amp;NR=3309894A1$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25544,76293</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19840920&amp;DB=EPODOC&amp;CC=DE&amp;NR=3309894A1$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>G. SCHULZ,JOHANN</creatorcontrib><creatorcontrib>P. BARIE,JR,WALTER</creatorcontrib><creatorcontrib>T. EURICH,JAMES</creatorcontrib><title>KUNSTHARZ-FORMKOERPER UND VERFAHREN ZU IHRER HERSTELLUNG</title><description>Novel resin products produced by reacting unique polycyclic, aromatic, polycarboxylic acid products with low molecular weight polyols display satisfactory toughness properties and good Barcol hardness values. The process for preparing these novel resin products first involves preparing an intimate, finely divided mixture comprising the acid product derived from the nitric acid oxidation of naturally occurring solid carbonaceous material, a roughly equivalent amount of a liquid polyol, and a suitable acid catalyst. The mixture is then subjected to a precure step which involves heating at temperatures between 80 DEG and 150 DEG C. for from about fifteen minutes to about four hours. The precured mixture may thereafter be subjected to suitable molding conditions at a temperature below about 220 DEG C.</description><subject>CHEMISTRY</subject><subject>COMPOSITIONS BASED THEREON</subject><subject>MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONSONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS</subject><subject>METALLURGY</subject><subject>ORGANIC MACROMOLECULAR COMPOUNDS</subject><subject>THEIR PREPARATION OR CHEMICAL WORKING-UP</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>1984</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZLDwDvULDvFwDIrSdfMP8vX2dw0KcA1SCPVzUQhzDXJz9Ahy9VOIClXwBDKCFDxcg4JDXH18Qv3ceRhY0xJzilN5oTQ3g4Kba4izh25qQX58anFBYnJqXmpJvIursbGBpYWliaOhMRFKAFe4KJg</recordid><startdate>19840920</startdate><enddate>19840920</enddate><creator>G. SCHULZ,JOHANN</creator><creator>P. BARIE,JR,WALTER</creator><creator>T. EURICH,JAMES</creator><scope>EVB</scope></search><sort><creationdate>19840920</creationdate><title>KUNSTHARZ-FORMKOERPER UND VERFAHREN ZU IHRER HERSTELLUNG</title><author>G. SCHULZ,JOHANN ; P. BARIE,JR,WALTER ; T. EURICH,JAMES</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_DE3309894A13</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>ger</language><creationdate>1984</creationdate><topic>CHEMISTRY</topic><topic>COMPOSITIONS BASED THEREON</topic><topic>MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONSONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS</topic><topic>METALLURGY</topic><topic>ORGANIC MACROMOLECULAR COMPOUNDS</topic><topic>THEIR PREPARATION OR CHEMICAL WORKING-UP</topic><toplevel>online_resources</toplevel><creatorcontrib>G. SCHULZ,JOHANN</creatorcontrib><creatorcontrib>P. BARIE,JR,WALTER</creatorcontrib><creatorcontrib>T. EURICH,JAMES</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>G. SCHULZ,JOHANN</au><au>P. BARIE,JR,WALTER</au><au>T. EURICH,JAMES</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>KUNSTHARZ-FORMKOERPER UND VERFAHREN ZU IHRER HERSTELLUNG</title><date>1984-09-20</date><risdate>1984</risdate><abstract>Novel resin products produced by reacting unique polycyclic, aromatic, polycarboxylic acid products with low molecular weight polyols display satisfactory toughness properties and good Barcol hardness values. The process for preparing these novel resin products first involves preparing an intimate, finely divided mixture comprising the acid product derived from the nitric acid oxidation of naturally occurring solid carbonaceous material, a roughly equivalent amount of a liquid polyol, and a suitable acid catalyst. The mixture is then subjected to a precure step which involves heating at temperatures between 80 DEG and 150 DEG C. for from about fifteen minutes to about four hours. The precured mixture may thereafter be subjected to suitable molding conditions at a temperature below about 220 DEG C.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language ger
recordid cdi_epo_espacenet_DE3309894A1
source esp@cenet
subjects CHEMISTRY
COMPOSITIONS BASED THEREON
MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONSONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
METALLURGY
ORGANIC MACROMOLECULAR COMPOUNDS
THEIR PREPARATION OR CHEMICAL WORKING-UP
title KUNSTHARZ-FORMKOERPER UND VERFAHREN ZU IHRER HERSTELLUNG
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-27T22%3A18%3A48IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=G.%20SCHULZ,JOHANN&rft.date=1984-09-20&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EDE3309894A1%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true