DE3303097

For the sulphating roasting of sulphidic raw materials, calcium carbonate of a maximum particle size of 0.1 mm is admixed with the raw materials. During the subsequent roasting, CO2 is liberated from the calcium carbonate and thus aids the separation of the sulphur, the operation being carried out a...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: HANS, WALTER, , KINDBERG-AUMUEHL, AT, MUELLNER, PAUL, , TRAUN, AT, REITERER, HANS-DETLEF., GRAZ, AT, KATZENSTEINER, KARL, , LINZ, AT
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator HANS, WALTER, , KINDBERG-AUMUEHL, AT
MUELLNER, PAUL, , TRAUN, AT
REITERER, HANS-DETLEF., GRAZ, AT
KATZENSTEINER, KARL, , LINZ, AT
description For the sulphating roasting of sulphidic raw materials, calcium carbonate of a maximum particle size of 0.1 mm is admixed with the raw materials. During the subsequent roasting, CO2 is liberated from the calcium carbonate and thus aids the separation of the sulphur, the operation being carried out at low temperatures of at least 200 DEG C, and in particular 400-1000 DEG C. The operation is preferably carried out within the range of 450-850 DEG C, i.e. therefore below the decomposition temperature of pure calcium carbonate.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_DE3303097C2</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>DE3303097C2</sourcerecordid><originalsourceid>FETCH-epo_espacenet_DE3303097C23</originalsourceid><addsrcrecordid>eNrjZOB0cTU2NjA2sDTnYWBNS8wpTuWF0twMCm6uIc4euqkF-fGpxQWJyal5qSXxcPXORsZEKAEAy0oaag</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>DE3303097</title><source>esp@cenet</source><creator>HANS, WALTER, , KINDBERG-AUMUEHL, AT ; MUELLNER, PAUL, , TRAUN, AT ; REITERER, HANS-DETLEF., GRAZ, AT ; KATZENSTEINER, KARL, , LINZ, AT</creator><creatorcontrib>HANS, WALTER, , KINDBERG-AUMUEHL, AT ; MUELLNER, PAUL, , TRAUN, AT ; REITERER, HANS-DETLEF., GRAZ, AT ; KATZENSTEINER, KARL, , LINZ, AT</creatorcontrib><description>For the sulphating roasting of sulphidic raw materials, calcium carbonate of a maximum particle size of 0.1 mm is admixed with the raw materials. During the subsequent roasting, CO2 is liberated from the calcium carbonate and thus aids the separation of the sulphur, the operation being carried out at low temperatures of at least 200 DEG C, and in particular 400-1000 DEG C. The operation is preferably carried out within the range of 450-850 DEG C, i.e. therefore below the decomposition temperature of pure calcium carbonate.</description><edition>4</edition><language>eng</language><subject>CHEMISTRY ; COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSESC01D OR C01F ; FERROUS OR NON-FERROUS ALLOYS ; INORGANIC CHEMISTRY ; METALLURGY ; PRETREATMENT OF RAW MATERIALS ; PRODUCTION AND REFINING OF METALS ; TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><creationdate>1985</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19850711&amp;DB=EPODOC&amp;CC=DE&amp;NR=3303097C2$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19850711&amp;DB=EPODOC&amp;CC=DE&amp;NR=3303097C2$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>HANS, WALTER, , KINDBERG-AUMUEHL, AT</creatorcontrib><creatorcontrib>MUELLNER, PAUL, , TRAUN, AT</creatorcontrib><creatorcontrib>REITERER, HANS-DETLEF., GRAZ, AT</creatorcontrib><creatorcontrib>KATZENSTEINER, KARL, , LINZ, AT</creatorcontrib><title>DE3303097</title><description>For the sulphating roasting of sulphidic raw materials, calcium carbonate of a maximum particle size of 0.1 mm is admixed with the raw materials. During the subsequent roasting, CO2 is liberated from the calcium carbonate and thus aids the separation of the sulphur, the operation being carried out at low temperatures of at least 200 DEG C, and in particular 400-1000 DEG C. The operation is preferably carried out within the range of 450-850 DEG C, i.e. therefore below the decomposition temperature of pure calcium carbonate.</description><subject>CHEMISTRY</subject><subject>COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSESC01D OR C01F</subject><subject>FERROUS OR NON-FERROUS ALLOYS</subject><subject>INORGANIC CHEMISTRY</subject><subject>METALLURGY</subject><subject>PRETREATMENT OF RAW MATERIALS</subject><subject>PRODUCTION AND REFINING OF METALS</subject><subject>TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>1985</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZOB0cTU2NjA2sDTnYWBNS8wpTuWF0twMCm6uIc4euqkF-fGpxQWJyal5qSXxcPXORsZEKAEAy0oaag</recordid><startdate>19850711</startdate><enddate>19850711</enddate><creator>HANS, WALTER, , KINDBERG-AUMUEHL, AT</creator><creator>MUELLNER, PAUL, , TRAUN, AT</creator><creator>REITERER, HANS-DETLEF., GRAZ, AT</creator><creator>KATZENSTEINER, KARL, , LINZ, AT</creator><scope>EVB</scope></search><sort><creationdate>19850711</creationdate><title>DE3303097</title><author>HANS, WALTER, , KINDBERG-AUMUEHL, AT ; MUELLNER, PAUL, , TRAUN, AT ; REITERER, HANS-DETLEF., GRAZ, AT ; KATZENSTEINER, KARL, , LINZ, AT</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_DE3303097C23</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>1985</creationdate><topic>CHEMISTRY</topic><topic>COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSESC01D OR C01F</topic><topic>FERROUS OR NON-FERROUS ALLOYS</topic><topic>INORGANIC CHEMISTRY</topic><topic>METALLURGY</topic><topic>PRETREATMENT OF RAW MATERIALS</topic><topic>PRODUCTION AND REFINING OF METALS</topic><topic>TREATMENT OF ALLOYS OR NON-FERROUS METALS</topic><toplevel>online_resources</toplevel><creatorcontrib>HANS, WALTER, , KINDBERG-AUMUEHL, AT</creatorcontrib><creatorcontrib>MUELLNER, PAUL, , TRAUN, AT</creatorcontrib><creatorcontrib>REITERER, HANS-DETLEF., GRAZ, AT</creatorcontrib><creatorcontrib>KATZENSTEINER, KARL, , LINZ, AT</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>HANS, WALTER, , KINDBERG-AUMUEHL, AT</au><au>MUELLNER, PAUL, , TRAUN, AT</au><au>REITERER, HANS-DETLEF., GRAZ, AT</au><au>KATZENSTEINER, KARL, , LINZ, AT</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>DE3303097</title><date>1985-07-11</date><risdate>1985</risdate><abstract>For the sulphating roasting of sulphidic raw materials, calcium carbonate of a maximum particle size of 0.1 mm is admixed with the raw materials. During the subsequent roasting, CO2 is liberated from the calcium carbonate and thus aids the separation of the sulphur, the operation being carried out at low temperatures of at least 200 DEG C, and in particular 400-1000 DEG C. The operation is preferably carried out within the range of 450-850 DEG C, i.e. therefore below the decomposition temperature of pure calcium carbonate.</abstract><edition>4</edition><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_DE3303097C2
source esp@cenet
subjects CHEMISTRY
COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSESC01D OR C01F
FERROUS OR NON-FERROUS ALLOYS
INORGANIC CHEMISTRY
METALLURGY
PRETREATMENT OF RAW MATERIALS
PRODUCTION AND REFINING OF METALS
TREATMENT OF ALLOYS OR NON-FERROUS METALS
title DE3303097
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-28T16%3A17%3A16IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=HANS,%20WALTER,%20,%20KINDBERG-AUMUEHL,%20AT&rft.date=1985-07-11&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EDE3303097C2%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true