Recovery of atactic polypropylene after propylene polymerisation - by passage of soln. through heated tube
Atactic polypropylene is recovered from soln. formed as a by-product in the prepn. of a polymer contg. propylene, i.e. a propylene homopolymer, or a copolymer of propylene with another alpha-olefin. This is by vaporising the solvent in an elongated tubular heating zone, pref. at 120-300 degrees c. A...
Gespeichert in:
Hauptverfasser: | , , , , |
---|---|
Format: | Patent |
Sprache: | eng ; ger |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | OOKA,TATUO SADOTOMO,HIDEO SHIOMURA,TETSUNOSUKE HAGIWARA,KAZUO KOBAYASHI,TAKASHI |
description | Atactic polypropylene is recovered from soln. formed as a by-product in the prepn. of a polymer contg. propylene, i.e. a propylene homopolymer, or a copolymer of propylene with another alpha-olefin. This is by vaporising the solvent in an elongated tubular heating zone, pref. at 120-300 degrees c. A press. difference of >=3, (3-50) kg/cm2 is maintained between the entry and exit, the exit speed being >=40, (40-160) m/sec. Fine molten particles of atactic polypropylene practically free of solvent are formed in suspension. These are sepd. from solvent in a sepn. zone. Method is easy to perform, allowing recovery without blocking or clogging of the evapn. appts., and without needing (BE868380) mechanical entrainment appts. |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_DE2825843A1</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>DE2825843A1</sourcerecordid><originalsourceid>FETCH-epo_espacenet_DE2825843A13</originalsourceid><addsrcrecordid>eNqNjLsKwkAQRdNYiPoP8wMRTBTSBo1Yi32YrDcPWTPL7kTYv9eAYGt1uJzLWSaPK4y84CNJS6xsdDDkxEbnxUWLEcStwtNvz_YJPwTWQUZKqYnkOATuMEeC2HFL2nuZup56sOJOOjVYJ4uWbcDmy1VC5-p2vKRwUiM4Np-61qcqK7JDsc_LXf7H5Q1gtED2</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Recovery of atactic polypropylene after propylene polymerisation - by passage of soln. through heated tube</title><source>esp@cenet</source><creator>OOKA,TATUO ; SADOTOMO,HIDEO ; SHIOMURA,TETSUNOSUKE ; HAGIWARA,KAZUO ; KOBAYASHI,TAKASHI</creator><creatorcontrib>OOKA,TATUO ; SADOTOMO,HIDEO ; SHIOMURA,TETSUNOSUKE ; HAGIWARA,KAZUO ; KOBAYASHI,TAKASHI</creatorcontrib><description>Atactic polypropylene is recovered from soln. formed as a by-product in the prepn. of a polymer contg. propylene, i.e. a propylene homopolymer, or a copolymer of propylene with another alpha-olefin. This is by vaporising the solvent in an elongated tubular heating zone, pref. at 120-300 degrees c. A press. difference of >=3, (3-50) kg/cm2 is maintained between the entry and exit, the exit speed being >=40, (40-160) m/sec. Fine molten particles of atactic polypropylene practically free of solvent are formed in suspension. These are sepd. from solvent in a sepn. zone. Method is easy to perform, allowing recovery without blocking or clogging of the evapn. appts., and without needing (BE868380) mechanical entrainment appts.</description><edition>3</edition><language>eng ; ger</language><subject>CHEMISTRY ; COMPOSITIONS BASED THEREON ; MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVINGCARBON-TO-CARBON UNSATURATED BONDS ; METALLURGY ; ORGANIC MACROMOLECULAR COMPOUNDS ; THEIR PREPARATION OR CHEMICAL WORKING-UP</subject><creationdate>1980</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=19800103&DB=EPODOC&CC=DE&NR=2825843A1$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76290</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=19800103&DB=EPODOC&CC=DE&NR=2825843A1$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>OOKA,TATUO</creatorcontrib><creatorcontrib>SADOTOMO,HIDEO</creatorcontrib><creatorcontrib>SHIOMURA,TETSUNOSUKE</creatorcontrib><creatorcontrib>HAGIWARA,KAZUO</creatorcontrib><creatorcontrib>KOBAYASHI,TAKASHI</creatorcontrib><title>Recovery of atactic polypropylene after propylene polymerisation - by passage of soln. through heated tube</title><description>Atactic polypropylene is recovered from soln. formed as a by-product in the prepn. of a polymer contg. propylene, i.e. a propylene homopolymer, or a copolymer of propylene with another alpha-olefin. This is by vaporising the solvent in an elongated tubular heating zone, pref. at 120-300 degrees c. A press. difference of >=3, (3-50) kg/cm2 is maintained between the entry and exit, the exit speed being >=40, (40-160) m/sec. Fine molten particles of atactic polypropylene practically free of solvent are formed in suspension. These are sepd. from solvent in a sepn. zone. Method is easy to perform, allowing recovery without blocking or clogging of the evapn. appts., and without needing (BE868380) mechanical entrainment appts.</description><subject>CHEMISTRY</subject><subject>COMPOSITIONS BASED THEREON</subject><subject>MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVINGCARBON-TO-CARBON UNSATURATED BONDS</subject><subject>METALLURGY</subject><subject>ORGANIC MACROMOLECULAR COMPOUNDS</subject><subject>THEIR PREPARATION OR CHEMICAL WORKING-UP</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>1980</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNjLsKwkAQRdNYiPoP8wMRTBTSBo1Yi32YrDcPWTPL7kTYv9eAYGt1uJzLWSaPK4y84CNJS6xsdDDkxEbnxUWLEcStwtNvz_YJPwTWQUZKqYnkOATuMEeC2HFL2nuZup56sOJOOjVYJ4uWbcDmy1VC5-p2vKRwUiM4Np-61qcqK7JDsc_LXf7H5Q1gtED2</recordid><startdate>19800103</startdate><enddate>19800103</enddate><creator>OOKA,TATUO</creator><creator>SADOTOMO,HIDEO</creator><creator>SHIOMURA,TETSUNOSUKE</creator><creator>HAGIWARA,KAZUO</creator><creator>KOBAYASHI,TAKASHI</creator><scope>EVB</scope></search><sort><creationdate>19800103</creationdate><title>Recovery of atactic polypropylene after propylene polymerisation - by passage of soln. through heated tube</title><author>OOKA,TATUO ; SADOTOMO,HIDEO ; SHIOMURA,TETSUNOSUKE ; HAGIWARA,KAZUO ; KOBAYASHI,TAKASHI</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_DE2825843A13</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; ger</language><creationdate>1980</creationdate><topic>CHEMISTRY</topic><topic>COMPOSITIONS BASED THEREON</topic><topic>MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVINGCARBON-TO-CARBON UNSATURATED BONDS</topic><topic>METALLURGY</topic><topic>ORGANIC MACROMOLECULAR COMPOUNDS</topic><topic>THEIR PREPARATION OR CHEMICAL WORKING-UP</topic><toplevel>online_resources</toplevel><creatorcontrib>OOKA,TATUO</creatorcontrib><creatorcontrib>SADOTOMO,HIDEO</creatorcontrib><creatorcontrib>SHIOMURA,TETSUNOSUKE</creatorcontrib><creatorcontrib>HAGIWARA,KAZUO</creatorcontrib><creatorcontrib>KOBAYASHI,TAKASHI</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>OOKA,TATUO</au><au>SADOTOMO,HIDEO</au><au>SHIOMURA,TETSUNOSUKE</au><au>HAGIWARA,KAZUO</au><au>KOBAYASHI,TAKASHI</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Recovery of atactic polypropylene after propylene polymerisation - by passage of soln. through heated tube</title><date>1980-01-03</date><risdate>1980</risdate><abstract>Atactic polypropylene is recovered from soln. formed as a by-product in the prepn. of a polymer contg. propylene, i.e. a propylene homopolymer, or a copolymer of propylene with another alpha-olefin. This is by vaporising the solvent in an elongated tubular heating zone, pref. at 120-300 degrees c. A press. difference of >=3, (3-50) kg/cm2 is maintained between the entry and exit, the exit speed being >=40, (40-160) m/sec. Fine molten particles of atactic polypropylene practically free of solvent are formed in suspension. These are sepd. from solvent in a sepn. zone. Method is easy to perform, allowing recovery without blocking or clogging of the evapn. appts., and without needing (BE868380) mechanical entrainment appts.</abstract><edition>3</edition><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | eng ; ger |
recordid | cdi_epo_espacenet_DE2825843A1 |
source | esp@cenet |
subjects | CHEMISTRY COMPOSITIONS BASED THEREON MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVINGCARBON-TO-CARBON UNSATURATED BONDS METALLURGY ORGANIC MACROMOLECULAR COMPOUNDS THEIR PREPARATION OR CHEMICAL WORKING-UP |
title | Recovery of atactic polypropylene after propylene polymerisation - by passage of soln. through heated tube |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-02T22%3A40%3A34IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=OOKA,TATUO&rft.date=1980-01-03&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EDE2825843A1%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |